Tungsten Stingers, Angle Burs, Carbide Ball Burs
I've got some tungsten Stingers, angle burs, and ball burs. The stingers are for tig welding I believe but I'm not sure. They were made by Diamond Ground Products. They are precut and presharpened. The manufacturer said this tungsten was the highest quality because the company they were made for did nuclear welding. I've got about 40 or so of the angle burs and about 25 or so of the ball burs. Email me or text me if your interested at 662-295-5480.
-
-
Re: Tungsten Stingers, Angle Burs, Carbide Ball Burs
Do you have any pics and/or prices you can post here. I'm not interested but it would save people time in having to contact you if you would just cut to the chase and state your price. Who are you? This is your first post on WeldingWeb, how does anyone know they can trust you?
-
Post Thanks / Like - 2 Likes, 0 Dislikes
-
Re: Tungsten Stingers, Angle Burs, Carbide Ball Burs
As Traditional stated, post pics, price, shipping etc. There are some members here who don't do the whole text thing. You posting those once is about 3-5 minutes of work. It will save every member the time required to ask those questions if you do not have what is wanted or the price is wrong.
I am interested in some of the burrs if the price is right.
Millermatic 252 MIG
Miller Dynasty 200DX TIG
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
Arclight Dynamics 4x8 plasma table
www.psacustomcreations.com
-
Re: Tungsten Stingers, Angle Burs, Carbide Ball Burs
I understand. I didn't an option to add pics when I posted. I'll check it out. My dad worked at Babcock & Wilcox for 30 plus years. I ran across these items in his storage unit when he passed away.
-
Re: Tungsten Stingers, Angle Burs, Carbide Ball Burs
https://photos.app.goo.gl/X8fm9K2oiVU2R2CDA
These are electrodes that are used for TIG welding and they are pre-cut and pre-sharpened.
Diamond Ground Products told me these were custom made for Babcock and Wilcox, they do nuclear welding so the material is of the highest quality. The material is made by Wolfram in Germany, it's not the lower quality Chinese stuff you would pick up at the local gas supplier.
3/32" diameter
1.750" length
25 degree included angle on one end
.010" tip flat
2% Thoriated material
Last edited by rebsfan; 05-16-2020 at 10:50 AM.