Page 2 of 2 FirstFirst 12
Results 26 to 29 of 29

Thread: If a 30a breaker eventually trips, how much extra would 40a go?

  1. #26
    Join Date
    Dec 2007
    Location
    Los Angeles
    Posts
    7,823
    Post Thanks / Like

    Re: If a 30a breaker eventually trips, how much extra would 40a go?

    I think there is a time chart for Circuit Breakers as to how much "more" they can handle for a certain time before opening.
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Miller 125c Plasma 120v
    SO 2020 bender
    Beer in the fridge

  2. #27
    Join Date
    Oct 2014
    Posts
    915
    Post Thanks / Like

    Re: If a 30a breaker eventually trips, how much extra would 40a go?

    Give it 33% more input amps then it will be close to 33% more than the output amps it had before. The benefit would be mostly linear I believe.

  3. #28
    Join Date
    Jul 2020
    Posts
    257
    Post Thanks / Like

    Re: If a 30a breaker eventually trips, how much extra would 40a go?

    I was able to run 3x 1/8" 6011's back to back at ~115 amps, no pop on the breaker.

    I got through 1-1/2 5/32" 6011's at ~130 amps and the breaker popped.

    The 3x 1/8" 6011's at ~115 amps is a pretty good indicator for me. That should be plenty of welding power. Any of the thick steel I'll weld would be short pieces that would likely be less than 1 rod would give me anyway, just perhaps multi-pass (cleaning between passes = some cool down time anyway). I may even be able to run some 5/32" in some fab also, but that would be pushing it. We'll see.

    Here is a video on the results.


  4. #29
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    1,847
    Post Thanks / Like

    Re: If a 30a breaker eventually trips, how much extra would 40a go?

    If run new wire it only the cost of the wire. Even plug and breaker is same price.

    Dave

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,604,031,771.25614 seconds with 13 queries