    Before I ruin this by experimenting I wondered if anyone here has drilled a hole in a magnet successfully. I need to put a 5/16" hole in this one and thought about starting with a small bit and incrementing my way up?
    Attached Images Attached Images  

  2. #2
    Join Date
    Aug 2018
    Location
    'ta town, KS
    Posts
    454
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    That works.. but is that magnet chipping? It will be challenging to do if it is already chipping

    Sent from my SM-G960U using Tapatalk
    I haven't built anything I can't throw away. Perfection is the journey.

    Mac

  3. #3
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    18,081
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Never tried it myself but starting small and working up was my first thought as well. Sharp drills and go SLOW would be my suggestion.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  4. #4
    Join Date
    May 2010
    Location
    Ct.
    Posts
    1,771
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Looks like a ceramic (ferrite)magnet.
    You could try grinding a hole with a Dremel
    tool , die grinder, Du-more grinder etc. with a small
    mounted stone.
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  5. Likes Denis G liked this post
  6. #5
    Join Date
    Nov 2005
    Location
    ca
    Posts
    151
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Syncrowave 250 w/ coolrunner
    MM210 W/spoolgun
    SP 135
    Victor O/A
    Ramsond cut 50
    Titanium Stick 225.

  7. Likes walker liked this post
  8. #6
    Join Date
    May 2007
    Posts
    4,589
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    i had the same scenario u goin through i think. i had magnets come out of a $53 stabila torpedo . i tired to drill, but couldnt. ive seen torpedo magnets w/ holes through them though

  9. #7
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    783
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    You need a mag drill

  10. #8
    Join Date
    Jan 2015
    Location
    Lewis Center/Powell Ohio
    Posts
    970
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Home Depot has some Neodymium magnets with the right size hole in them but they're too strong for what I need. Guess I'll just start with my smallest bit and work up.

  11. #9
    Join Date
    May 2012
    Location
    Ontario, Canada
    Posts
    1,505
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    I'd try an abrasive diamond grit bit.

  12. Likes William McCormick liked this post
  13. #10
    Join Date
    Apr 2006
    Location
    Sydney Australia
    Posts
    1,224
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Quote Originally Posted by 123weld View Post
    i had the same scenario u goin through i think. i had magnets come out of a $53 stabila torpedo . i tired to drill, but couldnt. ive seen torpedo magnets w/ holes through them though
    Some magnets are Cobalt , now that would take some drilling .
    Some however are iron .
    A good guess is better than a bad measurement

  14. #11
    Join Date
    Jan 2015
    Location
    Lewis Center/Powell Ohio
    Posts
    970
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    There's some of those over at Home Depot with the right size hole in them. But they're too strong for what I need it for. Guess I'll just start with my smallest bit and gradually go up. Don't know what it's made of, just some cheap magnet so maybe iron.

  15. #12
    Join Date
    Jan 2015
    Location
    Lewis Center/Powell Ohio
    Posts
    970
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    I had to give up. A drill bit won't even make a pockmark in the surface. Moving on to find another solution.

  16. #13
    Join Date
    Feb 2016
    Location
    Six Mile SC
    Posts
    79
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Quote Originally Posted by JD1 View Post
    There's some of those over at Home Depot with the right size hole in them. But they're too strong for what I need it for. Guess I'll just start with my smallest bit and gradually go up. Don't know what it's made of, just some cheap magnet so maybe iron.
    When a magnet is too strong, I often coat it with a layer or two of duct tape.
    CG

  17. #14
    Join Date
    Mar 2015
    Location
    Milwaukee, WI
    Posts
    615
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Try using the same type of bit used for drilling ceramic tile.

  18. Likes Capt B, William McCormick liked this post
  19. #15
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    575
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Try https://www.kjmagnetics.com/
    KJ has rare earth mag. many with holes.
    Magnets hate heat once you hit the curie point they lose mag.

  20. Likes William McCormick liked this post
  21. #16
    Join Date
    Aug 2018
    Location
    'ta town, KS
    Posts
    454
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    I have drilled through speaker magnets on multiple occasions. To mount diamonds for dressing the grinder store. Very slow speeds and patience.

    Sent from my SM-G960U using Tapatalk
    I haven't built anything I can't throw away. Perfection is the journey.

    Mac

  22. #17
    Join Date
    Oct 2014
    Posts
    2,135
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    That kind of magnet is not very hard at all.

  23. #18
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    A lot of the jewelry crowd uses micro core bits and other assorted diamond covered tooling. you could also rig up a redneck EM setup and bore through with electrical

  24. #19
    Join Date
    Aug 2012
    Location
    AR
    Posts
    2,468
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Quote Originally Posted by tackit View Post
    If that was a solid magnet, I would have tried to spot heat it in the center with a torch, and then drive a small center punch through it.
    As Reebz said, if you heat a magnet past the Curie point (temp), you will no longer have a magnet.

  25. Likes William McCormick liked this post
  26. #20
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    575
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Check out K&J magnet. They have them in all shapes and sizes. Neodymium mags. are amazing.

  27. Likes William McCormick liked this post
  28. #21
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    14,977
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Thinking about those ones that were available with the hole, but too strong. How about a variation on the duct tape idea, and coat them with fiberglass resin? Can't you weaken a magnet by dropping it? Not sure how many million drops that would take if you wanted it to happen though...
    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Vevor MIG 200A
    Victor Medalist 350 O/A
    Vevor Cut 50 Plasma
    Les

  29. #22
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    783
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    Q. What do you get when you heat a rare earth magnet?

    A. Rare earth.

  30. #23
    Join Date
    Sep 2014
    Posts
    2,372
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    I would go with a wet diamond bit.


    https://www.amazon.com/Diamond-Drill...6787867&sr=8-7


    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  31. #24
    Join Date
    Sep 2014
    Posts
    2,372
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    These look better.

    https://www.amazon.com/uxcell-Diamon...WT5PZJ0KS&th=1

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  32. Likes ronsii liked this post
  33. #25
    Join Date
    Jan 2021
    Posts
    15
    Post Thanks / Like

    Re: Drilling a hole in a magnet?

    To drill a hole in a magnet, you will need to apply the tip of a power drill onto the surface of the magnet and gently push it down into the center. For the best results, you should proceed with frequent stops to flush the holes with a coolant solution to prevent adverse effects.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,291,298.11410 seconds with 21 queries