    Tig welding aluminum air line/piping

    Hello all ,

    Ua local 10 welder/fitter .

    I have a job coming up . 700 ft of sch 40 2 inch , 1 inch welded aluminum air line . Most will be done in position. Tie ins eithier threaded or out of position is minimal ..

    I'm pretty proficient with sch 5 /10 stainless and duplex , inconel , nickel , heavy wall steam tig and stick . But i havent welded aluminum in years , and to be honest not even sure I can cut the cheese. None of this will xray type stuff but it obviously needs to be quality for 200 psi of air.


    Any suggestions for anyone who has welded any socket type aluminum piping . Is there anything I can work on to help me.

    Sent from my SM-G973U using Tapatalk

  2. #2
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    501
    Post Thanks / Like

    Re: Tig welding aluminum air line/piping

    Most of my experience with the aluminum is on the bench. I weld sch40 sockets into sch 10 for pressure gauges, adding elbows, and bungs, mostly low pressure stuff. If you can do sch 10 stainless in position, I would think a little practice is all you'll need. I find doing the stainless sch 10 more challenging, aluminum seems more forgiving to me. Especially sch 40 socket welds, the 1" might be a little trickier because of the tight radius. Is this going to be TIG welding, and is it up in the air/ceiling ? After a little practice you'll be OK, when your almost finished you'll be great. Then you won't do one again for a couple of years.

    Best of luck

    ps post pic if you can, unless its a Navy/CG job or something where its not allowed.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D

  3. #3
    Join Date
    Aug 2019
    Location
    northeastern PA.
    Posts
    83
    Post Thanks / Like

    Re: Tig welding aluminum air line/piping

    Do a some practice and get yourself tuned. YOU GOT THIS !!!

  4. #4
    Join Date
    Mar 2010
    Location
    East Tennessee
    Posts
    1,234
    Post Thanks / Like

    Re: Tig welding aluminum air line/piping

    Easy peasy. The machine will make a difference. My dynasty will eat it up. Aluminum out of position no big deal.
    Attached Images Attached Images  

  5. Likes l0w n slow liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,624,580.24004 seconds with 13 queries