    I was finally able to lay down a stack of dimes!

    Name:  5A1D7C58-E78F-4AE3-B23A-261A1462211B.jpeg
Views: 1313
Size:  110.2 KB


    lol.
    Miller Trailblazer Pro 350D
    Miller Suitcase MIG
    Miller Spectrum 2050
    Miller Syncrowave 250DX
    Lincoln 210MP

  2. #2
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,607
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    That'll cost ya'

  3. Likes 12V71, scsmith42 liked this post
  4. #3
    Join Date
    Dec 2016
    Posts
    280
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    no way you got that with this tunsgten point

  5. Likes scsmith42 liked this post
  6. #4
    Join Date
    Nov 2012
    Posts
    3,046
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    What were your settings???

  7. #5
    Join Date
    Jul 2009
    Location
    western north carolina
    Posts
    78
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    Looks like you need to adjust your angle a little bit

  8. #6
    Join Date
    May 2018
    Location
    the Netherlands
    Posts
    237
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    No wetting at the toes.
    Kemppi minarc 150
    Esab powercut 400

  9. #7
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,607
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    I wish I could weld that good... then maybe this hitch could be saved, it just has a couple cracks I think I can mig it with some 030 fluxcore I'l let you know how it goes...
    Name:  trailerhitch-weld2.JPG
Views: 782
Size:  274.8 KB

  10. Likes 12V71 liked this post
  11. #8
    Join Date
    Apr 2006
    Location
    Outside of Raleigh, NC
    Posts
    1,121
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    Wow, that trailer must have a LOT of miles on it to have worn out the inside of the ball socket that badly.
    Miller Trailblazer Pro 350D
    Miller Suitcase MIG
    Miller Spectrum 2050
    Miller Syncrowave 250DX
    Lincoln 210MP

  12. #9
    Join Date
    Oct 2016
    Location
    Delavan WI
    Posts
    506
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    Grease your ball or balls, if you have several.

  13. #10
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    7,260
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    Quote Originally Posted by scsmith42 View Post
    Name:  5A1D7C58-E78F-4AE3-B23A-261A1462211B.jpeg
Views: 1313
Size:  110.2 KB


    lol.
    And you did it left handed! Did you really go get a roll of dimes just for that photo?

    On steel, try Hastelloy, or ever 308L, you'll love the weld shape. Expensive stuff, but pretty.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  14. Likes ronsii, scsmith42 liked this post
  15. #11
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,607
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    Quote Originally Posted by scsmith42 View Post
    Wow, that trailer must have a LOT of miles on it to have worn out the inside of the ball socket that badly.
    Yeah it's about 10 years old, get s a *lot* of heavy miles

    The balls go get greased but I think that is just part of the issue as there is always dirt/sand/concrete on everything and it just sticks to the grease... and lets face it nobody wants to clean a dirty ball off just before hitching up

  16. #12
    Join Date
    Jun 2020
    Location
    Texas
    Posts
    8
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    Quote Originally Posted by scsmith42 View Post
    Name:  5A1D7C58-E78F-4AE3-B23A-261A1462211B.jpeg
Views: 1313
Size:  110.2 KB


    lol.

    You should post a YouTube tutorial. I always have the hardest time getting Roosevelt's hair just right. I think it's not enough heat, but every time I turn up the heat, he ends up with a nappy fro.

  17. Likes scsmith42 liked this post
  18. #13
    Join Date
    Apr 2006
    Location
    Outside of Raleigh, NC
    Posts
    1,121
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    Quote Originally Posted by Willie B View Post
    And you did it left handed! Did you really go get a roll of dimes just for that photo?

    On steel, try Hastelloy, or ever 308L, you'll love the weld shape. Expensive stuff, but pretty.
    I recently ordered some Hasteloy W for a project and am looking forward to trying it out.
    Miller Trailblazer Pro 350D
    Miller Suitcase MIG
    Miller Spectrum 2050
    Miller Syncrowave 250DX
    Lincoln 210MP

  19. #14
    Join Date
    Nov 2012
    Posts
    3,046
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    Quote Originally Posted by scsmith42 View Post
    I recently ordered some Hasteloy W for a project and am looking forward to trying it out.
    If I never have to weld Hastelloy again, it will still be too soon.

  20. #15
    Join Date
    Oct 2014
    Posts
    3,243
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    Forget dimes, I want to see a stack of silver dollars! Teacher in school did a lot of specialty Tig and said Monel was tricky to weld because it had the consistency of butter when it was hot.

  21. Likes scsmith42 liked this post
  22. #16
    Join Date
    Nov 2012
    Posts
    3,046
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!

    Not hardly, more like trying to weld clay. Better put it where you want it, because wherever you put it, that's where it's gonna stay. All the high nickel alloys are like that.

  23. #17
    Join Date
    Apr 2010
    Posts
    2,938
    Post Thanks / Like

    Re: I was finally able to lay down a stack of dimes!


    scsmith42


    Did the burn of the 'cellulose wrap' provide enough ambient Oxygen
    displacement - or did you have to augment with cover gas ?

    And, where is your 'run-off' ledge . . . ?


    Quote Originally Posted by TimmyTIG View Post
    . . . Better put it where you want it, because wherever you put it,
    that's where it's gonna stay . . .
    Building on TimmyTIG's experience, [for the arm chair welder] Nickel
    is not a five cent metal
    - it produces super alloys. Nickel maintains
    structural integrity to 80%+ of its melting point. This is the metal of
    Nukes and Jet Turbine fins [research Hastelloy on your own].

    In short - Nickel refuses to conduct heat . . .

    Common Stainless [low nickel content] warps, 4 to 6 X compared to
    mild steel . . . because, heat is not wicked away . . .

    hth


    Opus

  24. Likes scsmith42 liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,614,524,778.11396 seconds with 14 queries