    HELP! Puff of white smoke when adding filler, TIG

    Recently got a new to me Miller Econo Twin HF stick/Tig machine. I can weld fine without adding filler, get a good stable arc and practiced welding lines, but as soon as I go to add any filler the pool puffs a cloud of white smoke that covers my mask in two to three dabs. Also covers the weld cup and shoots tiny metal particales everywhere. I first thought i wasn't getting things clean enough but after putting on a new gas lens, cleaning the practice pieces with a flap disc and rubbing them and the filler down liberally with acetone I still run into the same problem. I'm at a loss as to what to try next.
    PLEASE help me figure out what i'm doing wrong.

    running just over 100 amps on 11 gauge mild steel
    wp-17 torch with HF start button attached
    1/16 thoriated tungsten with 1/16ER 70s-2 filler
    Name:  40C2C5B5-4CBC-49C7-BDEA-3B3813BFA38A.jpg
Views: 403
Size:  86.9 KB
    Name:  391009BF-5F77-4EB9-8FD5-9C927965F9D9.jpg
Views: 402
Size:  122.3 KB
    Name:  F15486DE-9980-4D94-9C6D-B001CC372695.jpg
Views: 400
Size:  100.7 KB
    Last edited by Wwelder99; 10-08-2019 at 04:35 PM. Reason: Corrections/images

  2. #2
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    450
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    What sort of CFH are you running? Are you sure the mild steel isn't galvanized? If it's galvanized you really don't want to breath that white smoke! Do you have other steel to try?
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P
    Spoolmatic 30A
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  3. #3
    Join Date
    Oct 2019
    Posts
    6
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Knew i forgot something, started at 15 cfh then went up to 20 but didn't appear to make a difference. I'm sure it's not galvanized as the sheet metal was sitting outside and had a layer of rust over it that i ground down to bare steel. I've tried other pieces and have the same result, works well without filler but puffs and coughs as soon as i add filler.
    Thanks for the response.

  4. #4
    Join Date
    Nov 2012
    Location
    North Carolina / Maine
    Posts
    90
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    It sure looks like something is galvanized. What about the filler wire? What is it and where did you get it? I can't think of anything that's in mild steel that could make a mess like that. The fact that you can run lines on the base metal without filler material says that it's not the problem. Something about the filler is not right. Could you be using flux core wire by chance?

  5. #5
    Join Date
    Mar 2017
    Location
    Qatar
    Posts
    345
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Have you tried another filler? Could be your filler is severely contaminated. Even some stainless filler as you are just practicing.


    Sent from my iPhone using Tapatalk
    Miller Dynasty 280 DX TIGRunner
    Fronius Transsteel 2200

  6. #6
    Join Date
    Oct 2019
    Posts
    6
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Picked the filler up from the DFW welding supply nearby, like I said it's ER 70 s-2 at least that's what the guy wrote on the package and gave to me when I told him what I was welding. When i wiped them down there was a black residue that came off onto the rag but i wiped until there was black no more. I do have some 308L filler so i'll give that a shot now and see if it makes a difference.
    Thanks for the responses!

  7. #7
    Join Date
    Oct 2019
    Posts
    6
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Name:  A4EE34D7-69A7-4E85-9704-18838C07A4AB.jpg
Views: 297
Size:  117.0 KB
    SUCCESS!!
    Thanks so much everyone for the quick replies and suggestions, the 308l welds exactly how I imagined TIG to be, now I can finally get to practice. (I’m sure you can tell I need it)
    What do you think could have caused such serious contamination on the ER 70? Manufacture? Storage? I haven’t had it but a week before I used it, and kept it in the plastic bag provided.
    Thanks again everyone, don’t know why I didn’t try the 308 before.

  8. #8
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    450
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    My guess is the guy grabbed the wrong filler rod for you. How is the filler rod marked? The ends are usually flattened and stamped on modern TIG filler rods.

    In a pinch you can buy MIG ER70S-6 wire and twist it by making a loop, attaching one half to a fixed point and then the other end to a bolt in a drill and spin away. I've done this with .035 wire and the braided wire you wind up with is fine for practicing or working on thinner metal. That's a lot cheaper than burning up your 308 practicing.
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P
    Spoolmatic 30A
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  9. #9
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    5,156
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Quote Originally Posted by Wwelder99 View Post
    Picked the filler up from the DFW welding supply nearby, like I said it's ER 70 s-2 at least that's what the guy wrote on the package and gave to me when I told him what I was welding
    That's my vote as to what went wrong. He could have given you mild steel filler wire for Oxy-Acet possibly. I've never ran it under a TIG arc, but I believe it is different.
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

  10. #10
    Join Date
    Oct 2019
    Posts
    6
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Negative on the crimped marked ends, just a bronze/gold 36” rod.
    The 308L does have the crimps and is marked as such.
    Thanks for the advice on using mig wire, I have a 5lb spool for my mig, now I’ll have a use for the 13’ of wire that is normally wasted when the spool is out.

  11. #11
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    5,156
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    If it looks like silicon-bronze filler rod, then it might be just that. It looks bronze/gold-ish. Not sure it would give off white smoke though. Might want to check Google if O-A rod would give off fumes when under an electric arc.
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

  12. #12
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    2,966
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Check to see if the filler rod is attracted to a magnet.

  13. #13
    Join Date
    Jul 2008
    Posts
    2,608
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Brass brazing rod? That might give off zinc...it sure looks like zinc oxide on your shield.

  14. #14
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    8,681
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Quote Originally Posted by walker View Post
    Check to see if the filler rod is attracted to a magnet.
    X2 on this

  15. #15
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,586
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Quote Originally Posted by Wwelder99 View Post
    Picked the filler up from the DFW welding supply nearby, like I said it's ER 70 s-2 at least that's what the guy wrote on the package and gave to me when I told him what I was welding. When i wiped them down there was a black residue that came off onto the rag but i wiped until there was black no more. I do have some 308L filler so i'll give that a shot now and see if it makes a difference.
    Thanks for the responses!
    I like a happy ending!

    Moral of the story. Never buy tig filler that is not marked or flagged accompanied by MTRs(material test reports-certs).
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Li ncolnSW2002ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig4ea,MigMax1ea.

  16. #16
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,632
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Quote Originally Posted by Oscar View Post
    That's my vote as to what went wrong. He could have given you mild steel filler wire for Oxy-Acet possibly. I've never ran it under a TIG arc, but I believe it is different.
    I've tig welded with oxy/fuel rods. It's a little less clean, but no big clouds of white.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  17. #17
    Join Date
    Apr 2017
    Location
    Long Island, NY
    Posts
    345
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Whatever you end up doing, at the very least bring that crap back to where you bought it and ask for a refund!
    Lincoln Invertec V205-T Tig/stick
    Miller Coolmate 1.3 Coolant System
    Millermatic 211 Mig Welder
    Speedglas Adflo PAPR 9100 FX-Air
    CertiFlat FB2430 fabBlock U-Weld Kit Welding Table
    FW3012 CertiFlat fabWing 30" X 12" Extension Table

  18. #18
    Join Date
    Oct 2019
    Posts
    6
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    That would definitely make more sense that I was given the wrong filler. Iím out of town for work so wonít be able to check magnetism until Friday. I will definitely be taking the pound of unknown filler back and explain the situation, though Iíll probably wait until I need to refill my argon as the welding supply is a bit of a drive into town. Ordered some er70s-2 off fleabay in the meantime BlueDemon brand, as well as some lanthanated tungsten.

  19. #19
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    450
    Post Thanks / Like

    Re: HELP! Puff of white smoke when adding filler, TIG

    Quote Originally Posted by Wwelder99 View Post
    Ordered some er70s-2 off fleabay in the meantime BlueDemon brand, as well as some lanthanated tungsten.
    I've been very happy with BlueDemon er70S-6 so far and didn't notice any difference when compared with some of the more expensive brands. I've heard folks say they got some that was oily, but I haven't had that issue. Looking forward to hearing if you ever figure out what they heck rod they gave you!
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P
    Spoolmatic 30A
    Hobart Champion Elite
    Everlast PowerTig 210EXT

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,606,146,337.55781 seconds with 12 queries