    Lis2323
    I got the Mag drill on Friday and started making my jig. I ran out of energy, too much going on. I will hope post Monday. I'm going to copy your second design. Drill, slide the work piece, drop the pin in the hole just drilled. then flip and hope the holes line up.
    Thanks for all your help.

  2. Likes Lis2323 liked this post
  3. #127
    Join Date
    Oct 2015
    Location
    South Lyon, MI
    Posts
    83
    Post Thanks / Like

    Re: Best method to drill hundreds of holes

    Wouldn't a gang drill that can get several steps done at once be more appropriate here? Just looking at this from a man-hours POV.

  4. #128
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    152
    Post Thanks / Like

    Re: Best method to drill hundreds of holes

    I completely forgot to follow up on this thread.
    Here is what I came up with. I got 24 drill bushings and found a machines to drill and tap them in some flat stock. They are spaced every two inches. I clamp the flat stock down and use a center punch to mark hole location. The I built a simple jig one for 3x2 rectangular tubing and another for 3x3 square. I got long 1/4 drill bits from McMaster-Car and drill thru both sides in one shot. Then I come back and use a 5/8 drill bite. It works perfectly. The magnetic drill is a big time savor.Name:  2.jpg
Views: 92
Size:  138.5 KBName:  1.jpg
Views: 92
Size:  121.1 KBName:  3.jpg
Views: 93
Size:  148.7 KB

  5. Likes ronsii liked this post
  6. #129
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    152
    Post Thanks / Like

    Re: Best method to drill hundreds of holes

    Thanks guys. The squat racks turn out perfect every time.

  7. #130
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    2,749
    Post Thanks / Like

    Re: Best method to drill hundreds of holes

    Quote Originally Posted by Reebz View Post
    Thanks guys. The squat racks turn out perfect every time.
    As we knew they would!! Good work
    :

  8. #131
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    152
    Post Thanks / Like

    Re: Best method to drill hundreds of holes

    Thanks man. My jig is a little tight, at some point I will do as you suggested drill a hole, move the material drop a pin in, and drill another hole, repeat. You folks are great

  9. Likes DavidR8 liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,832,081.88431 seconds with 15 queries