    Looks great

    Dave


    Quote Originally Posted by MetalMan23 View Post
    I'm thinking of heating the flatbar in the forge, twisting/bending it into the proper shape, I rolled this plate to the required radius, and then heating the half round and welding it on as I go, matching the core of the solid bar, it'll probably take a fusion weld, minimal filler rod, then just smooth it out with the sanding pad.

    Sent from my moto g power using Tapatalk

  2. #27
    Join Date
    Oct 2014
    Posts
    3,027
    Post Thanks / Like

    Re: Bending oval stainless tubing into spiral: how???

    Another way that may be possible but a lot of work is cutting a bunch of pie shaped vee's out of the tubing and closing them up to make the curve.

  3. #28
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,971
    Post Thanks / Like

    Re: Bending oval stainless tubing into spiral: how???

    is the chalk mark the pattern? Add support to the form. Also, add a way to reference level/twist, the cap will want to twist. Make a bending/twisting fork. I suspect the side of your fixture you end on will need to be trimmed or over bent to allow you to reach your target radius. Even trimming the excess above the line would be wise to assist clamping. Make sure you have plenty of clear space around you to compete the bend. A torch will work and will not need to remove the part once you start. Since, you have 3 then you will have some practice. Good luck
    Last edited by tapwelder; 11-26-2020 at 04:22 PM.

  4. #29
    Join Date
    Apr 2006
    Location
    Sydney Australia
    Posts
    1,159
    Post Thanks / Like

    Re: Bending oval stainless tubing into spiral: how???

    Please post some pics when you have finished , would love to see them .
    A good guess is better than a bad measurement

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,611,090,698.98450 seconds with 13 queries