Hi all, rescued a sad ranger 8, from an estate, along with another pile of dead power equipment. It had been sitting 5 plus years...varnish gas, mouse nests etc. I've been tinkering with it in my free time.
Got it running, and runs great considering the old gas in it. No power to the ignition coil so I jumpered it off the battery. At first I had zero output from everything. Cleaned the commutater with sand paper, and now we have 110v, but still no welding power. What would you check next?