    miller deltaweld 650

    I recently purchased a deltaweld 650 from a tech school. When I go to weld with it, the wire is hot WITHOUT the trigger pulled and as soon as the trigger is pressed the wire feeds thru like normal but without any current to weld. Can anyone give me an idea of where to start troubleshooting this issue? thanks

  2. #2
    Join Date
    Dec 2013
    Posts
    1,499
    Post Thanks / Like

    Re: miller deltaweld 650

    Is the remote contactor switch turned on? The manual says "When the remote contactor switch is in the "ON" position, open circuit voltage is present at both positive weld output terminals for as long as the welding power source is energized."

    Page 19 of the manual I looked at.

    Find it here:https://www.millerwelds.com/support/manuals-and-parts
    ---Meltedmetal

  3. #3
    Join Date
    Jul 2020
    Posts
    2
    Post Thanks / Like

    Re: miller deltaweld 650

    Both are in the off position

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,596,653,952.46594 seconds with 13 queries