Results 1 to 14 of 14

Thread: Victor torch head in a fire: rebuild or not?

  1. #1
    Join Date
    Aug 2016
    Location
    Michigan
    Posts
    173
    Post Thanks / Like

    Victor torch head in a fire: rebuild or not?

    I did a cursory look online, but can't find anything on it.

    My victor journeyman torch head was in a trash can fire. I know, draped over the edge is no place to put it. I'm a mess.

    Can i rebuild this head? I think probably the valves are toast, but the basic head/tip? Clean and reuse? Gauges were no where near and
    i had the gas off. The end 6 inches or so of the lines were toast, i cut it off. Rest of the hoses look ok.

    Thoughts?
    Miller Syncrowave 300(s)
    Miller 330 A/BP
    Miller CP-200 Haas / Kamp'd / CP-300 in process
    Miller Radiator 1
    Miller 30A /S-52E feeders
    Hobart GR-303

  2. #2
    Join Date
    Oct 2014
    Posts
    2,007
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    Do you have some pics. of it?

  3. #3
    Join Date
    Aug 2016
    Location
    Michigan
    Posts
    173
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    Here you go. Just as i found it.

    Sent from my LG-TP450 using Tapatalk
    Miller Syncrowave 300(s)
    Miller 330 A/BP
    Miller CP-200 Haas / Kamp'd / CP-300 in process
    Miller Radiator 1
    Miller 30A /S-52E feeders
    Hobart GR-303

  4. #4
    Join Date
    May 2016
    Location
    Southern California
    Posts
    146
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    see below, duplicate post
    Last edited by _Dom; 05-24-2020 at 04:11 PM.
    Miller Multimatic 220AC
    Miller Thunderbolt 225
    Victor OA

  5. #5
    Join Date
    May 2016
    Location
    Southern California
    Posts
    146
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    Member here OAdoctor services equipment. Has been very helpful in the past. Hasn't posted in a few years but website looks alive. Give him a call;
    https://regulatortorchrepair.com/
    Miller Multimatic 220AC
    Miller Thunderbolt 225
    Victor OA

  6. #6
    Join Date
    Aug 2016
    Location
    Michigan
    Posts
    173
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    Thanks. I wire wheeled everything. As expected the valves did not survive. All orings turned to powder. Valves and orings should do it.

    Sent from my LG-TP450 using Tapatalk
    Miller Syncrowave 300(s)
    Miller 330 A/BP
    Miller CP-200 Haas / Kamp'd / CP-300 in process
    Miller Radiator 1
    Miller 30A /S-52E feeders
    Hobart GR-303

  7. #7
    Join Date
    Apr 2010
    Posts
    2,622
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?


    86turbodsl


    Quote Originally Posted by 86turbodsl View Post
    . . . My victor journeyman torch head was in a trash
    can fire. I know, draped over the edge . . .
    What is 'The Rest of the Story' ?


    Opus

  8. #8
    Join Date
    Jul 2016
    Location
    Midwest
    Posts
    375
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    If you send it in for repair they do total refurb. Good as new after that. Check valves and cutting plunger are probably cooked too. Just send it to a repair facility like Mckenzie repair and have a warranty fix. But. the cost will be the same as an aftermarket complete kit.
    Thermal Arc 320SP ( Lorch )
    Cobra Pythons
    Thermal Arc 300 AC/DC ( Sanrex )
    ESAB 301i AC/DC ( Lorch )
    Thermal Arc 161STL ( WTL )
    Thermal Arc 190S ( Sanrex )
    Cut Master 82, 42. Cut45 ( WTL )
    Victor Gas Apps.
    Boxes and boxes of welding crap.

  9. #9
    Join Date
    Aug 2016
    Location
    Michigan
    Posts
    173
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    Ok, the rest of the story -

    Repairing a shop fan, didn't have any sawhorses left. My main set got repurposed into holding up a desk top in the house as my boss gave me 1 day to make a home office for the lockdown. We've got some of the most draconian lock down policy here in Michigan. As a result i haven't been going to the store and just making due with everything at home as much as possible.

    so i was repairing the fan blade cage on the shop fan, and had it sitting on the edge of the trash can. there wasn't much in the can that was flamable, but enough i guess. I tacked the angle iron in place and went indoors for lunch. Came back an hour and half later and the flames were just finishing up. shop full of smoke. It must have smoldered for at least an hour before lighting up.

    Lost my mig gun, a harbor freight grinder, the fan cord, and the torch handle. Ironically, the fan is ok.
    I think the torch handle is rebuildable, probably just valves and orings. The grinder and mig gun is toast.

    the mig gun was the expensive part. 400A bernard 15' The ends are ok, the cable is toast.

    I'm lucky the shop didn't burn down, but high ceilings and nothing sitting around the burning pile probably saved it. My lesson was don't be stupid and careless around fire.

    I'm rethinking putting a few wood tools in the same space as the welding/fab.
    Miller Syncrowave 300(s)
    Miller 330 A/BP
    Miller CP-200 Haas / Kamp'd / CP-300 in process
    Miller Radiator 1
    Miller 30A /S-52E feeders
    Hobart GR-303

  10. #10
    Join Date
    Aug 2016
    Location
    Michigan
    Posts
    173
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    Quote Originally Posted by Rondo View Post
    If you send it in for repair they do total refurb. Good as new after that. Check valves and cutting plunger are probably cooked too. Just send it to a repair facility like Mckenzie repair and have a warranty fix. But. the cost will be the same as an aftermarket complete kit.
    Probably overkill. Looks like just valves and orings. Victor 100FC torch handle. haven't found the orings for the flashback arrestors though. Just whole arrestors.
    At $25 ea it's probably cheaper to buy a whole handle on epay.
    Miller Syncrowave 300(s)
    Miller 330 A/BP
    Miller CP-200 Haas / Kamp'd / CP-300 in process
    Miller Radiator 1
    Miller 30A /S-52E feeders
    Hobart GR-303

  11. #11
    Join Date
    Oct 2014
    Posts
    2,007
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    You probably need new flashback arrestor cartridges too but if it were mine, I'd just replace it and be glad I didn't lose a lot more. You don't know if it did any damage to the lines inside the handle but looks like it got fairly hot.

  12. #12
    Join Date
    Aug 2016
    Location
    Michigan
    Posts
    173
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    whats in those arrestor cartridges? Looks like just metal and orings to me, but i can't see inside them so i guessing.

    Anybody know if you can buy bernard mig cables without all the end hardware? So far all i've found is whole assemblies.
    Miller Syncrowave 300(s)
    Miller 330 A/BP
    Miller CP-200 Haas / Kamp'd / CP-300 in process
    Miller Radiator 1
    Miller 30A /S-52E feeders
    Hobart GR-303

  13. #13
    Join Date
    Aug 2016
    Location
    Michigan
    Posts
    173
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    Quote Originally Posted by Welder Dave View Post
    You probably need new flashback arrestor cartridges too but if it were mine, I'd just replace it and be glad I didn't lose a lot more. You don't know if it did any damage to the lines inside the handle but looks like it got fairly hot.
    I took the handle completely apart. didn't find anything inside that was warped or anything. It all screws together nice still.
    Miller Syncrowave 300(s)
    Miller 330 A/BP
    Miller CP-200 Haas / Kamp'd / CP-300 in process
    Miller Radiator 1
    Miller 30A /S-52E feeders
    Hobart GR-303

  14. #14
    Join Date
    Aug 2016
    Location
    Michigan
    Posts
    173
    Post Thanks / Like

    Re: Victor torch head in a fire: rebuild or not?

    I grabbed a 2nd hand victor WH260C torch handle off ebay for half the price of the flashback arrestor cost.
    I doubt i'll get the use out of a new set. I might pickup the torch 6 times a year. My tanks have lasted the last 10.
    Last edited by 86turbodsl; 05-24-2020 at 08:49 PM.
    Miller Syncrowave 300(s)
    Miller 330 A/BP
    Miller CP-200 Haas / Kamp'd / CP-300 in process
    Miller Radiator 1
    Miller 30A /S-52E feeders
    Hobart GR-303

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,593,797,554.46335 seconds with 11 queries