    Mig Max 215

    when using c25 is the gas flow supposed to shut off immediately after you release the trigger or should it flow for a second or two before shutting off.
    Thanks
    candyman

  2. #2
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,553
    Post Thanks / Like

    Re: Mig Max 215

    Quote Originally Posted by candyman View Post
    when using c25 is the gas flow supposed to shut off immediately after you release the trigger or should it flow for a second or two before shutting off.
    Thanks
    Typically shuts off when the arc does. Would not bother me for a second or 2 of post flow though to keep the wire stub clean.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig4ea,MigMax1ea.

  3. #3
    Join Date
    Jul 2016
    Location
    Midwest
    Posts
    405
    Post Thanks / Like

    Re: Mig Max 215

    Most of the smaller machines have a couple second post flow now days. It's designed for those who weld stainless. Nothing hurt on the other processes except a few cents worth of gas out of every tank. Also if your burn back isn't turned up more than needed, Post flow can help keep the wire ball to a minimum.
    Thermal Arc 320SP ( Lorch )
    Cobra Pythons
    Thermal Arc 300 AC/DC ( Sanrex )
    ESAB 301i AC/DC ( Lorch )
    Thermal Arc 161STL ( WTL )
    Thermal Arc 190S ( Sanrex )
    Cut Master 82, 42. Cut45 ( WTL )
    Victor Gas Apps.
    Boxes and boxes of welding crap.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,490,265.62102 seconds with 13 queries