    Re: Countersink recommendation?

    A good titanium nitride coating is absolutely NOT a gimmick, it will improve tool life several times over.
    NRA LIFE MEMBER
    UNITWELD 175 AMP 3 IN1 DC MIG/STICK/TIG
    MIDSTATES 300 AMP AC MACHINE
    GOD BLESS AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  2. #27
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    3,097
    Post Thanks / Like

    Re: Countersink recommendation?

    A good tool with a quality titanium nitride coating is absolutely NOT a gimmick, it will increase tool life several times over.
    NRA LIFE MEMBER
    UNITWELD 175 AMP 3 IN1 DC MIG/STICK/TIG
    MIDSTATES 300 AMP AC MACHINE
    GOD BLESS AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  3. #28
    Join Date
    Mar 2011
    Location
    McGregor, Iowa
    Posts
    120
    Post Thanks / Like

    Re: Countersink recommendation?

    I use a MA Ford HSS Chatterless 6 Flute Countersink ALtima® Blaze Coated and its the best countersink I have ever used. I have and used HSS, carbide, Ticn coated, 0-6 flute and the 6 is by far the best. More flutes equals less chip load than a single flute which helps when countersinking flat heads. For just deburring a hole a single flute works decent so it doesn't dig in.

  4. #29
    Join Date
    Jan 2015
    Location
    Ohio
    Posts
    654
    Post Thanks / Like

    Re: Countersink recommendation?

    @ferret I didn't see your post before I bought something or else I would have checked on that one.

    I called Fastenal and checked on a couple Keo countersinks but they'd have to order them in. Then I checked with MSC and they had one: 82 degree, 3 flute, cobalt so I drove over there and got it. I don't have any knowledge base to compare it to but it seems fine to me. They didn't list a 6 flute with a 5/8" body.

    Vibrates at all speeds, not smooth like a drill bit but perhaps that's normal. Probably a 6 flute would vibrate a little less. The zero flute one with the big hole in it might run smooth but the Keo engineer said it was for deburring.

    The little needle like shards my countersink creates are nasty. Some are almost microscopic and seems like their mission in life is to dig into your skin. Even with vacuuming, some escape and nail you and you have to put a magnifying hood on to remove them. I may put a magnet in a plastic bag and see if that works better.

    The one I got has a 5/8" body which I thought would be fine for countersinking 5/16" flat head machine screws but no. So I have to go to 1/4" machine screws to hold my table top on. The countersink was $20 with tax and I don't want to go back to buy a bigger one.

  5. #30
    Join Date
    Oct 2013
    Location
    Long Island, NY
    Posts
    2,154
    Post Thanks / Like

    Re: Countersink recommendation?

    Quote Originally Posted by JD1 View Post
    The engineer from Keo that answered my email said that chatter usually means the RPM's are too high. I don't know myself, not real experienced with countersinks.

    Fastenal has a location here and they're showing a number of different 82 degree cobalt Keo countersinks on their site. I may call them Monday and see what's in stock, then run over there.
    I ran it at 90 rpm. :/
    www.FirehouseFabricators.com

    [B]

    Lincoln 210mp
    Lincoln SW200
    Hypertherm Powermax 45xp
    2x4 CNC Plasma Table.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,594,261,693.78731 seconds with 11 queries