    iMIG 230i thin metal

    I ask this in general terms, not trying to do the absolute thinnest possible. :-)

    Got a iMIG 230i and haven’t been able to get everything setup and going yet, getting close.

    Out of curiosity, using Lincoln L-56 .030 wire, 75/25 gas what’s the thinnest practical metal can weld?

    I realize can get .023 wire and it would be better for thin metal, just wondering with what I have, the thinnest practical metal is. And I know that an experienced/skilled welder can weld thinner stuff than I can.

    Thinking more along the lines of fixing/repairing small things that need little welding done. When don’t want to change wire and do simple repairs and such. Not welding car body panels or something that needs to have nice looking welds.

    Again, just general question, not the absolute thinnest etc

    When I get it going shortly I’ll try and see what I can do, but thought I’d ask.

    Cheers, Allen

  2. #2
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: iMIG 230i thin metal

    Probably around 22 gauge. But on average 20 gauge.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  3. #3
    Join Date
    Nov 2014
    Posts
    47
    Post Thanks / Like

    Re: iMIG 230i thin metal

    That’s pretty impressive, didn’t realize it would work on that thin of metal with .030 wire. Anxious to get it going and start welding with it.

  4. #4
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: iMIG 230i thin metal

    Adjustable inductance makes a world of difference.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,300,583.75706 seconds with 19 queries