    LN-8 and K114 Squirt Gun SUBARC Welding

    We have a DC600 power source and a LN8 feeder pushing 3/32" wire through a K114 SUBARC gun.
    We're having some issues with crappy welds due to varying arc length. The gun is clamped in fixture and the work is rotated on a positioner.
    I believe the feeder has to push way to hard to get the wire through the gun.
    Can anyone tell me how much force it should take to hand feed some 3/32" wire through the gun/hose/liner ?
    Can you do it by hand pushing or does it take a pair of visegrips clamped onto wire pushing with two hands?


    Just wondering!

  2. #2
    Join Date
    Oct 2014
    Posts
    5,270
    Post Thanks / Like

    Re: LN-8 and K114 Squirt Gun SUBARC Welding

    I think you should be able to push it by hand. I'm not sure if your gun has a replaceable liner but you could try blowing air through it. Being sub-arc I would guess it gets used a lot. If the drive rolls are a little tight (or lots of use) tiny bits of wire will flake off and can plug up the liner. Dry graphite spray in the liner could help too. A lot of flux-core wire has a graphite coating. That's why your hands get black when you handle it. Check the contact tip too and make sure there are no sharp bends in the gun cable.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,256,163.29194 seconds with 19 queries