    Hey fellows, I need a board for my millermatic 211 auto set. I’ve had it four years and the board just quit on me. Anyone know where I can find one other than miller?
    Miller 211
    Miller Dynasty 210

  2. #2
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Millermatic 211

    I don't believe there are any aftermarket boards out there for the 211's.... you might be able to find a pull on ebay.amz/fb... but it won't be much better than your board was two minutes before it quit

    I would pull the board and see if you can find a repair place that will fix it... there are a couple common issues with the 2ng gen 211's that blow a couple components... I'm guessing this is a 2nd gen 211...?

  3. Likes bamadogred liked this post
  4. #3
    Join Date
    Oct 2016
    Location
    Tuscumbia, Alabama
    Posts
    9
    Post Thanks / Like

    Re: Millermatic 211

    Yes it is. It was only a month out of warranty when it blew and miller wouldn’t work with me. The board looks really clean doesn’t look like anything is wrong. But they said the board was out and it would cost 700 to repair it. So I thought I would check here.
    Miller 211
    Miller Dynasty 210

  5. #4
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Millermatic 211

    Quote Originally Posted by bamadogred View Post
    Yes it is. It was only a month out of warranty when it blew and miller wouldn’t work with me. The board looks really clean doesn’t look like anything is wrong. But they said the board was out and it would cost 700 to repair it. So I thought I would check here.
    If you can... take some good res pics of the board and post them up

    I'd be willing to bet it's the same components that blew as a few other threads here on the welding web forum... of course there's always a chance it is something else... but odds favor the common issues

  6. #5
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Millermatic 211

    Here's a couple pics of the last 211 I had blow... this one took out D45 and D6 diodes... sometimes (most times) it takes out a transistor and maybe a resistor also... but this one didn't....


    Name:  miller211-board-badcompnents2.jpg
Views: 2408
Size:  115.5 KB

    Name:  miller211-board-badcompnents1.jpg
Views: 1948
Size:  87.9 KB

  7. #6
    Join Date
    Oct 2016
    Location
    Tuscumbia, Alabama
    Posts
    9
    Post Thanks / Like

    Re: Millermatic 211

    Thanks for the info. My father in-law has it now trying to fix it. I will tell him to take pics and I will post them. I never had a problem with this welder until I hooked my aluminum spool gun and in ten minutes it went down.
    Miller 211
    Miller Dynasty 210

  8. Likes ronsii liked this post
  9. #7
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Millermatic 211

    hmmmm. don't recall anything about spoolguns causing issues??? mine have not ran spoolguns.. so yours may be something different???

    Oh, the transistor tor the right and down(from the diodes/in the heatsink) is the one that usually blows( I forget the board number) but it's a to220 case or similar IIRC....

  10. #8
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    10,317
    Post Thanks / Like

    Re: Millermatic 211

    Curious, where was machine purchased
    at ??
    We had a issue with a first generation Miller XMT 304. It was 6 months out of warranty and our welding supplier repaired it under warranty. Machine was purchased from them.


    Sent from my iPhone using Tapatalk

  11. #9
    Join Date
    Oct 2016
    Location
    Tuscumbia, Alabama
    Posts
    9
    Post Thanks / Like

    Re: Millermatic 211

    It was purchased at Airgas. They didn’t want to help much. And we spend a lot of money with them. I bought my other two home welders from another weld supply store. They have been more helpful.
    Miller 211
    Miller Dynasty 210

  12. #10
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    10,317
    Post Thanks / Like

    Re: Millermatic 211

    Quote Originally Posted by bamadogred View Post
    It was purchased at Airgas. They didn’t want to help much. And we spend a lot of money with them. I bought my other two home welders from another weld supply store. They have been more helpful.
    Air Gas sucked years ago. Now they are even worse. They bought out my local supplier and their cylinder exchanges are off the charts ! I drive 30 miles to a Ma and PA supplier and avoid Air Gas.


    Sent from my iPhone using Tapatalk

  13. #11
    Join Date
    Oct 2016
    Location
    Tuscumbia, Alabama
    Posts
    9
    Post Thanks / Like

    Re: Millermatic 211

    I agree. I won’t buy another welder from them for sure. Luckily we have young’s welding. It’s a smaller family owned shop, they just can’t get low enough on they’re gas bottles for us to use them solely.
    Miller 211
    Miller Dynasty 210

  14. #12
    Join Date
    Mar 2010
    Location
    East Tennessee
    Posts
    1,254
    Post Thanks / Like

    Re: Millermatic 211

    Glad I bought a first generation 211 when they were phasing them out for the 2nd gens. It was $999 with a $200 mail in rebate. Purrs like a kitten.

  15. Likes ronsii liked this post
  16. #13
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Millermatic 211

    Quote Originally Posted by Showdog75 View Post
    Glad I bought a first generation 211 when they were phasing them out for the 2nd gens. It was $999 with a $200 mail in rebate. Purrs like a kitten.
    A fat heavy kitten!!!

  17. Likes Dave66 liked this post
  18. #14
    Join Date
    Jun 2016
    Posts
    1,002
    Post Thanks / Like

    Re: Millermatic 211

    is a first generation 211 the one with the suite case handle in the top center of the case?
    lincoln 125sp
    dayton 250 ac/dc
    miller 211 w/spool gun
    ahp 200 sx tig
    lotos ltp5000d
    kubota b3200 FEL BH
    of course duramax diesel

  19. #15
    Join Date
    Feb 2019
    Location
    Snyder TX
    Posts
    643
    Post Thanks / Like

    Re: Millermatic 211


  20. #16
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: Millermatic 211

    Quote Originally Posted by duramax-rob View Post
    is a first generation 211 the one with the suite case handle in the top center of the case?
    Yes.

    Name:  RWMoELI.jpeg
Views: 2069
Size:  271.7 KB
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  21. #17
    Join Date
    Oct 2016
    Location
    Tuscumbia, Alabama
    Posts
    9
    Post Thanks / Like

    Re: Millermatic 211

    This is a picture of the board. And I hear ya show dog 75. I wish I had the first gen. I can’t believe this one sucked.

    Name:  EC613C1B-08F7-49B0-A54B-1938319D4B2E.jpg
Views: 2193
Size:  140.1 KB
    Miller 211
    Miller Dynasty 210

  22. #18
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Millermatic 211

    I smoked one of those 211's, but it was my fault for not really paying attention to the duty cycle.
    1st on WeldingWeb to have a scrolling sig!



  23. #19
    Join Date
    Dec 2016
    Posts
    320
    Post Thanks / Like

    Re: Millermatic 211

    shame on miller for crapping on you so close out of warranty.

  24. #20
    Join Date
    Mar 2022
    Posts
    1
    Post Thanks / Like

    Re: Millermatic 211

    Do you know the values of these components? I refer to D6 and D45.

  25. #21
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    8,961
    Post Thanks / Like

    Re: Millermatic 211

    Its great to know there is a fix. We had a balancer with a problem, logic i guess but no fix and another plasma i might pull off the shelf to re look at one of these days.

  26. #22
    Join Date
    Jan 2022
    Posts
    45
    Post Thanks / Like

    Re: Millermatic 211

    I have worked with Miller Electric for over 40 years and never had a problem stretching a warranty over several months. I even had the honor a recall on a transformer in a machine that was 10 years old.
    Your problem, as was stated earlier , was your supplier. I always went to bat for my customers and I knew who at Miller who I needed to contact to get things done.
    You must remember when buying equipment, its not the company that you are buying from, it's the man representing the company.
    His or hers honesty and integerity is what you are counting on with your purchase. I guess that is why my customers buy from me. They know that they get a little part of me with the sale.

  27. Likes wb4rt, yooper liked this post
  28. #23
    Join Date
    Nov 2023
    Posts
    1
    Post Thanks / Like

    Re: Millermatic 211

    I know this is an old thread but I was hoping someone my know the value of the resistors that also blow (c63 and c64)
    Thanks

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,289,192.52486 seconds with 19 queries