    ESAB Warrior 500i issues

    Hi all. I have some problems regarding MMA on ESAB Warrior 500i. I am using E8018 electrode. During welding, there seem to be large fluctuations of Amps which causes instability and splatter while welding. I would appreciate your help and guidance. Thank you very much.

  2. #2
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    4,233
    Post Thanks / Like

    Re: ESAB Warrior 500i issues

    Call ESAB tech support and ask them. How old is the welder?

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Tags for this Thread

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,276,946.83646 seconds with 17 queries