+ Reply to Thread
Results 1 to 6 of 6

Thread: Licoln Weldanpower AC-225/DC-210-210/6 Idler Board Replacement

  1. #1
    Join Date
    Sep 2020
    Posts
    4
    Post Thanks / Like

    Lightbulb Licoln Weldanpower AC-225/DC-210-210/6 Idler Board Replacement

    Hello,

    I've been coming across these boards going bad semi regularly. Would anyone be interested in me making a new updated aftermarket replacement board? If anyone has the schematic, I would really appreciate it. I have a design, but would like to be able to finalize it and check my work. Thanks

    -Tyler
    Last edited by tbmusic; 09-04-2020 at 02:23 AM.

  2. Likes FlyFishn liked this post
  3. #2
    Join Date
    Sep 2014
    Location
    texas
    Posts
    298
    Post Thanks / Like

    Re: Licoln Weldanpower AC-225/DC-210-210/6 Idler Board Replacement

    I have two of these machines, both with the 16hp briggs, neither has CV taps. The idler board is not the same between the two. If you email Lincoln, they will send you the correct schematic...or least they sent them to me. I have no idea which drive I have them saved on. With my luck, they're on either my old desktop or old laptop, both of which are dead. Will have to check my backup drives to see if they're saved there. You might also check the lincoln site. Not sure, but I'm pretty sure I pulled up one or the other of them there at some point in the past.

  4. Likes tbmusic liked this post
  5. #3
    Join Date
    Sep 2020
    Posts
    4
    Post Thanks / Like

    Re: Licoln Weldanpower AC-225/DC-210-210/6 Idler Board L-6325 Replacement

    Quote Originally Posted by machinisttx View Post
    I have two of these machines, both with the 16hp briggs, neither has CV taps. The idler board is not the same between the two. If you email Lincoln, they will send you the correct schematic...or least they sent them to me. I have no idea which drive I have them saved on. With my luck, they're on either my old desktop or old laptop, both of which are dead. Will have to check my backup drives to see if they're saved there. You might also check the lincoln site. Not sure, but I'm pretty sure I pulled up one or the other of them there at some point in the past.
    My man, thank you! I'll get an email to them today

  6. #4
    Join Date
    Sep 2020
    Posts
    4
    Post Thanks / Like

    Re: Licoln Weldanpower AC-225/DC-210-210/6 Idler Board L-6325 Replacement

    Ok the design is finished and I can have them done in a week or two. I'll be listing them on ebay or you can message me here.

    https://www.ebay.com/itm/264859220287

  7. #5
    Join Date
    Dec 2014
    Location
    Wasilla, Alaska
    Posts
    205
    Post Thanks / Like

    Re: Licoln Weldanpower AC-225/DC-210-210/6 Idler Board L-6325 Replacement

    tbmusic, are your L-6325 boards for the CC or CC/CV machines?. Didn't see a reference in your post or ad. Thx.

  8. #6
    Join Date
    Sep 2020
    Posts
    4
    Post Thanks / Like

    Re: Licoln Weldanpower AC-225/DC-210-210/6 Idler Board L-6325 Replacement

    Quote Originally Posted by wasillashack View Post
    tbmusic, are your L-6325 boards for the CC or CC/CV machines?. Didn't see a reference in your post or ad. Thx.
    https://www.lincolnserviceparts.com/...COLN1/P138.pdf

    Per this manual, the Idler Board is the same. Let me know if you're seeing differently.

    The parts that do change between the two are . . . Flashing Diode Assem, Selector Switch, Rheostat, and Name Plate (Obviously)

    Thanks
    Last edited by tbmusic; 11-16-2020 at 12:29 PM. Reason: Forgot Link

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,246,780.26220 seconds with 20 queries