    PM1000 torch issue?

    I was changing out the nozzle on the original torch of my PM 1000 and saw what looks like corrosion. I use it maybe 1-2 times a month and have never had any issues.

    Do I need to worry about this?
    Name:  C5D4D41C-26A8-488B-A5C2-245DCBDFA043.jpg
Views: 180
Size:  65.9 KB
    Miller Dynasty 200 DX
    Millermatic 211
    Lincoln X-Tractor 1GC
    Hypertherm Powermax 1000

  2. #2
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    3,609
    Post Thanks / Like

    Re: PM1000 torch issue?

    that's arcing between the electrode and the piston. Either caused by dirt between them or the electrode is hanging up a little
    in the swirl baffle. Clean off piston with scotchbrite and replace the electrode and swirl baffle before using again.
    That is the power connection between the electrode and piston so keep it clean.
    You should be able to assemble the nozzle, electrode and swirl baffle and hold between your fingers. Electrode should move freely
    when you move your hand.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,185,250.61119 seconds with 12 queries