Re: How to make a dead end cap on tubing?
Originally Posted by
BluCllrPlt
All the texts/handbooks I have read only indicate a 45 degree angle. In the morning I will submit a photo of the angle that I think you have a question about.
No need. I found this printed reference from the Pipefitters Handbook provided by someone who seems to know this stuff. He is way helpful. I'm sure he'd share resources with you. :^)
And that printed reference clearly says 37.5 degree bevel (for a total 75 degree V Groove).
-
-
Post Thanks / Like - 1 Likes, 0 Dislikes