    I either Tig, Mig, or Fluxcore, haven't stick welded in at least 30+yrs. Anyway, been messing with some 6011, noticed no real slag on the welds. Even opened up a fresh, sealed box cause the first few I tried were old, and laying on the bench in the open. Normal for 6011? Any thoughts? Thanks!
    Yeah, same question on other forums.

  2. #2
    Join Date
    Jun 2012
    Location
    CT
    Posts
    4,059
    Post Thanks / Like

    Re: no slag

    Yeah, pretty normal. 6011 has a light slag coating that never completely covers the weld bead.
    Syncrowave 250
    Purox Metalmaster

  3. #3
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    5,189
    Post Thanks / Like

    Re: no slag

    6011 has a cellulose based coating so most of it goes up in smoke.
    Mike
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"
    Hobart G-213 portable
    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  4. #4
    Join Date
    Jul 2008
    Posts
    2,612
    Post Thanks / Like

    Re: no slag

    I think carbon dioxide from the burning cellulose does most of the "shielding." I've read that 6010/11 are like "spray arc" in mig, regarding in the way the weld metal is deposited.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,606,311,509.92520 seconds with 11 queries