Thread: Aluminum Gate Installation

  1. #1
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    292
    Post Thanks / Like

    Aluminum Gate Installation

    Last fall I prepared detailed drawings for the driveway gate for my friend Scott, who is an engineer that I work with. Scott had previously designed the piers and arranged their construction. The piers are actually an armature of stainless steel, which goes about five feet deep into a footing. The bricks of the pier rest on the footing and are built up around the armature. The first picture shows my SolidWorks design of the gate assembly.

    1. Gate Assembly
    Name:  1. Gate Assembly.jpg
Views: 494
Size:  57.0 KB
    The second picture shows the gate leaf components.

    2. Gate leaf asm
    Name:  2. Gate leaf asm.jpg
Views: 499
Size:  50.6 KB

    The third picture shows the weld callouts for the gate leaf. The gate consists of 2" x 4" Aluminum tubing as well as three solid bocks that have tapped holes in them. The curved tube is bent the hard way and we couldn't find anyone willing and able to bend the tube in the Detroit area, so we had a company in Chicago bend it for us. I sent the design out to one of my company's local fabrication venders for welding, because I was concerned that the job was a little big for me and that my Dynasty 200 DX welder wouldn't have enough power to weld the heavy blocks, even with a Helium Argon mix.

    3. Gate leaf weld callouts
    Name:  3. Gate leaf weld callouts.jpg
Views: 489
Size:  52.8 KB

    I chose to use spherical bearings for the hinge bearings so that the bearings wouldn't fight each other if the pintles weren't perfectly aligned. I used a thrust bearing that had a concave recess that matched the diameter of the ball, so the thrust bearing would also accommodate misalignment.

    4. Spherical bearing and thrust washer
    Name:  4. Spherical bearing and thrust washer.JPEG
Views: 493
Size:  177.4 KB

    The pintles are 1" stainless steel with 1"-8 UNC threads on them. My design called for the pintles to be reverse bored as shown below to add a proper finish and to make the bearings fit in the blocks that had to mount to the 4" wide tubing.

    5. Spherical and thrust bearing
    Name:  5. Spherical and thrust bearing.jpg
Views: 484
Size:  42.3 KB
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  2. Likes ronsii liked this post
  3. #2
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    292
    Post Thanks / Like

    Re: Aluminum Gate Installation

    The next step was to do a dry run with all of the details to insure that we had all of the proper hardware and everything fit.

    6. Checking fit and our measurements
    Name:  6. Checking fit and our measurements.jpg
Views: 485
Size:  104.3 KB

    The first thing that we found is that the pintles bottomed out by hitting concrete before they were in the correct position, so I brought the pintles home and cut 1" off the end.

    7. Cutting down the pintles
    Name:  7. Cutting down the pintles.jpg
Views: 483
Size:  118.9 KB

    8. Pintles cut down
    Name:  8. Pintles cut down.jpg
Views: 494
Size:  171.4 KB

    This is a welding forum, so here are three pictures that the fabrication vender sent to me.

    9. Gate leaf weld
    Name:  9. Gate leaf weld.jpg
Views: 494
Size:  72.5 KB

    10. Leaf welded
    Name:  11. Gate leaf welded.jpg
Views: 485
Size:  79.1 KB
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  4. Likes ronsii liked this post
  5. #3
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    292
    Post Thanks / Like

    Re: Aluminum Gate Installation

    11. Gate leaf welded
    Name:  11. Gate leaf welded.jpg
Views: 485
Size:  79.1 KB

    I found that the pivot pin of the gate actuator wouldn't fit in the bore of the gate bracket because of the powder coat, so I brought home the gate brackets and reamed them with an adjustable reamer.

    12. Reaming off powder coat from bore
    Name:  12. Reaming off powder coat from bore.jpg
Views: 489
Size:  90.5 KB

    13. Testing pivot pin in reamed hole
    Name:  13. Testing pivot pin in reamed hole.jpg
Views: 489
Size:  55.8 KB

    14. Reamer has just paint on it no Aluminum
    Name:  14. Reamer has just paint on it no Aluminum.jpg
Views: 490
Size:  117.7 KB

    The pier bracket had to be welded by me in the field and there was only 8" between the bracket and the ground, so I decided to chamfer the top so that I could weld it with two passes from the top instead of all the way around as specified. I also have only limited experience welding overhead with a mirror.

    15. Chamfered pier bracket
    Name:  15. Chamfered pier bracket.jpg
Views: 490
Size:  115.7 KB
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  6. Likes ronsii liked this post
  7. #4
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    292
    Post Thanks / Like

    Re: Aluminum Gate Installation

    Last Saturday we installed the gate. Here is a close up picture of the hinge block and the pintle. After some experimenting we found that it was easiest to mount the top block to the gate leaf, then hang the gate and then slide the lower bearing block onto the lower pintle and finally mount the lower bearing block to the gate.

    16. Upper bearing block mounted on pintle
    Name:  16. Upper bearing block mounted on pintle.jpg
Views: 484
Size:  66.0 KB

    Here is a picture of the gate bracket bolted to the gate.

    17. Gate bracket mounted
    Name:  17. Gate bracket mounted.jpg
Views: 483
Size:  57.3 KB

    Here is a close up of my two pass stainless steel TIG weld, which attaches the pier bracket to the plate in the pier.

    19. Pier bracket welded to plate in pier
    Name:  19. Pier bracket welded to plate in pier.jpg
Views: 485
Size:  126.3 KB

    The following picture shows the linear actuator temporarily mounted to the newly welded pier bracket.

    20. Linear actuator mounted
    Name:  20. Linear actuator mounted.jpg
Views: 486
Size:  138.8 KB
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  8. Likes ronsii, farmersammm liked this post
  9. #5
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    292
    Post Thanks / Like

    Re: Aluminum Gate Installation

    Here is a picture of the mounted closed gate from the street.

    21. Gate closed
    Name:  21. Gate closed.jpg
Views: 487
Size:  151.4 KB

    Last but not least here is a picture of the opened gate, looking towards the street.

    22. Gate opened
    Name:  22. Gate opened.jpg
Views: 492
Size:  158.2 KB

    -Don
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  10. #6
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,348
    Post Thanks / Like

    Re: Aluminum Gate Installation

    Very nicely documented and great work again. Please keep on posting your work.
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  11. Likes ronsii liked this post
  12. #7
    Join Date
    Feb 2016
    Location
    Myrtle Beach
    Posts
    571
    Post Thanks / Like

    Re: Aluminum Gate Installation

    Great looking gates. Nice work!
    Lincoln 350MP
    Millermatic 350P
    Syncrowave 250
    1969 SA200
    HTP Invertig 221

  13. Likes ronsii liked this post
  14. #8
    Join Date
    Dec 2011
    Location
    Tampa FL
    Posts
    1,109
    Post Thanks / Like

    Re: Aluminum Gate Installation

    Very nice, looks well designed and executed.
    Mike

  15. Likes ronsii liked this post
  16. #9
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,859
    Post Thanks / Like

    Re: Aluminum Gate Installation

    wonderful

  17. #10
    Join Date
    Mar 2011
    Location
    Bilbao, Spain
    Posts
    863
    Post Thanks / Like

    Re: Aluminum Gate Installation

    Great step by step post! I love it!

  18. #11
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,554
    Post Thanks / Like

    Re: Aluminum Gate Installation

    Really great attention to detail - nicely done

    ...house is gorgeous!!
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  19. #12
    Join Date
    Apr 2006
    Location
    Sydney Australia
    Posts
    1,127
    Post Thanks / Like

    Re: Aluminum Gate Installation

    Lovely gates Don
    Just a Q.
    When doing larger gates like yours , we would normally have the pivots into top and bottom of the gate .
    Why did you opt to go with off set face fixed pivots ?
    Brett
    A good guess is better than a bad measurement

  20. #13
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    292
    Post Thanks / Like

    Re: Aluminum Gate Installation

    Quote Originally Posted by Brett View Post
    Lovely gates Don
    Just a Q.
    When doing larger gates like yours , we would normally have the pivots into top and bottom of the gate .
    Why did you opt to go with off set face fixed pivots ?
    Brett
    The reason for the offset bearing blocks is to eliminate the pinch point that typically occurs when the hinges are on the edge of the gate. The city that Scott lives in is very fussy about the design of gates and have extensive codes that the gate needs to meet. Attached are two pictures of the last gate that I worked on. You can see that as the gate is opened the vertical edge of the gate will get closer to the pier creating a pinch point. In this case the pier is a 6x6 post. In the case of Scott's gate the pier is wider so it would be a tighter pinch point.

    1. Whole gate asm
    Name:  1. Whole gate asm.jpg
Views: 164
Size:  96.0 KB

    2. Close up of hinge
    Name:  2. Close up of hinge.jpg
Views: 164
Size:  68.4 KB
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  21. Likes ronsii liked this post
  22. #14
    Join Date
    Apr 2006
    Location
    Sydney Australia
    Posts
    1,127
    Post Thanks / Like

    Re: Aluminum Gate Installation

    I see,
    Cheers mate
    Brett
    A good guess is better than a bad measurement

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,509,014.04580 seconds with 15 queries