    Tig Welding Magnesium?

    I am looking to Tig weld a magnesium lawn mower deck.

    What is the proper rod for this application?

    Any advice?

  2. #2
    Join Date
    Jan 2011
    Location
    Hutchinson Kansas
    Posts
    619
    Post Thanks / Like

    Re: Tig Welding Magnesium?

    Harris offers 2 tig fillers for magnesium.
    AZ61A
    AZ92A
    Lincolin Power Wave 450, Lincoln Powermig 255, Lincoln Pro Mig 140, Lincoln Squarewave Tig 275, Miller Big 40 G(with Hobart Hefty suitcase), Thermal Arc 95S and Esab PCM875 in an already full machine shop.

  3. #3
    Join Date
    Jul 2008
    Posts
    3,312
    Post Thanks / Like

    Re: Tig Welding Magnesium?

    $$$$$$$$$$$$$$$$$$$$

    I suspect it'd be cheaper to buy a new mower (or three).

  4. #4
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: Tig Welding Magnesium?

    Az101
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  5. #5
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    10,930
    Post Thanks / Like

    Re: Tig Welding Magnesium?

    Just buy this filler and have at it. $35 shipped.

    https://www.ebay.com/i/301935363371?...xoCFF0QAvD_BwE
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  6. Likes ronsii liked this post
+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,243,321.62049 seconds with 20 queries