    I have the 301 and I know that several on here have the 200. My question is, What does the 201 offer for AC Hz option at 200 amps? Is it 200 or 100? or. Also with the 201 does your AC Hz depend on amperage selected or do you get full AC Hz range no matter what high amperage you select.
    Thanks.
    Thermal Arc 320SP ( Lorch )
    Cobra Pythons
    Thermal Arc 300 AC/DC ( Sanrex )
    ESAB 301i AC/DC ( Lorch )
    Thermal Arc 161STL ( WTL )
    Thermal Arc 190S ( Sanrex )
    Cut Master 82, 42. Cut45 ( WTL )
    Victor Gas Apps.
    Boxes and boxes of welding crap.

  2. #2
    Join Date
    Jul 2016
    Location
    Midwest
    Posts
    405
    Post Thanks / Like

    Re: ESAB Lorch AC/DC

    The reason I ask is I just acquired yet another tig unit but it will only do 100 AC Hz at 200 amps but will do 250 Hz at 100 amps. Not sure this is normal. May have something to do with duty cycle some how but I'm not seeing how.
    Thermal Arc 320SP ( Lorch )
    Cobra Pythons
    Thermal Arc 300 AC/DC ( Sanrex )
    ESAB 301i AC/DC ( Lorch )
    Thermal Arc 161STL ( WTL )
    Thermal Arc 190S ( Sanrex )
    Cut Master 82, 42. Cut45 ( WTL )
    Victor Gas Apps.
    Boxes and boxes of welding crap.

  3. #3
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    935
    Post Thanks / Like

    Re: ESAB Lorch AC/DC

    My Lorch handytig 200, which is a cut-down T series, does 200hz at all amps. I would have thought it should do the full range whatever the amps, for all lorch based models, they're very good for duty cycle.

    It will also do some very funky things when you apply a high frequency pulse on top of AC... e.g. a 400hz pulse on a 200hz AC wave Their inverter cores are very versatile that way.
    Last edited by Munkul; 08-19-2020 at 03:56 AM.

  4. Likes Rondo liked this post
  5. #4
    Join Date
    Jan 2005
    Posts
    4,140
    Post Thanks / Like

    Re: ESAB Lorch AC/DC

    The Caddie tig was similar in freq response, but not quite so radical ini operation . The 200 hz is available at all ac amps with the Lorch/Esab machines..(AKA Sanrex style)
    Esab/Lorch ET-220i
    Esab 160i caddy
    Thermal LM-200 Lincoln feeders
    Thermal Pee-Wee 85s
    Thermal 60i- 3phase /RPC powered (Beast)
    Thermal Drag-gun 35C
    INE 1500
    Klutch 140i

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,622,980.24611 seconds with 12 queries