    gas/air regulation

    I have a PPro 256Si. I would like to run a manifold ( Tee Block ) to control both the air/gas into. I would prefer one way valves as well so I can just turn the argon on and the air off or visa versa to run thru the machine. I can find plenty of 1/4 in suggestions but the 256Si uses a 5/8 CGA fitting. Anyone have any suggestions? I would like to mount this on the top and connect a single line down to the gas receiver at the bottom of the machine.

  2. #2
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,009
    Post Thanks / Like

    Re: gas/air regulation

    There are plenty out there. The 5/8 CGA is common and standard in the industry. Western has one. https://www.weldingstore.com/product...hoCrrcQAvD_BwE
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,593,682,983.13824 seconds with 13 queries