    I was cutting a small steel angle (2"x2") in my FEIN cold metal chop saw and it slipped from the vise jaw, rotated, then cracked and fractured (made a small hole) to the alum cast base. Grrrr!

    Is it possible to use an alum spool MIG gun (with argon) and repair this alum casting?

    Name:  2CB5BF38-0946-44C6-928E-C43171AC98D4.jpg
Views: 382
Size:  64.2 KB
    LINCOLN Power MIG 210 MP

    LINCOLN Ranger 330 MPX

    MILLER Thunderbolt AC/DC

    HYPERTHERM Powermax 190C

    HYPERTHERM Powermax 45XP

    HOUGAN HMD 505

    HOUGAN HMD 130

    FEIN/SLUGGER 14" COLD METAL CHOP SAW

  2. #2
    Join Date
    Oct 2014
    Posts
    2,617
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    Maybe but Tig would be better because if it was dirty Tig would burn the impurities out easier. Cleaning it really good a series of Mig tacks may work. May have to grind out dirty welds till it's clean.

  3. Likes Ingenuity liked this post
  4. #3
    Join Date
    Oct 2015
    Posts
    2,723
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    It can be done with a spool gun if you are careful . Use a piece of copper for a backer when welding up the hole. It will help a lot. If you can't find some copper get a piece of copper plumbing pipe. Cut a short piece off, Heat it to about 800 degrees and quench it in water to anneal it. Then take a hammer to flatten it. It will work for what you need to do.

  5. Likes ronsii liked this post
  6. #4
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,554
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    In addition to copper, steel also works as a backer for aluminum.

    Good luck on the repair.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  7. Likes ronsii, shovelon liked this post
  8. #5
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,858
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    Any possibility it could be magnesium?

  9. #6
    Join Date
    Aug 2016
    Posts
    101
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    Welder Dave, thegary and MinnesotaDave - thanks for your insight. I was intending on using copper backing - I purchased some recently for some carbon steel backing to groove welds.

    tapwelder - you may be right. My only experience with magnesium has been with concrete screeds/floats - and they tend to weather/discolor to a dark grey color. How would I 'litmus test' the saw base to check if magnesium or aluminum?
    LINCOLN Power MIG 210 MP

    LINCOLN Ranger 330 MPX

    MILLER Thunderbolt AC/DC

    HYPERTHERM Powermax 190C

    HYPERTHERM Powermax 45XP

    HOUGAN HMD 505

    HOUGAN HMD 130

    FEIN/SLUGGER 14" COLD METAL CHOP SAW

  10. #7
    Join Date
    Oct 2014
    Posts
    2,617
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    Be careful because magnesium will burn and you can't use water to put it out. It will explode. I read where you can put some vinegar on it and if it reacts it's magnesium and if it doesn't do anything it's aluminum. You can also file some shavings and see they burn like a sparkler. If I had to guess I'd say it's probably aluminum.
    Last edited by Welder Dave; 4 Weeks Ago at 02:28 AM.

  11. Likes Ingenuity liked this post
  12. #8
    Join Date
    Aug 2016
    Posts
    101
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    Thanks Welder Dave.

    I shall try the 'burn-the-filings' trick. Thanks.
    LINCOLN Power MIG 210 MP

    LINCOLN Ranger 330 MPX

    MILLER Thunderbolt AC/DC

    HYPERTHERM Powermax 190C

    HYPERTHERM Powermax 45XP

    HOUGAN HMD 505

    HOUGAN HMD 130

    FEIN/SLUGGER 14" COLD METAL CHOP SAW

  13. #9
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    487
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    Your chance of igniting solid magnesium, even under welding conditions is super low. It burns like the devil once ignited, but lighting it is not easy. Anytime someone wants to show mag burning it is with filings/dust to get enough surface area to ignite easily.

    But if you try to use alum weld on a mag part, that ain't gonna work.... so.... look up the saw on Fein's website and see if it is mag. Since that is a feature (lighter, costlier) if it is mag they will say it for sure.
    -Dave
    XMT304 with: 22A Feeder, or HF251 Hi Freq DC TIG air cooled

  14. #10
    Join Date
    Aug 2016
    Posts
    101
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    Quote Originally Posted by davec View Post
    Your chance of igniting solid magnesium, even under welding conditions is super low. It burns like the devil once ignited, but lighting it is not easy. Anytime someone wants to show mag burning it is with filings/dust to get enough surface area to ignite easily.

    But if you try to use alum weld on a mag part, that ain't gonna work.... so.... look up the saw on Fein's website and see if it is mag. Since that is a feature (lighter, costlier) if it is mag they will say it for sure.
    davec:

    Great idea. I looked it up, and it is alum cast base.

    Name:  36DC20BF-2BB8-483E-9B71-D4D0B0BF877B.jpg
Views: 234
Size:  24.4 KB

    Thanks.
    LINCOLN Power MIG 210 MP

    LINCOLN Ranger 330 MPX

    MILLER Thunderbolt AC/DC

    HYPERTHERM Powermax 190C

    HYPERTHERM Powermax 45XP

    HOUGAN HMD 505

    HOUGAN HMD 130

    FEIN/SLUGGER 14" COLD METAL CHOP SAW

  15. #11
    Join Date
    Nov 2004
    Location
    Southern Montana
    Posts
    919
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    I think I would drop by HF, pick up some low temperature aluminum welding rods to use with propane, and give it a try with some type of backing.

  16. #12
    Join Date
    Jul 2013
    Posts
    301
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    I've used Alumiweld. It's great for some things but I don't think it's right for this repair. It doesn't flow and wet out like solder. It only wets well where you can scratch the base metal with a sharp tool while the puddle is molten. It's going to be hard to scratch the surface down into that crack.

    I give a plus one to using a backer with TIG.

    And I'd add preheat to of the part to about 400-500 F so the part is up to temp for at least 5 minutes. It helps empty the air pockets in the aluminum porosity. My experience is if you don't preheat it will feel like trying to weld styrofoam. I think a 4043 rod will work but I've also used 4943 rod that's supposed to be better for cast aluminum.

  17. Likes shovelon liked this post
  18. #13
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,553
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    Quote Originally Posted by sand_man_red View Post
    I've used Alumiweld. It's great for some things but I don't think it's right for this repair. It doesn't flow and wet out like solder. It only wets well where you can scratch the base metal with a sharp tool while the puddle is molten. It's going to be hard to scratch the surface down into that crack.

    I give a plus one to using a backer with TIG.

    And I'd add preheat to of the part to about 400-500 F so the part is up to temp for at least 5 minutes. It helps empty the air pockets in the aluminum porosity. My experience is if you don't preheat it will feel like trying to weld styrofoam. I think a 4043 rod will work but I've also used 4943 rod that's supposed to be better for cast aluminum.
    4943 would definitely be the better of the two for a better strength match to the cast. 5356 would even be better. Too bad we don't know where your location as it would be a very simple tig repair. And I agree with clamping a steel backer to hold flat.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig4ea,MigMax1ea.

  19. Likes TJS liked this post
  20. #14
    Join Date
    Oct 2014
    Posts
    2,617
    Post Thanks / Like

    Re: Crack and small hole repair to alum casting

    400-500 deg. preheat seems high for aluminum and this isn't a very thick casting.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,490,652.72047 seconds with 14 queries