    I've seen passing mention of using a switch to enable and disable the CE MIG 170 capacitor mod, but not much information on what kinds of voltages and amperages the switch needs to be rated for, and what gauge wire to use for connecting it.

    Is there a switch that can handle the current, or would adding a relay be the smarter option? Something like this, perhaps?

    https://www.ebay.com/itm/SSR-100-DD-....c100290.m3507

  2. #2
    Join Date
    May 2009
    Location
    Wyoming US
    Posts
    3,261
    Post Thanks / Like

    Re: HF MIG 170 Cap Mod Switch selection

    The wires can be 10 gauge, a 50A switch will be fine.
    NAPA sells a switch , part # 786100

  3. #3
    Join Date
    Jul 2019
    Posts
    17
    Post Thanks / Like

    Re: HF MIG 170 Cap Mod Switch selection

    Thanks, looks like they have it locally to me. I'm planning on using 6awg wire, what crimp connectors would be best? Most automotive-style don't seem to be up to the task, perhaps something like these?

    https://www.ebay.com/itm/20-Pack-6-7...AAAOSw7Phc-z2O

  4. #4
    Join Date
    Oct 2016
    Posts
    450
    Post Thanks / Like

    Re: HF MIG 170 Cap Mod Switch selection

    I tried a 50 amp switch from the local farm store, with about 112,000uf

    it melted the internals down in just a couple welding projects. Same result with automotive 40 amp relays

    Went with this switch and been trouble free- probably a bit overkill, unlike the relays don't need another power source

    https://www.ebay.com/itm/300A-BATTER....c100005.m1851
    Last edited by 455dan; 07-24-2019 at 06:00 PM.
    HTP Pro Pulse 220 MTS (Anniversary Edition)
    1962 Idealarc TIG 300 300
    1974 Idealarc TIG 300 300
    1988 HF Power MIG 150
    2015 Lotos Ltpdc2000d plasma/Stick/TIG
    Victor 100 torch, 200- 210 Oxy/Acet gauges

  5. #5
    Join Date
    Jul 2019
    Posts
    17
    Post Thanks / Like

    Re: HF MIG 170 Cap Mod Switch selection

    Excellent, thanks. I'm a little annoyed that my eBay searches for switches didn't bring that item up. It's amazing how few high-amp switches there seems to be out there. Looks like it will accept 1/4 copper 6awg ring terminals, too.

  6. #6
    Join Date
    Jul 2019
    Posts
    17
    Post Thanks / Like

    Re: HF MIG 170 Cap Mod Switch selection

    I ended up using one of those switches, has worked fine so far, but I've only done a few small test welds. You can see my implementation here;

    https://weldingweb.com/vbb/showthread.ph...-upgrade-REDUX

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,292,596.14726 seconds with 19 queries