    Hello to the esab forum. I am a new guy to the forum. Coming to get some help from your veterans.
    A little bit of background. We are a auto repair shop, we purchased the rebel emp 215ic a few years back. The machine stopped working a few month ago, no power up. I opened up the side panel, found a part on the main powerboard was burnt, soot was found all over the surrounding area.
    The question is, what the part is, I am guessing a thermistor. It is marked with VR1, right between line 1 and line 2. Since it was burnt really good, I could not find any mark on the part to know the real part number of the spec of it. Tried a lws, new board only, they don't repair the board, it cost more than a new machine. I did not take the board out yet, I will try to load a picture to show it better.
    thanks in advance.Name:  IMG_20190917_081601.jpg
Views: 757
Size:  131.0 KBName:  IMG_20190917_081728.jpg
Views: 741
Size:  149.6 KB

  2. #2
    Join Date
    Jun 2011
    Location
    Aiken SC area
    Posts
    1,184
    Post Thanks / Like

    Re: ESAB REBEL EMP 215IC power board problem

    Looking at the location of the destroyed part, it appears to be between the inputs, L2 and ?. Indicating to me that it is an MOV to protect the circuit from high voltage spikes, etc. The foil on the reverse side could also be blown off or damaged. They are sized according to voltage, 300,600,etc. This could be the only damaged part on the board but you won't know until you remove the board and examine the foil circuitry. Good luck, Bob

  3. #3
    Join Date
    Sep 2019
    Posts
    7
    Post Thanks / Like

    Re: ESAB REBEL EMP 215IC power board problem

    Hi rhunt, thanks a lot for your input.

  4. #4
    Join Date
    Feb 2019
    Location
    Snyder TX
    Posts
    96
    Post Thanks / Like

    Re: ESAB REBEL EMP 215IC power board problem

    Check with Inovat Corp.

    https://www.innovatcorp.com/

  5. #5
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,048
    Post Thanks / Like

    Re: ESAB REBEL EMP 215IC power board problem

    This machine isn't too old. I don't think they will have them at Innovat unless there is a high failure rate. It may still be under warranty. Find out when you bought it. It has a three year warranty.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  6. #6
    Join Date
    Feb 2019
    Location
    Snyder TX
    Posts
    96
    Post Thanks / Like

    Re: ESAB REBEL EMP 215IC power board problem

    Innovat can repair the board - might be less expensive that a new one.

  7. #7
    Join Date
    Sep 2019
    Posts
    7
    Post Thanks / Like

    Re: ESAB REBEL EMP 215IC power board problem

    Hi everyone,
    I finally received the MOV(390V, 20MM diameter for a greater survival amp) and had some time today to work on the machine. Replaced the burnt MOV, checked the continuity, one of the power switch blade shot too. It is a 25A rated switch in the machine, could only find a 15A piece. After checking everything, hooked to 240V, everything worked. Did not have much time, ran a few 6010, worked.
    So, I believe the high volt reached the clamping limit of the MOV and shot the MOV itself together with the switch. Cost $20. Thanks everyone especially rhunt for your input.

  8. #8
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,048
    Post Thanks / Like

    Re: ESAB REBEL EMP 215IC power board problem

    That's good news. $20.00 is cheap for a welder repair these days.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  9. #9
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    3,609
    Post Thanks / Like

    Re: ESAB REBEL EMP 215IC power board problem

    Blown input MOV is not covered under ESABs warranty. Most of the time the cause is voltage spikes or wrong line voltage.
    Check you line.

  10. #10
    Join Date
    Sep 2019
    Posts
    7
    Post Thanks / Like

    Re: ESAB REBEL EMP 215IC power board problem

    Right, high voltage for sure. Shop has 208 and 120 only. Just did not know what happened, it is a shop machine, lots of hands reach it.

  11. #11
    Join Date
    Apr 2016
    Location
    CA
    Posts
    7,031
    Post Thanks / Like

    Re: ESAB REBEL EMP 215IC power board problem

    Hmmm... .. . Interesting repair... .. .
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,153,448.22284 seconds with 12 queries