    In the middle of a big fence project and tired of buying 10 lb boxes of Washington Alloy 6010 from LWS and not willing to fork over $180 for a 50 lb can of Lincoln. Found a deal online for 50 lb of ESAB Sureweld 6010 for $94. Are these decent rods? I don’t need X-ray quality, just for high school boys to run on pipe fence.


    Sent from my iPhone using Tapatalk

  2. #2
    Join Date
    Nov 2012
    Posts
    3,274
    Post Thanks / Like

    Re: ESAB Sureweld 6010

    I have never run their 6010, but their 7018 has always been great.

  3. #3
    Join Date
    Apr 2017
    Posts
    43
    Post Thanks / Like

    Re: ESAB Sureweld 6010

    Just a thought, if this is for a school, you may be able to get some samples from ESAB. That would allow you to try some before you commit to an order.

  4. #4
    Join Date
    Mar 2018
    Posts
    78
    Post Thanks / Like

    Re: ESAB Sureweld 6010

    Quote Originally Posted by pprobus View Post
    Just a thought, if this is for a school, you may be able to get some samples from ESAB. That would allow you to try some before you commit to an order.
    No school. I just hired some high school boys for the summer.


    Sent from my iPhone using Tapatalk

  5. #5
    Join Date
    Oct 2014
    Posts
    5,270
    Post Thanks / Like

    Re: ESAB Sureweld 6010

    I recall CEP really liked Esab Sureweld 10P 6010 and said it runs the best on an inverter. 6010 can be a challenge on some inverters so I'd say you should be good.
    Last edited by Welder Dave; 07-10-2020 at 01:59 AM.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,278,436.54706 seconds with 17 queries