    OK, don’t laugh too much but here is my first attempt at a lamb’s tongue. I think I bent the big loop a little too much.

    Name:  77503FEF-95B5-41DB-AE56-E987CF3D49A2.jpeg
Views: 785
Size:  111.3 KB
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  2. Likes William McCormick, mcspeed liked this post
  3. #27
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,801
    Post Thanks / Like

    Re: Fab School

    Perfect

    Sent from my moto g power using Tapatalk

  4. Likes William McCormick liked this post
  5. #28
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    5,897
    Post Thanks / Like

    Re: Fab School

    Quote Originally Posted by wb4rt View Post
    OK, don’t laugh too much but here is my first attempt at a lamb’s tongue. I think I bent the big loop a little too much.

    Name:  77503FEF-95B5-41DB-AE56-E987CF3D49A2.jpeg
Views: 785
Size:  111.3 KB

    Not bad. It is your preference. They will be bent different on straight rail vs pitched, if you want them to stick out the same amount.

  6. Likes William McCormick liked this post
  7. #29
    Join Date
    Mar 2007
    Location
    MidWest
    Posts
    594
    Post Thanks / Like

    Re: Fab School

    Quote Originally Posted by wb4rt View Post
    OK, don’t laugh too much but here is my first attempt at a lamb’s tongue. I think I bent the big loop a little too much.

    Name:  77503FEF-95B5-41DB-AE56-E987CF3D49A2.jpeg
Views: 785
Size:  111.3 KB
    Burt, first try congrats. I never bent one but soon as I settle on a bender i will give it a shot.

    By the way. May I ask what model bender you used and the die size you settle on?

    Appears from your profile me and you are about in the same boat.....lots candles on the cake
    Geezer
    Power Mig 255C
    185 TIG
    Blue 175 MIG
    Ranger 8 Kohler 20HP
    1974 5K Lincoln/Wisconsin Powered (Cherry)
    Victor/Harris O/A
    K 487 Spool Gun

  8. Likes William McCormick liked this post
  9. #30
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,294
    Post Thanks / Like

    Re: Fab School

    Hey Geezer,

    Yep a few candles on the cake but my only able-bodied friend is 82 and I’m a bit younger than him. Almost everyone my age has a bad back or heart or something so I have to call Bob when I need a hand.

    Per Phil’s post #25, I used a 1 1/4” with a 1 1/2” die for the small loop on the end. I used a 2 1/2” for the larger loop. My 1” die is missing or I would have used it with the 1 1/4”. I think it would look a little better.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  10. Likes William McCormick liked this post
  11. #31
    Join Date
    Mar 2007
    Location
    MidWest
    Posts
    594
    Post Thanks / Like

    Re: Fab School

    Thanks Burt, may I ask:

    what type bender you have?

    assume you are bending 1 15/16" cap?? I imagine the 1 3/4" would bend easy also assuming large enough throat on the bender.

    thanks, i sure enjoy this thread. I have several feet of handrail to build
    Geezer
    Power Mig 255C
    185 TIG
    Blue 175 MIG
    Ranger 8 Kohler 20HP
    1974 5K Lincoln/Wisconsin Powered (Cherry)
    Victor/Harris O/A
    K 487 Spool Gun

  12. Likes William McCormick liked this post
  13. #32
    Join Date
    Mar 2007
    Location
    MidWest
    Posts
    594
    Post Thanks / Like

    Re: Fab School

    post 31 should read 2 1/4" versus 1 3/4". Couldn't get edit feature to cooperate
    Geezer
    Power Mig 255C
    185 TIG
    Blue 175 MIG
    Ranger 8 Kohler 20HP
    1974 5K Lincoln/Wisconsin Powered (Cherry)
    Victor/Harris O/A
    K 487 Spool Gun

  14. #33
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,294
    Post Thanks / Like

    Re: Fab School

    Sorry Geezer, I had that in my first reply but it got erased before I posted it.

    I think it is a Harbor Freight bender. I bought it off Craig’s List 5-6 years ago. They are all pretty much the same I think. HF has it for less than $90 but they may be hard to find. They told me they are supposed to get some in August. You should try Northern Tools also. They seem to be better stocked.

    I’m using 1 5/8” cap I think.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  15. Likes William McCormick liked this post
  16. #34
    Join Date
    Mar 2007
    Location
    MidWest
    Posts
    594
    Post Thanks / Like

    Re: Fab School

    Quote Originally Posted by wb4rt View Post
    Sorry Geezer, I had that in my first reply but it got erased before I posted it.

    I think it is a Harbor Freight bender. I bought it off Craig’s List 5-6 years ago. They are all pretty much the same I think. HF has it for less than $90 but they may be hard to find. They told me they are supposed to get some in August. You should try Northern Tools also. They seem to be better stocked.

    I’m using 1 5/8” cap I think.
    Thanks Burt, appears those HF benders are fitting many uses. My local store sold out, but they said inventory is on its way.

    I feel like I am back in welding school. Just prior to retiring I signed up for courses at a local JC.....attended at night. Then after retirement went during the day. They basically ran us through most of the common welding disciplines, Stick, MIG (solid and gas shield), TIG all at most positions. Welded with a buzz box for years prior to that, but felt like my out of position welding really lack some skill....and it did. So I am a hobby guy that does allot of free work. Now building handrails around this old house and the club house.

    Dunno why I gave you that bio, senior moment I guess........will keep eyes peeled on benders, thanks a ton.
    Geezer
    Power Mig 255C
    185 TIG
    Blue 175 MIG
    Ranger 8 Kohler 20HP
    1974 5K Lincoln/Wisconsin Powered (Cherry)
    Victor/Harris O/A
    K 487 Spool Gun

  17. Likes William McCormick liked this post
  18. #35
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,294
    Post Thanks / Like

    Re: Fab School

    Geezer.

    PM sent.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  19. #36
    Join Date
    Mar 2007
    Location
    MidWest
    Posts
    594
    Post Thanks / Like

    Re: Fab School

    PM answered
    Geezer
    Power Mig 255C
    185 TIG
    Blue 175 MIG
    Ranger 8 Kohler 20HP
    1974 5K Lincoln/Wisconsin Powered (Cherry)
    Victor/Harris O/A
    K 487 Spool Gun

  20. #37
    Join Date
    Sep 2014
    Posts
    2,372
    Post Thanks / Like

    Re: Fab School

    Every now and then my boss would make a wild-looking lambs tongue kind of like the image I included. But to be honest, it looked like something that would catch a jacket pocket or pocketbook strap, so I tended to avoid making them that pronounced.

    Just once he put a kink in the lamb's tongue it looked a little too lifelike and creepy to me. But definitely realistic.

    Name:  lambstongue.png
Views: 720
Size:  9.1 KB

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  21. #38
    Join Date
    Jan 2015
    Posts
    33
    Post Thanks / Like

    Re: Fab School

    Awesome I learned a lot thanks

    Sent from my SM-G930V using Tapatalk

  22. #39
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    9,894
    Post Thanks / Like

    Re: Fab School

    I have ask about Fabrication
    Take a good drafting class.
    It show how too and the rule of thumb. It also helps in shop for layout the parts is can be lot of drafting on parts.

    Dave

  23. Likes William McCormick liked this post
  24. #40
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,294
    Post Thanks / Like

    Re: Fab School

    Here is my latest handrails with lamb’s tongues I bent per Phil’s instructions. I got metal delivered last Friday and installed today (1 week later). My powder coater rushed them for me.

    I thought they turned out well and Customer was very happy.


    Name:  BD7CF1B5-A6FF-406E-BB59-7F7F8BB20365.jpg
Views: 759
Size:  369.1 KB

    Name:  C98F2AAD-1CBE-4702-8599-2F34D9AD756E.jpeg
Views: 718
Size:  179.7 KB
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  25. Likes William McCormick liked this post
  26. #41
    Join Date
    Mar 2007
    Location
    MidWest
    Posts
    594
    Post Thanks / Like

    Re: Fab School

    Quote Originally Posted by wb4rt View Post
    Here is my latest handrails with lamb’s tongues I bent per Phil’s instructions. I got metal delivered last Friday and installed today (1 week later). My powder coater rushed them for me.

    I thought they turned out well and Customer was very happy.


    Name:  BD7CF1B5-A6FF-406E-BB59-7F7F8BB20365.jpg
Views: 759
Size:  369.1 KB

    Name:  C98F2AAD-1CBE-4702-8599-2F34D9AD756E.jpeg
Views: 718
Size:  179.7 KB
    Well Burt you are on a roll. I bet the customer liked the lambs tongue, makes a job look complete with nice lines. I assume you welded the landing cap to the stair cap?? Looks like a fer piece past 8ft.
    Geezer
    Power Mig 255C
    185 TIG
    Blue 175 MIG
    Ranger 8 Kohler 20HP
    1974 5K Lincoln/Wisconsin Powered (Cherry)
    Victor/Harris O/A
    K 487 Spool Gun

  27. Likes William McCormick liked this post
  28. #42
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,294
    Post Thanks / Like

    Re: Fab School

    Quote Originally Posted by geezer View Post
    Well Burt you are on a roll. I bet the customer liked the lambs tongue, makes a job look complete with nice lines. I assume you welded the landing cap to the stair cap?? Looks like a fer piece past 8ft.
    Actually the cap is one piece - about 11’ total. Saved trying to blend the cap which takes time and I never do well enough to not show.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  29. Likes William McCormick, geezer liked this post
  30. #43
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,294
    Post Thanks / Like

    Re: Fab School

    I sent Phil a PM, but maybe someone else can advise me about using cast iron spears on a gate project. How do I weld them? Just regular MIG or is a special wire required or ? Any advise is appreciated. I will be using 1/2” square pickets.

    Also any design suggestions to match/coordinate with my rails in this other thread — starting post #59 — https://weldingweb.com/vbb/threads/7...-choices/page2

    Here is my initial design:
    (Sorry about the orientation)

    Name:  295047C8-F9D0-490A-870E-1D159119CA78.jpg
Views: 522
Size:  91.4 KB
    Last edited by wb4rt; 04-16-2021 at 06:19 PM.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  31. #44
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,294
    Post Thanks / Like

    Re: Fab School

    Well, customer had another idea. Here is more of what he wants.

    Name:  373F71B1-B696-4D52-ACF6-3AB39B3B420A.jpg
Views: 497
Size:  135.8 KB

    (I can never get the pictures to post right, no matter how I orient the camera.)
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  32. #45
    Join Date
    Mar 2007
    Location
    MidWest
    Posts
    594
    Post Thanks / Like

    Re: Fab School

    Hey Burt, how did your gate project wind up? Kinda like this last design.
    Geezer
    Power Mig 255C
    185 TIG
    Blue 175 MIG
    Ranger 8 Kohler 20HP
    1974 5K Lincoln/Wisconsin Powered (Cherry)
    Victor/Harris O/A
    K 487 Spool Gun

  33. #46
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,294
    Post Thanks / Like

    Re: Fab School

    Quote Originally Posted by geezer View Post
    Hey Burt, how did your gate project wind up? Kinda like this last design.
    Pretty good for me. Customer really likes it. Took a lot of planning and measuring to get it right.

    Name:  63E7553C-6294-4C5C-98F2-7919CF4E977D.jpg
Views: 411
Size:  247.7 KB

    Name:  9C94D620-9C1B-4273-AC83-83F2A6014BCB.jpg
Views: 386
Size:  188.7 KB
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  34. Likes William McCormick, ccogg liked this post
  35. #47
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,294
    Post Thanks / Like

    Re: Fab School

    Now I have a question on a potential new project.

    Anybody done an inside rail like this? Any hints or tips on how to do it?

    Name:  3307AC1B-1F0F-44E9-A1D3-49FFAA67A4EC.jpg
Views: 402
Size:  105.7 KB

    The designer wants a steel cap instead of wood.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  36. #48
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,801
    Post Thanks / Like

    Re: Fab School

    Quote Originally Posted by wb4rt View Post
    Now I have a question on a potential new project.

    Anybody done an inside rail like this? Any hints or tips on how to do it?

    Name:  3307AC1B-1F0F-44E9-A1D3-49FFAA67A4EC.jpg
Views: 402
Size:  105.7 KB

    The designer wants a steel cap instead of wood.
    I've done that with square pickets

    It's challenging lemme see if i can find a picture

    Sent from my SM-G973U using Tapatalk

  37. #49
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,294
    Post Thanks / Like

    Re: Fab School

    Hi Phil.

    There are two parts to be made. One is only 6 open steps and the other is a balcony rail. I think if I make a template of the steps I will be able to get the pitch and picket lengths. The flat run should be pretty straightforward. She wants round pickets and molded cap.

    My main questions before I take on this job is how to anchor the posts and the pickets in the wood tread?
    Do you oversized the holes for the pickets or tight fit?
    Do you use adhesive/epoxy for pickets?
    Do posts use mounting plates?
    What size post would be required (1 1/2 x 1 1/2)?

    Any help based on your experience is very much appreciated?
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  38. #50
    Join Date
    Sep 2014
    Posts
    2,372
    Post Thanks / Like

    Re: Fab School

    Quote Originally Posted by wb4rt View Post
    Hi Phil.

    There are two parts to be made. One is only 6 open steps and the other is a balcony rail. I think if I make a template of the steps I will be able to get the pitch and picket lengths. The flat run should be pretty straightforward. She wants round pickets and molded cap.

    My main questions before I take on this job is how to anchor the posts and the pickets in the wood tread?
    Do you oversized the holes for the pickets or tight fit?
    Do you use adhesive/epoxy for pickets?
    Do posts use mounting plates?
    What size post would be required (1 1/2 x 1 1/2)?

    Any help based on your experience is very much appreciated?
    I am sharing some ways I have done them, a lot of the reasons I did them in different ways was the tools I had to work with. And what was important or whether or not I had woodworking equipment.

    If you are set up for it you can use a hanger bolt with a machine thread head into the stairs for a blind install. Then tap each vertical on one end to accept the machine thread. Unless you can get access underneath the treads then you can just drill a clearing hole and bolt them in. That is best. If you are going to tap the verticles and you do not have a lathe, you should make a jig to drill them.

    Dado the bottom of the wooden rail to whatever the width and thickness of the flange you make for the top of the verticles, it can be a 1"x 3" x 1/8" flange. Offset the flange so that the side of the flange that is higher is overhung just enough to get the screw into the flange without hitting the vertical on the obtuse angle side. Then the difficult side that is blocked by the verticle because of the acute angle can be easily worked on. Just small #10 or #12 wood screws, 3/4" to 1" long to fasten the flanges to the handrail, pre-drill especially in hardwood. If you create a deep dado you do not even have to have each flange bottom out in the dado, if one or two on each steep do not reach the rail it will not matter.

    Another way to do it, you can also take a Forstner bit the exact size of the verticle and drill each vertical into the step just 3/16" deep, to give you some adjustment in case, when you set the rail with the verticles already mounted to the rail, you find a step or two are on an odd angle. The Forstner bit will leave a center indent that you can drill a pilot hole for the hanger bolt.

    You can also just grind down the verticle because the thread will be deeper than the steel hanger bolt so it will not bottom out if you feel you want to get them all to hit the inside of the dado in the handrail or if there is no Dado and you cannot create one.

    If you can get under the steps just drill and bolt them in.

    Sincerely,

    William McCormick
    Last edited by William McCormick; 08-24-2021 at 10:49 PM.
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,266,509.26724 seconds with 19 queries