    Hi, I've been reading through the owner's manual and don't see a spot weld function for the dynasty 210 dx. Is it in a hidden menu?

    Many thanks,

    Harold

  2. #2
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    466
    Post Thanks / Like

    Re: Dynasty 210 Dx have spot weld function?

    I'm pretty sure it doesn't have a dedicated spot weld function, but you could come up with one using the sequencer options.

    P.S. posting the same question in two places is generally frowned upon on most forums. It's better to have all the answers in one place rather than spread out in multiple threads.
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P
    Spoolmatic 30A
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  3. #3
    Join Date
    Jan 2020
    Posts
    6
    Post Thanks / Like

    Re: Dynasty 210 Dx have spot weld function?

    Thanks G-ManBart for your fast response, I'll check the sequencer options. Apologies for the multiple posts, a bit of a fumbling start on my part.

  4. #4
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    3,677
    Post Thanks / Like

    Re: Dynasty 210 Dx have spot weld function?

    Looks like it does. See owners manual on how to access the tech menu. section 11-2 scroll to weld timers and set it up.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,607,104,121.89675 seconds with 11 queries