    Contact Tip and Nozzle Lengths Question

    Do they make different length nozzles and/or tips? On mine, the tip is recessed in about 1/4". Seems like if the tip were more flush to the nozzle end I would have a little better visibility when using .023 wire. The nozzle is so close to the work piece it's hard for me to get a good sight on the puddle and/or wire.

    I use the 5/8" ones that fit in the Lincoln Magnum 100L style guns. Just wondering.

    Name:  IMG_20200731_213515-01.jpg
Views: 226
Size:  83.7 KB

    Name:  IMG_20200731_213539-01.jpg
Views: 228
Size:  97.4 KB
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    I'm a HOBBYIST, not a structural welder (Duh!)
    I do Yard Art, NOT Trailers

  2. #2
    Join Date
    Oct 2014
    Posts
    2,187
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    Looks like a KP21-50-F nozzle is flush. Just make sure it's a Magnum 100L and not a Magnum Pro 100L.

    https://images.homedepot-static.com/...56c9227002.pdf
    Last edited by Welder Dave; 4 Days Ago at 01:37 AM.

  3. Likes Shootr liked this post
  4. #3
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    4,938
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    BTW, either your contact tip is severely worn out, or its the wrong size.
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

  5. Likes Shootr liked this post
  6. #4
    Join Date
    May 2020
    Location
    Arizona
    Posts
    203
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    Quote Originally Posted by Oscar View Post
    BTW, either your contact tip is severely worn out, or its the wrong size.
    Name:  IMG_20200801_072449-01.jpg
Views: 207
Size:  94.1 KB

    Arrrrgh...wrong tip ...Must be awesome to have good eyes! Grassy ***.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    I'm a HOBBYIST, not a structural welder (Duh!)
    I do Yard Art, NOT Trailers

  7. #5
    Join Date
    May 2020
    Location
    Arizona
    Posts
    203
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    Quote Originally Posted by Welder Dave View Post
    Looks like a KP21-50-F nozzle is flush. Just make sure it's a Magnum 100L and not a Magnum Pro 100L.

    https://images.homedepot-static.com/...56c9227002.pdf
    Awesome - thanks for posting this Between having the correct contact tip in it and a flush nozzle - be interesting to see how things change/improve.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    I'm a HOBBYIST, not a structural welder (Duh!)
    I do Yard Art, NOT Trailers

  8. #6
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    4,938
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    Welcome. You can always slice off the needed amount off the old nozzle if you can spare it. For 023 wire, might even be best to have it protrude 1/16"-1/8".
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

  9. Likes Shootr liked this post
  10. #7
    Join Date
    May 2020
    Location
    Arizona
    Posts
    203
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    Quick update: Sliced off a bit of the existing nozzle (have 3 spares) to get it flush with the (correct) .023 tip.

    Name:  IMG-20200802-085031-01.jpg
Views: 146
Size:  123.6 KB

    Probably need to turn up the gas flow a touch, but bottle ran dry after 5 beads (was at 20CF/H). Visibility is better and I think I can tell where the fine tuning still needs work. Moving the gun more smoothly, watching the stick out distance better, angle of the gun, etc.

    On this one, if I were to self-critique, looks like the toes on the bottom horizontal piece weren't quite wetted(?). Maybe the wire angle/direction was favoring the vertical piece a little?
    Name:  IMG-20200802-084410-01-01.jpg
Views: 147
Size:  100.8 KB

    This one, not sure what the occlusions are from. Maybe gas running low.
    Name:  IMG-20200802-084439-01.jpg
Views: 146
Size:  92.0 KB

    So, starting to get comfortable in this position - only a zillion left to go...
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    I'm a HOBBYIST, not a structural welder (Duh!)
    I do Yard Art, NOT Trailers

  11. #8
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    4,938
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    Don't assume it's all technique. There is such a thing as incorrect MIG settings, but overall looks good from here. You have to be able to describe the big picture in order to see the big picture. Also, are you using CO2 or C25 ?
    Last edited by Oscar; 3 Days Ago at 12:45 PM.
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

  12. #9
    Join Date
    May 2020
    Location
    Arizona
    Posts
    203
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    Quote Originally Posted by Oscar View Post
    Don't assume it's all technique. There is such a thing as incorrect MIG settings, but overall looks good from here. You have to be able to describe the big picture in order to see the big picture. Also, are you using CO2 or C25 ?
    The settings were: C25 at 20CF/H, 125A at 23.5V, .023 solid wire.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    I'm a HOBBYIST, not a structural welder (Duh!)
    I do Yard Art, NOT Trailers

  13. #10
    Join Date
    Oct 2014
    Posts
    2,187
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    Your gas flow is fine but get some nozzle dip to prevent spatter from sticking. Spatter build up can cause problems, especially when it decides to let go into the puddle. Looks like your travel speed could be a little faster. On a proper size fillet weld the leg length (distance from inside corner to edge of weld) should be equal to the thickness of the thinner plate. If both plates are 1/8", the weld should 1/8" out from the corner and 1/8" up from the corner. If the plates were different thicknesses the leg only has to equal the thinner plate. You could try slowly twisting your wrist side to side to wash the edges of the puddle in. Below are some examples of nozzle dip. Cooter Snot seems like you pay a lot for the name.

    https://www.amazon.com/Best-Welds-We.../dp/B01LW3SXZ0

  14. Likes Shootr liked this post
  15. #11
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    4,938
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    Quote Originally Posted by Shootr View Post
    The settings were: C25 at 20CF/H, 125A at 23.5V, .023 solid wire.
    125A is bordering on the limit of what 023 diameter wire can carry AFAIK. For anything over 70A or so, I'd suggest 030 wire. Don't get me wrong, you can obviously run 023 wire up into the higher WFS ranges, but there come a point where the wire will no longer carry any more amperage so you might not get the proper toe-fusion you are looking for. Since the wire will no longer carry anymore amperage, the metal deposition will still be there, but it will be missing heat from the [missing] amperage, and you can't compensate with more voltage because you'll just get tons of spatter. Just my take from my observations.
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

  16. Likes Shootr liked this post
  17. #12
    Join Date
    Jul 2018
    Location
    Beavercreek, Ohio
    Posts
    221
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    I've been using this anti spatter.....on my table, weldment and mig nozzle.....works well.

    I use it in a small spray bottle.

    https://www.amazon.com/Simple-Green-...6459770&sr=8-1
    Gregg
    Hobart Handler 210 MVP
    Hobart Stickmate 210i

  18. #13
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    4,938
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    Quote Originally Posted by Rangerhgm View Post
    I've been using this anti spatter.....on my table, weldment and mig nozzle.....works well.

    I use it in a small spray bottle.

    https://www.amazon.com/Simple-Green-...6459770&sr=8-1
    I didn't even know Simple Green made that! Is it a gel or a regular liquid?
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

  19. #14
    Join Date
    Jul 2018
    Location
    Beavercreek, Ohio
    Posts
    221
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    It's a thin clear liquid. I put it in small plastic spray bottle and use it to spray the table, weldment and nozzle. It's worked well for me, and a gallon will last a loooong time.
    Gregg
    Hobart Handler 210 MVP
    Hobart Stickmate 210i

  20. #15
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,235
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    In regards to anti-spatter, Fireball tools tested over 40 products in this video.



    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  21. #16
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    4,938
    Post Thanks / Like

    Re: Contact Tip and Nozzle Lengths Question

    Nevermind, lol.
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

  22. Likes Shootr liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,596,653,173.54858 seconds with 14 queries