    finally got around to finishing it... only a week in advance!





    Still needs a rub up with brasso or something to get rid of the pinkish tinge and smooth the surface up ever so slightly.

  2. Likes dmcnally, 12V71, Lis2323 liked this post
  3. #27
    Join Date
    Apr 2014
    Location
    Illinois
    Posts
    2,391
    Post Thanks / Like

    Re: Cake stand

    Awesome, totally awesome. Just like I said, a piece that can be passed down generation to generation.
    --
    Finished and with plenty of time left to smooth the surface. Way to go Munkul!!! Now git yourself to that alter. ; )
    MM 211
    Smith Tru Lite O/A set, Thanks Bob!
    Lincoln AC-225
    --
    But you must not change one thing, one pebble, one grain of sand, until you know what good and evil will follow on that act. The world is in balance, in Equilibrium- Ursula K. Le Guin

  4. #28
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    437
    Post Thanks / Like

    Re: Cake stand

    Have you tried putting anything similar to similar cake weight on it yet? Or even just pushing down on the top tier? Might be a good idea to test it out prior to polishing...
    -Dave
    XMT304, 22A Feeder

  5. #29
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    853
    Post Thanks / Like

    Re: Cake stand

    I was leaning on it with the DA to sand out the scratches, so yes, I'm confident enough of the strength

    Funny stuff, copper. I annealed one of the helical spars to get a slight bend straightened out. It was then soft as butter. Flexed it a bit one way and then the other, and most of that annealed state vanished in two bends. In its work hardened state, it's pretty rigid.

  6. #30
    Join Date
    Mar 2004
    Location
    hueytown, ala
    Posts
    97
    Post Thanks / Like

    Re: Cake stand

    when the caterer sees it, they will want to buy it or you give it to them !!

    j

  7. #31
    Join Date
    Feb 2016
    Location
    Myrtle Beach
    Posts
    494
    Post Thanks / Like

    Re: Cake stand

    Looks great!
    Lincoln 350MP
    Millermatic 350P
    Syncrowave 250
    1969 SA200
    HTP Invertig 221

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,594,126,991.91269 seconds with 13 queries