Re: Powercut 1300 Help.
Originally Posted by
Torhino
I was cutting with it tonight it was working like a champ then it stopped. Showed E21 PIP No Continuity. Replaced nozzle and electrode. Checked air at 80 psi. Still does not work. I have air coming out of torch on power on. The air stops and then the E21 code comes back. Anyone have any ideas?
Thanks,
Todd
PIP is parts in place. Usually means that the consumables aren't seated or tightened properly or, The little plunger safety switch that gets pushed in when the nozzle gets tightened isn't pushed in far enough. Good luck.
Thermal Arc 320SP ( Lorch )
Cobra Pythons
Thermal Arc 300 AC/DC ( Sanrex )
ESAB 301i AC/DC ( Lorch )
Thermal Arc 161STL ( WTL )
Thermal Arc 190S ( Sanrex )
Cut Master 82, 42. Cut45 ( WTL )
Victor Gas Apps.
Boxes and boxes of welding crap.