    Find Top Dead Center of a Hemisphere

    Name:  IMG_20200803_110233-01.jpg
Views: 454
Size:  131.8 KB

    Does anyone know of a way to determine the top dead center (or bottom center) of a hemisphere?

    I need to drill about 50 of these steel pieces with a 1/16" hole to hang them from a 1/16" water hard drill rod, and I want them to hang level. I'd like to think there is a trick out there to find the top center of a hemisphere - but I'm coming up blank.

    Thanks in advance for any ideas.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  2. #2
    Join Date
    Nov 2005
    Location
    ca
    Posts
    95
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Syncrowave 250 w/ coolrunner
    MM210 W/spoolgun
    SP 135
    Victor O/A
    Ramsond cut 50
    Titanium Stick 225.

  3. #3
    Join Date
    Apr 2015
    Location
    N 48 38.680 W 080 40.837
    Posts
    934
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Assume the dome is reasonably close to being a perfect circle.

    1) measure the diameter in several places and get an close average
    2) build a wood jig flat on a wood surface large enough to hold the dome and still clamp to the drill table. The jig is two pieces of wood (say 1" x 1") at 90 degrees (x and y axis) to nestle the dome into for drilling
    3) where the x and y axis meet is 0x by 0y. Fasten the jig to the drill table so that a coordinate of 1/2x diameter by 1/2y diameter is under the drill point

    Push the domes into the jig and drill.
    Last edited by John Bartley; 08-03-2020 at 03:54 PM.

  4. Likes Shootr liked this post
  5. #4
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,504
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    One option might be to put them on a turn table or lazy suzan. Put a sharpie or other marker in a jig to point it at near center.
    If you have a magnetic base dial indicator that should be able to hold the marker.
    Rotate the hemisphere so it draws a line around the center.
    Another option to get close to the center might be to rest a 4.5 inch grinder disc on the top of the hemisphere so it is level. Then use that to draw your circle.
    https://uploads.tapatalk-cdn.com/202...30ed99d3d0.jpg

    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  6. Likes Shootr liked this post
  7. #5
    Join Date
    Oct 2013
    Location
    W. WA
    Posts
    480
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Looks like only 1 1/2” dia. Lathe with 3-jaw chuck....
    Cap should fit flat against chuck body. Drill with tailstock.

  8. #6
    Join Date
    May 2020
    Location
    Arizona
    Posts
    419
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Quote Originally Posted by John Bartley View Post
    Assume the dome is reasonably close to being a perfect circle.

    1) measure the diameter in several places and get an close average
    2) build a wood jig flat on a wood surface large enough to hold the dome and still clamp to the drill table. The jig is two pieces of wood (say 1" x 1") at 90 degrees (x and y axis) to nestle the dome into for drilling
    3) where the x and y axis meet is 0x by 0y. Fasten the jig to the drill table so that a coordinate of 1/2x diameter by 1/2y diameter is under the drill point

    Push the domes into the jig and drill.
    Now if I just had a drill press lol. Sorry, should have mentioned that at first. I was hoping there was a way to just mark/dot the spot on the hemisphere to drill. I'll have to think about your solution - pretty sure a jig as you describe would indeed work for me, just have to figure out the marking mechanism.

    Thank you for the detailed reply.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  9. #7
    Join Date
    Oct 2013
    Location
    W. WA
    Posts
    480
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Name:  B2BF8A0E-CB2D-4110-87F7-22FEF38BAC8C.jpeg
Views: 433
Size:  36.7 KB
    Can you find a pvc plumbing cap whose id is your metal cap od, center drill that. Use that as jig to put over each metal cap, use sharpie to mark/center punch?

  10. Likes Shootr, MickOz, mcspeed, VaughnT liked this post
  11. #8
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    5,275
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Clamp your center punch vertical in the vise, then set the hemisphere concave side down on the punch. keep moving it around until level and tap it over the punch with a hammer.
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"
    Hobart G-213 portable
    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  12. Likes William McCormick, Weldalittle liked this post
  13. #9
    Join Date
    Oct 2014
    Posts
    3,018
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    A bunch of different ways to do it but if they are standard pipe caps let gravity be your friend. If they are square and flat, block them on a table and level them across the open end at least 3 different ways. A block of wood with a hole smaller than the OD to hold them would work good. Then put a drop of cutting oil in the dome. It will sit in the middle at the bottom so you can center punch them. The oil will help with drilling but any liquid, even water would work but only use a tiny amount to be more accurate. Having a drill press would make it fairly easy to set up a jig but manually drilling might have to mark each one separately.
    Last edited by Welder Dave; 08-03-2020 at 05:35 PM.

  14. #10
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,225
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    I use lathe and a 3 jaw.
    If have a 3 jaw Chuck just the center Chuck on drill press.

    Dave

    Quote Originally Posted by Shootr View Post
    Name:  IMG_20200803_110233-01.jpg
Views: 454
Size:  131.8 KB

    Does anyone know of a way to determine the top dead center (or bottom center) of a hemisphere?

    I need to drill about 50 of these steel pieces with a 1/16" hole to hang them from a 1/16" water hard drill rod, and I want them to hang level. I'd like to think there is a trick out there to find the top center of a hemisphere - but I'm coming up blank.

    Thanks in advance for any ideas.

  15. #11
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    7,134
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Pointed caliper. Adjust to turn an arc from the edge to center. Get very close to center. mark several arcs from the edge, Your point is at center of these marks.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  16. Likes Weldalittle liked this post
  17. #12
    Join Date
    Jun 2008
    Location
    Hardwood Lands, Nova Scotia, Canada
    Posts
    1,854
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Fasten two pieces of 1/2 plywood to your drill press table one on top of the other and both screwed together . Drill a hole the size of the cap in the top piece of plywood only using a hole saw or forsner bit, without moving the table, replace the hole saw with a small pilot drill and mark or drill thru the cap that you place in the previously drilled hole.................Mike

  18. Likes mcspeed liked this post
  19. #13
    Join Date
    Oct 2014
    Posts
    3,018
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    I think the problem is no drill press.

  20. #14
    Join Date
    Jun 2008
    Location
    Hardwood Lands, Nova Scotia, Canada
    Posts
    1,854
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    I think the problem is no drill press.
    Oops, missed that key piece of info LOL............Mike

  21. #15
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    7,093
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Quote Originally Posted by Willie B View Post
    Pointed caliper. Adjust to turn an arc from the edge to center. Get very close to center. mark several arcs from the edge, Your point is at center of these marks.
    I was thinking of that from another old post years ago where the guy had huge domes. I had forgotten what I described but it's the same as you say. Just finding the center of a circle with a compass/caliper, but 3-D.
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  22. #16
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,225
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Ok Hand drill, center punch and centering head with ruler.

    https://www.wonkeedonkeetools.co.uk/...-9/3PS-9-1.jpg
    Name:  3PS-9-1.jpg
Views: 411
Size:  29.3 KB

    I have in past works great do not buy or even look at Staerrter there are other brands a lot cheaper.

    Dave

    Quote Originally Posted by Welder Dave View Post
    I think the problem is no drill press.
    8
    Last edited by smithdoor; 08-03-2020 at 07:55 PM.

  23. #17
    Join Date
    Sep 2014
    Posts
    1,426
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Do you know someone with a lathe? That would be the quickest.


    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  24. Likes Shootr liked this post
  25. #18
    Join Date
    Sep 2014
    Posts
    1,426
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Back in the day before we had a drill press, this is what I used to make rather accurate holes in things. That piece on top is a drill bushing, you can interchange them as they wear out, or if you want to use different sized drill bits.

    The holder was cut from a solid piece of aluminum on a bandsaw. You can make the adjustment slot and then just weld the end shut if you do not wish to play around with welding the bandsaw blade back together after you put it through a starting hole if you want more adjustment or just leave it open like that one is. There is a countersink head screw under the plate that the wing nut tightens the holder to the plate.

    If you make that all you have to do is center one, and the rest you can just lay into a depression that is lined up with the drill guide.

    Name:  press5.jpg
Views: 419
Size:  35.6 KB

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  26. #19
    Join Date
    Sep 2014
    Posts
    1,426
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    If you get a 1/16" drill bushing you could even mount the bushing in a piece of wood, line it up once, and drill away.


    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  27. Likes CAVEMANN liked this post
  28. #20
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,966
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Polish the dome

    Hang a plumb line. Bob at dome height. Slide dome under bob. It will touch at TDC.

    Or plumb/level a bushing on top. Then drill down the center.

    For 50...I'd probably make a box/fixture, similar to what has been described. Center of the circle base is center of the top/dome.

  29. Likes Shootr liked this post
  30. #21
    Join Date
    May 2020
    Location
    Arizona
    Posts
    419
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    I can't thank you all enough for taking the time to provide these many great ideas. If this next project or two results in sales, top of the list is a drill press!

    As arduous as it sounds, the best option I'm coming up with is:

    Clamp a center punch in my vise vertically - just high enough to set a dome on it with the edges 1/8" or so above the jaws. Manually tweak the position of the dome until it's sitting level. Hold it steady and whack the dome with a hammer to mark the balance point. Drill from the inside.

    It took a couple minutes apiece to do three tests. They came out perfect and sat nice and level on the rod. I think doing it this way, as tedious as it may be, will also account for any imbalance in each individual dome from mis-stamping.




    If I can ask another question: The drill bits, as you can imagine, are very fragile. Would it be better to clamp them in my Dremel and drill at low (8000RPM) speed? My 1800rpm drill doesn't seem to want to make the hole in any kind of reasonable time.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  31. #22
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    5,275
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    This is where a bench top drill press would work very well. Since 1/16" bits are pretty much impossible to sharpen, I'm speaking for myself on this. 1800 RPM is still awfully fast IMO for even a 1/16" bit. If your drill is variable speed try to run it very slow. Buy a can of cutting oil and with the concave surface it will hold a small puddle of the oil on the hole while you're drilling.
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"
    Hobart G-213 portable
    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  32. #23
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,966
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Are those cast Iron or press steel?

  33. #24
    Join Date
    May 2020
    Location
    Arizona
    Posts
    419
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    Quote Originally Posted by tapwelder View Post
    Are those cast Iron or press steel?
    Pressed steel, what type I do not know. 0.080" +/- walls.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  34. #25
    Join Date
    Oct 2014
    Posts
    3,018
    Post Thanks / Like

    Re: Find Top Dead Center of a Hemisphere

    If you're going to use oil to drill why not use the oil to mark the center? Kill 2 birds with one stone. Depending on how high the dome is might be tricky to use a centering head.

  35. Likes Shootr liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,610,979,591.66820 seconds with 15 queries