+ Reply to Thread
Results 1 to 14 of 14

Thread: Lightning MTS 275, coming soon. Final testing

  1. #1
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Lightning MTS 275, coming soon. Final testing

    Here is our new "Lightning MTS 275". This represents the lastest Evolution of our product line of MTS units that started back in 2009. This will be our third AC/DC model released. Once again, a leading, industry first development. Digital unit with improved synergic "Power Set" function for all modes, MIG, TIG and Stick. Multiple units are in final testing stages. We are shooting for the end of the year.

    It has a digital panel of course, one of the largest TFT displays in a welder in the industry. One thing we wanted to resolve that is a common complaint of all digital screen and digital type units is the ability to access and SEE your parameters at a glance without scrolling. Our unique response to this was a careful design of the display to allow multiple settings to be displayed at a glance, without having to enter setup menus. It is focused on Intuitive operation. It has many of the similar features and specs of the PowerMTS 252STi, as far as power output, duty cycle and features. It welds E6010 as well. But it also has a few more surprises in store, which we'll reveal when the unit is fully in production or as details are finalized.

    As you can, see this unit has a water cooler and cart option that allows the unit to be conveniently packaged for mobility around the shop, or can be quickly decoupled for use in the field. It comes with the 36 Series Binzel type gun, Nova Brand foot Pedal, and 20 Series TIG torch, along with the stick electrode holder and work clamp.
    Name:  LIghtning 275 Front.jpg
Views: 4875
Size:  74.3 KBName:  Lightning 275 side.jpg
Views: 4799
Size:  72.3 KB
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  2. Likes XMilitary liked this post
  3. #2
    Join Date
    Sep 2011
    Posts
    78
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    It would be awesome to test one of these out.

  4. #3
    Join Date
    Mar 2014
    Posts
    860
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    Mark, do you have a ball-park on cost?

  5. #4
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    High 3k's. Low 4ks list with cooler, cart.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  6. #5
    Join Date
    Mar 2010
    Location
    Delaware
    Posts
    2,975
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    Mark, I see Christian Livingstone is promoting the MTS275 on other forums is he going to be one of the testers
    www.georgesplasmacuttershop.com
    Plasma Cutter and Welder Sales and Repairs--Ebay store
    Tec.Mo. Dealer Consumables for the PT and IPT torch's

  7. #6
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    I haven't even heard from him for a while. If he is promoting, it is and always has been of his own free volition. He's never been paid or encouraged to promote our products. All units are in testing now.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  8. #7
    Join Date
    Mar 2014
    Posts
    860
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    Mark, thanks for the reply. Send one to me! They would (could, depending) be a hit here. I'm serious! I have a trapline that it could be passed around within. One is the largest boat builder in AK.

  9. #8
    Join Date
    Jun 2016
    Location
    SE Saskatchewan, Canada
    Posts
    360
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    Am glad to see several of these machines being tested by fella's I follow on Instagram. It looks like just the ticket for my needs.
    Red Seal Journeyman Welder (2003), Red Seal Journeyman Metal Fabricator (2018), Welding Engineering Technologist (2005)
    Pressure - ASME Section IX
    Structural - CSA W47.1, CSA W47.2
    Transport tanker - CSA B620
    Aerospace - AWS D17.1

  10. #9
    Join Date
    Oct 2016
    Location
    USA
    Posts
    139
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    New MTS looks good!

  11. #10
    Join Date
    Oct 2016
    Location
    USA
    Posts
    139
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    Quote Originally Posted by Yofish View Post
    Mark, do you have a ball-park on cost?
    It's on their US site now.

    https://www.everlastgenerators.com/p...ti-tig-package

    Probably still not shipping yet but at least they list the price and some specs.

  12. #11
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    It is shipping.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  13. #12
    Join Date
    Nov 2012
    Posts
    3,274
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    i got mine yesterday. Did a little welding with it, getting set up for another smoker build. Seems pretty nice, so far. Is there a manual written by someone that has English as their first language? What do they mean by 'splash'?

  14. #13
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    Quote Originally Posted by TimmyTIG View Post
    i got mine yesterday. Did a little welding with it, getting set up for another smoker build. Seems pretty nice, so far. Is there a manual written by someone that has English as their first language? What do they mean by 'splash'?
    You can download a 100 page manual from our website. https://www.everlastgenerators.com/s...f01eaa6455.pdf
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  15. Likes TimmyTIG liked this post
  16. #14
    Join Date
    Nov 2012
    Posts
    3,274
    Post Thanks / Like

    Re: Lightning MTS 275, coming soon. Final testing

    Quote Originally Posted by lugweld View Post
    You can download a 100 page manual from our website. https://www.everlastgenerators.com/s...f01eaa6455.pdf
    That's much better than the one that came with the machine. Thank you!

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,303,620.14566 seconds with 19 queries