    Tig newby here. I recently acquired a #9 torch and a 7" tungsten is too long to fit inside the end cap.
    So I need to cut some in half for use in this torch.

    My bandsaw shatters them. They take the sharp angle off the edge of the grinding stone (wears the stone really fast). They are too long to fit in my ebay rotary tool sharpener.
    Suggestions?

    TIA,
    robert

  2. #2
    Join Date
    Feb 2015
    Posts
    182
    Post Thanks / Like

    Re: How to cut tungsten?

    I would suggest an abrasive cut-off wheel on a 4 1/2 inch anglehead grinder. Or use one in a die grinder. (One that is made for the die grinder.) Sometimes they are called zip disks, some call them Metabo wheels,etc. No matter the name, it is simply a thin abrasive disk designed to cut on the edge of the wheel. Good luck!

  3. Likes BD1, robert-r liked this post
  4. #3
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: How to cut tungsten?

    Yup, an 045 or 040 disk will slice them quick.
    1st on WeldingWeb to have a scrolling sig!



  5. Likes robert-r liked this post
  6. #4
    Join Date
    Apr 2020
    Location
    AntHome 92025
    Posts
    213
    Post Thanks / Like

    Re: How to cut tungsten?

    Thanks, dudes!!! & haha.... there is a grinder with a thin cutoff disc on the bench. Was out there whole time I was driving myself nuts.

  7. #5
    Join Date
    Mar 2018
    Posts
    17
    Post Thanks / Like

    Re: How to cut tungsten?

    A quick rap with a flat metal bar when resting on the edge of a metal table of bench vice will break it sharply and easily. i use that to knock of dips before sharpening. Yes I've had lots of those.

  8. Likes robert-r liked this post
  9. #6
    Join Date
    Feb 2016
    Location
    W. Texas
    Posts
    201
    Post Thanks / Like

    Re: How to cut tungsten?

    I use the edge of the bench grinder wheel to grind a V in the middle then snap it. Then touch up the point.

    Zach

  10. Likes robert-r, Rondo liked this post
  11. #7
    Join Date
    May 2007
    Posts
    4,589
    Post Thanks / Like

    Re: How to cut tungsten?

    Quote Originally Posted by WTXBTUMOVER View Post
    I use the edge of the bench grinder wheel to grind a V in the middle then snap it. Then touch up the point.

    Zach
    exactly

  12. #8
    Join Date
    Oct 2014
    Posts
    5,270
    Post Thanks / Like

    Re: How to cut tungsten?

    A couple pairs of pliers will snap them too.

  13. Likes robert-r liked this post
  14. #9
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    8,196
    Post Thanks / Like

    Re: How to cut tungsten?

    When i had to cut a bunch of pieces for short cap torches i would drill a hole in a wood block to the right depth and cut them with a very narrow (.035 x 3") disc on a right angle die grinder, then dump the hot piece in a tray. Didn't take long to cut a bunch up.

  15. Likes robert-r liked this post
  16. #10
    Join Date
    Apr 2020
    Location
    AntHome 92025
    Posts
    213
    Post Thanks / Like

    Re: How to cut tungsten?

    Thanks, Everyone!!! Great solutions!!! Very much appreciated.

  17. #11
    Join Date
    Apr 2010
    Posts
    2,963
    Post Thanks / Like

    Re: How to cut tungsten?


    robert-r


    Quote Originally Posted by robert-r View Post
    Thanks, Everyone!!! Great solutions!!! Very much appreciated.
    Stop thanking - there are many refinements - unposted . . .


    Opus

  18. Dislikes robert-r disliked this post
  19. #12
    Join Date
    Oct 2014
    Posts
    5,270
    Post Thanks / Like

    Re: How to cut tungsten?

    Here's a similar method to using pliers I borrowed from a Miller forum.

    I've grown fond of using 2 vice grips, nose to nose for quite some time...snaps 'em nice and easy. I prefer the 8WR's because they "square up" easy due to their width and I usually have a pair with me just about everywhere I tig. The splitting thing doesn't seem to be a problem for me this way.

  20. #13
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    2,221
    Post Thanks / Like

    Re: How to cut tungsten?

    You shouldn't snap any tungstens other than thoriated... not great advice IMO!
    Thoriated are the only type that reliably cleanly snap.

    Lanthanated tungstens can often hairline crack when you snap them, and welding with a cracked tungsten is horrible. Ceriated and other types are even worse, they splinter.
    This is common knowledge and something I've seen myself.

    Abrasive wheel is your friend. I use the corner of my diamond wheel to cut through them, you've then got half a prep on the ends straight away as well

  21. #14
    Join Date
    Apr 2006
    Location
    Outside of Raleigh, NC
    Posts
    1,805
    Post Thanks / Like

    Re: How to cut tungsten?

    Quote Originally Posted by 123weld View Post
    exactly
    Me too
    Miller Trailblazer Pro 350D
    Miller Suitcase MIG
    Miller Spectrum 2050
    Miller Syncrowave 250DX
    Lincoln 210MP

  22. #15
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: How to cut tungsten?

    Quote Originally Posted by WTXBTUMOVER View Post
    I use the edge of the bench grinder wheel to grind a V in the middle then snap it. Then touch up the point.

    Zach

    I just take the extra 2 seconds and cut all the way through so I don’t worry about splintering the tungsten

  23. Likes danielplace liked this post
  24. #16
    Join Date
    Jul 2008
    Posts
    3,312
    Post Thanks / Like

    Re: How to cut tungsten?

    Don't cut it -- just grind it back to a point again. I don't know why everybody seems to think new welders need to cut off tungstens. I've never cut a tungsten.

    It's like cutting an inch off a pencil before sharpening it. WTF? Who does that?
    Last edited by Kelvin; 04-29-2020 at 08:47 AM.

  25. #17
    Join Date
    Nov 2009
    Location
    Pensacola , Fla
    Posts
    1,622
    Post Thanks / Like

    Re: How to cut tungsten?

    he is using a short back cap, must cut
    DIY CNC Plasma table USB BOB Price THC
    Hypertherm 65
    Everlast PowerTig 255 EXT
    Miler 180 Mig
    13" metal lathe
    Mill/ Drill
    ECT, ECT,

  26. Likes danielplace liked this post
  27. #18
    Join Date
    Jul 2008
    Posts
    3,312
    Post Thanks / Like

    Re: How to cut tungsten?

    Quote Originally Posted by acourtjester View Post
    he is using a short back cap, must cut
    Well.
    That's very different, then.
    Never mind!


    Oh -- and, cutoff wheel!

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,290,365.42900 seconds with 20 queries