    240c Welding Machines that can d 120v

    What is the best 240v welding machine that can also be used on a 120v circuit?

    Right now i just bought the "125 flux core chicago electric" to mess around with for now until i get a reasonable 120v machine. I know how to use all processes but TIG is the one that im least trained in i only go and introduction to it. But i do want to try TIG out and actually get good with it and was wondering if its possible to tig weld on 120v atleast for aluminum and stuff even if you have to rig the welding gun to be able to do it. Probably not recommended not sure. But my uncle is a licensed electrician so he may be able to rig it safely.
    Trained In
    GMAW 2G (Horizontal)
    FCAW 3G Vertical and 4G Overhead
    SMAW 3G Vertical and 4G Overhead
    GMAW(Pulse) 3G Vertical and 4G Overhead
    GTAW (INTRO)
    Carbon Arc Gouging (INTRO)
    Weld Symbols (INTRO)
    Distrotion Control
    Oxy/Fuel Cutting (INTRO)



  2. #2
    Join Date
    Dec 2007
    Location
    Los Angeles
    Posts
    7,809
    Post Thanks / Like

    Re: 240c Welding Machines that can d 120v

    Best Dual Voltage Tig machine is a pretty wide open request.

    Since you mentioned aluminum it will have to be an AC/DC machine so that adds $$ over a simple machine that will only weld steel, a DC machine.

    All of the big brands have a machine for you.
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Miller 125c Plasma 120v
    SO 2020 bender
    Beer in the fridge

  3. #3
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    1,821
    Post Thanks / Like

    Re: 240c Welding Machines that can d 120v

    Just ever home in usa has 240 volts.
    1) One way is to two 120volt receipt one one each leg
    2) use dryer or range plug
    3) go to meter box and hope you have a spot to put a 240 volt circuit.
    Most TIG machines need a 40 amp 240 volt circuit 50 amp would be better.

    Dave

    Quote Originally Posted by WeldsFargo View Post
    What is the best 240v welding machine that can also be used on a 120v circuit?

    Right now i just bought the "125 flux core chicago electric" to mess around with for now until i get a reasonable 120v machine. I know how to use all processes but TIG is the one that im least trained in i only go and introduction to it. But i do want to try TIG out and actually get good with it and was wondering if its possible to tig weld on 120v atleast for aluminum and stuff even if you have to rig the welding gun to be able to do it. Probably not recommended not sure. But my uncle is a licensed electrician so he may be able to rig it safely.

  4. #4
    Join Date
    Apr 2020
    Location
    Canada
    Posts
    122
    Post Thanks / Like

    Re: 240c Welding Machines that can d 120v

    Iíve got a Primeweld 225 that runs on 110/220.
    It will put out about 100 amps on 110v.
    Works fine for steel up to about 1/8Ē
    I havenít tried it on aluminum so canít comment on that.


    Sent from my iPhone using Tapatalk
    David
    Millermatic 130
    Primeweld 225
    Victor Journeymen

  5. #5
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    1,821
    Post Thanks / Like

    Re: 240c Welding Machines that can d 120v

    That sounds like it is good welder.
    The best part is you can go to 240 volts for heavier welding.

    I have tried 120 two times both times I was not happy. But having the choice of 120 volt and 240 volt is a good way to go.

    Dave

    Quote Originally Posted by DavidR8 View Post
    Iíve got a Primeweld 225 that runs on 110/220.
    It will put out about 100 amps on 110v.
    Works fine for steel up to about 1/8Ē
    I havenít tried it on aluminum so canít comment on that.


    Sent from my iPhone using Tapatalk

  6. Likes DavidR8 liked this post
  7. #6
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    5,098
    Post Thanks / Like

    Re: 240c Welding Machines that can d 120v

    I can use any of my 240V welders on a 120V circuit, and the vast majority of them are not dual-voltage.

    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,318,918.72462 seconds with 14 queries