    What is this symbol?

    It's a torque spec and I understand they are saying 2 stages but the first stage says 5nm and the second says 95 with this symbol (where the blue arrow is pointing), anyone know what it means?
    Miller Challenger 172
    Miller Thunderbolt AC/DC 225/150
    Miller Maxstar 150 STL
    Victor 100C
    Victor Journeyman
    Oxweld OA
    Harris O/A
    Smith O/A little torch

    No, that's not my car.

  2. #2
    Join Date
    Feb 2016
    Location
    Myrtle Beach
    Posts
    881
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by bigb View Post
    It's a torque spec and I understand they are saying 2 stages but the first stage says 5nm and the second says 95 with this symbol (where the blue arrow is pointing), anyone know what it means?
    Pretty sure it's 95 degrees. Like you would torque a stretch bolt with a torque angle guage.
    Lincoln 350MP
    Millermatic 350P
    Syncrowave 250
    1969 SA200
    HTP Invertig 221

  3. Likes ronsii, MinnesotaDave liked this post
  4. #3
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    9,799
    Post Thanks / Like

    Re: What is this symbol?

    And probably with new sealing washers... although it doesn't say it... unless they are bonded washers???

  5. Likes Capt B liked this post
  6. #4
    Join Date
    Nov 2009
    Location
    Arizona
    Posts
    2,688
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by Capt B View Post
    Pretty sure it's 95 degrees. Like you would torque a stretch bolt with a torque angle guage.
    OK I get it. I just looked at angle gauges and they all get really bad reviews, I think I will just use my old camshaft degree wheel and call it good
    Miller Challenger 172
    Miller Thunderbolt AC/DC 225/150
    Miller Maxstar 150 STL
    Victor 100C
    Victor Journeyman
    Oxweld OA
    Harris O/A
    Smith O/A little torch

    No, that's not my car.

  7. Likes ronsii liked this post
  8. #5
    Join Date
    Feb 2016
    Location
    Myrtle Beach
    Posts
    881
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by bigb View Post
    OK I get it. I just looked at angle gauges and they all get really bad reviews, I think I will just use my old camshaft degree wheel and call it good
    That would work. With 95 degrees you could probably even just eyeball it.
    Lincoln 350MP
    Millermatic 350P
    Syncrowave 250
    1969 SA200
    HTP Invertig 221

  9. Likes ronsii liked this post
  10. #6
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    9,799
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by Capt B View Post
    That would work. With 95 degrees you could probably even just eyeball it.
    Yep, just be careful if you put a crowsfoot with an extension on it

  11. #7
    Join Date
    Nov 2009
    Location
    Arizona
    Posts
    2,688
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by Capt B View Post
    That would work. With 95 degrees you could probably even just eyeball it.

    eyeball it?? on a Mercedes??? Good God man what are you smoking?? Even the plastic air box has a torque spec!
    Miller Challenger 172
    Miller Thunderbolt AC/DC 225/150
    Miller Maxstar 150 STL
    Victor 100C
    Victor Journeyman
    Oxweld OA
    Harris O/A
    Smith O/A little torch

    No, that's not my car.

  12. Likes ronsii, Capt B, 12V71, CAVEMANN liked this post
  13. #8
    Join Date
    Nov 2009
    Location
    Arizona
    Posts
    2,688
    Post Thanks / Like

    Re: What is this symbol?

    Actually when I thought about it I think it is just a fancy way to say "5NM plus a quarter turn"
    Miller Challenger 172
    Miller Thunderbolt AC/DC 225/150
    Miller Maxstar 150 STL
    Victor 100C
    Victor Journeyman
    Oxweld OA
    Harris O/A
    Smith O/A little torch

    No, that's not my car.

  14. Likes Capt B, ronsii liked this post
  15. #9
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    9,799
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by bigb View Post
    Actually when I thought about it I think it is just a fancy way to say "5NM plus a quarter turn"
    ....and a 'tad'

  16. Likes Munkul liked this post
  17. #10
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,964
    Post Thanks / Like

    Re: What is this symbol?

    A tad plus another tad. Or just a smidge.

  18. Likes ronsii, Munkul liked this post
  19. #11
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,741
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by ronsii View Post
    Yep, just be careful if you put a crowsfoot with an extension on it
    Quote Originally Posted by bigb View Post
    eyeball it?? on a Mercedes??? Good God man what are you smoking?? Even the plastic air box has a torque spec!
    Quote Originally Posted by ronsii View Post
    ....and a 'tad'
    Quote Originally Posted by tapwelder View Post
    A tad plus another tad. Or just a smidge.
    You guys crack me up
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  20. Likes Capt B, ronsii liked this post
  21. #12
    Join Date
    Oct 2014
    Posts
    3,017
    Post Thanks / Like

    Re: What is this symbol?

    The torque turn method. If a pinch of salt is acceptable for a Michelin Star chef surely a tad, smidge or .... hair should acceptable for a mechanic.

  22. #13
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    9,799
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by Welder Dave View Post
    The torque turn method. If a pinch of salt is acceptable for a Michelin Star chef surely a tad, smidge or .... hair should acceptable for a mechanic.
    And when a hair is a bit much you use a different type of hair


  23. #14
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    3,494
    Post Thanks / Like

    Re: What is this symbol?

    We could differentiate between the blonde ones and the black ones, but that would be splitting hairs...
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  24. Likes ronsii liked this post
  25. #15
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,513
    Post Thanks / Like

    Re: What is this symbol?

    My favorite torque setting: go till it cracks, then back a 1/4 turn.

  26. Likes Capt B, ronsii, tapwelder liked this post
  27. #16
    Join Date
    Feb 2016
    Location
    Myrtle Beach
    Posts
    881
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by Fnord5 View Post
    My favorite torque setting: go till it cracks, then back a 1/4 turn.
    That reminds me of something a mechanic I use to work with would always say. "cross thread is better than a lock washer any day"
    Lincoln 350MP
    Millermatic 350P
    Syncrowave 250
    1969 SA200
    HTP Invertig 221

  28. #17
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,741
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by Fnord5 View Post
    My favorite torque setting: go till it cracks, then back a 1/4 turn.
    Quote Originally Posted by Capt B View Post
    That reminds me of something a mechanic I use to work with would always say. "cross thread is better than a lock washer any day"
    Tighten until it gets loose....back off 1/4 turn...
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  29. Likes ronsii, tapwelder liked this post
  30. #18
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,964
    Post Thanks / Like

    Re: What is this symbol?

    Hey, son I just made the bolt head disappear ....

    You've used that joke before, dad, it's in the socket, I'll get the hammer,chisel and tig welder.

  31. Likes MinnesotaDave, Capt B, ronsii liked this post
  32. #19
    Join Date
    Sep 2014
    Posts
    1,419
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by ronsii View Post
    Yep, just be careful if you put a crowsfoot with an extension on it

    Hey, wait a minute, I resemble that remark, haha.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  33. Likes ronsii liked this post
  34. #20
    Join Date
    Sep 2014
    Posts
    1,419
    Post Thanks / Like

    Re: What is this symbol?

    Quote Originally Posted by ronsii View Post
    And when a hair is a bit much you use a different type of hair


    I could never figure out how to use one. And if you split one you have to make Hosinfeffer out of it or else it is a sin to kill it.


    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  35. Likes ronsii, Capt B liked this post
  36. #21
    Join Date
    Oct 2014
    Posts
    1,025
    Post Thanks / Like

    Re: What is this symbol?

    90° and a RCH.

  37. Likes ronsii liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,610,921,516.46633 seconds with 14 queries