    Victor/Thermal Dynamics Cutmaster 102

    I purchased this from auction for my shop and have come to the realization it is just too big for the use I need it for. Most of the work I do with a plasma is thin sheetmetal/body panels, with nothing over 1/4". This is just a little overkill and I could use the money for other things going on in the shop.

    Unit works good. I had an issue when first wiring it up it was not recognizing the correct voltage, but some fiddling with the voltage input switch and it was able to recognize the 240V. Previous shop had it wired for 480V, I am currently running it from 1 Phase 240V. It pulls 98A (I think) at full load, but I have it only wired to a 50A plug so never go above about 1/4 power.

    I also purchased a new consumables kit for it as the torch was a little beat up. This evening I plan to go out and clean it up a bit as well as put the new consumables on the torch. It is under power in my shop and you're welcome to test it. I'd really prefer local pick up as it is pretty heavy. I am in Raleigh NC. I'd like to get $1000 for it (I spent $170 on the consumables kit alone).

    Name:  IMG_0198.jpg
Views: 511
Size:  96.5 KBName:  IMG_0203.jpg
Views: 520
Size:  136.2 KB

  2. #2
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    6,310
    Post Thanks / Like

    Re: Victor/Thermal Dynamics Cutmaster 102

    Nice!, wish you were closer to me

  3. #3
    Join Date
    Apr 2016
    Location
    Northern Virginia
    Posts
    94
    Post Thanks / Like

    Re: Victor/Thermal Dynamics Cutmaster 102

    How about $920 for WW members. prefer local on this, but might be able to ship it if it is sitting in another few weeks.

  4. #4
    Join Date
    Apr 2008
    Location
    NW ON Canada
    Posts
    3,377
    Post Thanks / Like

    Re: Victor/Thermal Dynamics Cutmaster 102

    These big cutters are really designed/intended to be run on higher voltage 3phase power.
    Jason
    Lincoln Idealarc 250 stick/tig
    Thermal Dynamics Cutmaster 52
    Miller Bobcat 250
    Torchmate CNC table
    Thermal Arc Hefty 2
    Ironworkers Local 720

  5. #5
    Join Date
    Apr 2016
    Location
    Northern Virginia
    Posts
    94
    Post Thanks / Like

    Re: Victor/Thermal Dynamics Cutmaster 102

    I am willing to ship this now for anyone interested. I get a good rate on fedex through work so could probably ship it for <$75 anywhere in the US.

  6. #6
    Join Date
    May 2008
    Location
    Matthews NC
    Posts
    119
    Post Thanks / Like

    Re: Victor/Thermal Dynamics Cutmaster 102

    Man I wish I would have seen this before I bought my Bobcat. If you got in another month or so I will ride up and get it from you.
    AWS CWI/CWE
    ASNT NDT Level 2 PT/MT
    AWS Certified Welder(aerospace)

  7. #7
    Join Date
    Apr 2016
    Location
    Northern Virginia
    Posts
    94
    Post Thanks / Like

    Re: Victor/Thermal Dynamics Cutmaster 102

    Quote Originally Posted by redcoupe View Post
    Man I wish I would have seen this before I bought my Bobcat. If you got in another month or so I will ride up and get it from you.
    Happy to take a down payment on it if you're serious

  8. #8
    Join Date
    May 2008
    Location
    Matthews NC
    Posts
    119
    Post Thanks / Like

    Re: Victor/Thermal Dynamics Cutmaster 102

    Hey do you still have this thing? I forgot all about this posting.
    AWS CWI/CWE
    ASNT NDT Level 2 PT/MT
    AWS Certified Welder(aerospace)

  9. #9
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    4,805
    Post Thanks / Like

    Re: Victor/Thermal Dynamics Cutmaster 102

    Dang that machine looks like a beast! I could run that on my 30HP phase converter! Sweet deal for who ever picked/picks it up!
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,593,942,251.96759 seconds with 14 queries