    Powercut 1300 Help.

    I was cutting with it tonight it was working like a champ then it stopped. Showed E21 PIP No Continuity. Replaced nozzle and electrode. Checked air at 80 psi. Still does not work. I have air coming out of torch on power on. The air stops and then the E21 code comes back. Anyone have any ideas?

    Thanks,

    Todd

  2. #2
    Join Date
    Jul 2016
    Location
    Midwest
    Posts
    404
    Post Thanks / Like

    Re: Powercut 1300 Help.

    Quote Originally Posted by Torhino View Post
    I was cutting with it tonight it was working like a champ then it stopped. Showed E21 PIP No Continuity. Replaced nozzle and electrode. Checked air at 80 psi. Still does not work. I have air coming out of torch on power on. The air stops and then the E21 code comes back. Anyone have any ideas?

    Thanks,

    Todd
    PIP is parts in place. Usually means that the consumables aren't seated or tightened properly or, The little plunger safety switch that gets pushed in when the nozzle gets tightened isn't pushed in far enough. Good luck.
    Thermal Arc 320SP ( Lorch )
    Cobra Pythons
    Thermal Arc 300 AC/DC ( Sanrex )
    ESAB 301i AC/DC ( Lorch )
    Thermal Arc 161STL ( WTL )
    Thermal Arc 190S ( Sanrex )
    Cut Master 82, 42. Cut45 ( WTL )
    Victor Gas Apps.
    Boxes and boxes of welding crap.

  3. #3
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    3,609
    Post Thanks / Like

    Re: Powercut 1300 Help.

    E21, if new tip and electrode in torch don't help.
    Do a continuity check on torch lead. make sure no leads are broken.
    If torch lead is good. then you might be looking at a new pilot arc IGBT.
    Hopefully there is not a problem with the control pcb that drives the IGBT.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,252,486.81111 seconds with 13 queries