    Oxy Acetylene welding

    I finally bought a torch setup, I’ve wanted one a long time but always been able to manage to get stuff to my uncles shop or a cousins place to use theirs.

    OA welding is how I learned my freshman year of high school in 1994, haven’t welded anything OA since probably 1998 though I have brazed a lot of stuff.
    Tonight I figured I’d teach my son who’s in the 6 th grade, I told him if he can learn this he can learn any of it. Watch the puddle, use the flame to move it, etc etc etc.
    Ran a puddle bead then said have at it. I don’t think his first hour of class tonight was bad at all. 1/4” mild steel


    Sent from my iPhone using Tapatalk

  2. Likes tapwelder, whtbaron liked this post
  3. #2
    Join Date
    Jul 2016
    Location
    Midwest
    Posts
    423
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by Birdhunter1 View Post
    I finally bought a torch setup, I’ve wanted one a long time but always been able to manage to get stuff to my uncles shop or a cousins place to use theirs.

    OA welding is how I learned my freshman year of high school in 1994, haven’t welded anything OA since probably 1998 though I have brazed a lot of stuff.
    Tonight I figured I’d teach my son who’s in the 6 th grade, I told him if he can learn this he can learn any of it. Watch the puddle, use the flame to move it, etc etc etc.
    Ran a puddle bead then said have at it. I don’t think his first hour of class tonight was bad at all. 1/4” mild steel


    Sent from my iPhone using Tapatalk
    I would consider 1/4" to be a little too thick to learn true torch welding. In my humble opinion the pupil should start with 20ga or 3/32 to start. Glad to see you're passing oxy-fuel welding to the next gen. good for you !!
    Thermal Arc 320SP ( Lorch )
    Cobra Pythons
    Thermal Arc 300 AC/DC ( Sanrex )
    ESAB 301i AC/DC ( Lorch )
    Thermal Arc 161STL ( WTL )
    Thermal Arc 190S ( Sanrex )
    Cut Master 82, 42. Cut45 ( WTL )
    Victor Gas Apps.
    Boxes and boxes of welding crap.

  4. Likes JimboTN liked this post
  5. #3
    Join Date
    Oct 2014
    Posts
    3,034
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Start on something around 12 gauge. After learning basic beads can do some lap welds and then butt welds where you have to keep a keyhole. Learning on a thick piece of old scrap kind of defeats the purpose.

  6. #4
    Join Date
    Jul 2007
    Location
    Murphysboro, IL
    Posts
    198
    Post Thanks / Like

    Re: Oxy Acetylene welding

    I did have some 16 gauge tube he was first trying on and kept burning holes in it. I knew that 1/4” he wouldn’t burn through, once he got a puddle it was like a big AH HA moment and he said ‘THERE IT IS’ and I said make it dance.

    Nothing to brag about but he was definitely seeing a puddle and trying to make it move. He did puddle a bead about 4” across that plate.

    When I learned we had 16 gauge x 1” wide pieces. Laps, butts, uphill horizontal and maybe overhead welding and brazing.


    Sent from my iPhone using Tapatalk

  7. Likes whtbaron liked this post
  8. #5
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    9,564
    Post Thanks / Like

    Re: Oxy Acetylene welding

    When I was an apprentice 50 years ago, oxy/act pipe welding was still being used.
    One oldtimer on the job told a young smart-*** stick welder he could do a 6" schedule 40 pipe weld faster with oxy/act.
    The kid said Ok.
    Well the old guy was done faster. I don't know by how much but it was something to see a one pass gas weld on 6" pipe.
    Talk about some heat !!


    Sent from my iPhone using Tapatalk

  9. #6
    Join Date
    Jul 2007
    Location
    Murphysboro, IL
    Posts
    198
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by BD1 View Post
    When I was an apprentice 50 years ago, oxy/act pipe welding was still being used.
    One oldtimer on the job told a young smart-*** stick welder he could do a 6" schedule 40 pipe weld faster with oxy/act.
    The kid said Ok.
    Well the old guy was done faster. I don't know by how much but it was something to see a one pass gas weld on 6" pipe.
    Talk about some heat !!


    Sent from my iPhone using Tapatalk
    That would have been impressive, I bet it wasn't the little skinny filler rods I learned on.

  10. #7
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,233
    Post Thanks / Like

    Re: Oxy Acetylene welding

    I like Oxy Acetylene welding I do not need a welding helmet.
    Most never run across being on job where all electric welding is band. Oxy Acetylene welding is good skill.

    Dave

    Quote Originally Posted by Birdhunter1 View Post
    I finally bought a torch setup, I’ve wanted one a long time but always been able to manage to get stuff to my uncles shop or a cousins place to use theirs.

    OA welding is how I learned my freshman year of high school in 1994, haven’t welded anything OA since probably 1998 though I have brazed a lot of stuff.
    Tonight I figured I’d teach my son who’s in the 6 th grade, I told him if he can learn this he can learn any of it. Watch the puddle, use the flame to move it, etc etc etc.
    Ran a puddle bead then said have at it. I don’t think his first hour of class tonight was bad at all. 1/4” mild steel


    Sent from my iPhone using Tapatalk
    Last edited by smithdoor; 6 Days Ago at 12:47 PM.

  11. #8
    Join Date
    Nov 2009
    Location
    Hellinois
    Posts
    5,784
    Post Thanks / Like

    Re: Oxy Acetylene welding

    When I got rid of all of my acetylene cylinders, I kept one small 80cf. Someday I will try gas welding and also brazing.
    "Where's Stick man????????" - 7A749
    "SHHHHHH!! I sent him over to snag that MIC-4 while tbone wasn't looking!" - duaneb55
    "I have bought a few of Tbone's things unlike Stick-Man who helps himself" - TozziWelding
    "Stick-man"

  12. #9
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    9,564
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by Birdhunter1 View Post
    That would have been impressive, I bet it wasn't the little skinny filler rods I learned on.
    I think the filler was 1/8 or 5/32. The old guy worked for the only shop that still did all gas welding. His speed and the end results were amazing. He was from Batron Rouge Louisiana. I'll never forget him.


    Sent from my iPhone using Tapatalk

  13. Likes whtbaron liked this post
  14. #10
    Join Date
    Oct 2014
    Posts
    3,034
    Post Thanks / Like

    Re: Oxy Acetylene welding

    O/A welding was part of my apprenticeship. You had to weld a 2" pipe in the 5G position and it had to have 100% penetration and pass a bend test. I think the pipe was around 10 gauge. I warped/melted my goggles from the reflected heat.

  15. #11
    Join Date
    Mar 2011
    Posts
    216
    Post Thanks / Like

    Re: Oxy Acetylene welding

    In my younger days almost all light tin work and car body work was oxy /acet I suppose now that has mostly been
    taken over by mig or tig. It's a pity to see all that skill disappearing nowadays

  16. #12
    Join Date
    Dec 2007
    Location
    Los Angeles
    Posts
    7,989
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by Birdhunter1 View Post
    I did have some 16 gauge tube he was first trying on and kept burning holes in it. I knew that 1/4” he wouldn’t burn through, once he got a puddle it was like a big AH HA moment and he said ‘THERE IT IS’ and I said make it dance.

    Nothing to brag about but he was definitely seeing a puddle and trying to make it move. He did puddle a bead about 4” across that plate.

    When I learned we had 16 gauge x 1” wide pieces. Laps, butts, uphill horizontal and maybe overhead welding and brazing.


    Sent from my iPhone using Tapatalk
    It is everything to brag about!! Good job.

    It is time with your kid and sounds like he enjoyed it.

    that's all that matters.


    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Miller 125c Plasma 120v
    SO 2020 bender
    Beer in the fridge

  17. Likes whtbaron liked this post
  18. #13
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    7,143
    Post Thanks / Like

    Re: Oxy Acetylene welding

    My first oxy welding was on a Jeep. It was rusted to oblivion. All that was left to save was the rear floor, and the top edge of the side panels. With a neighbor's advice, I cut away everything but the top edges. All the new was 16 gauge (1/16" thick, .0625"). Dad bought me that Jeep at age 13. I still have it 51 years later. The paint on that body is not pristine, but it is still VERY solid.

    Name:  keep.jpg
Views: 233
Size:  69.9 KB

    My daughter in law gave me this drawing at Christmas. The sort of faded blue is near accurate. Youngest son is currently reviving it. It has been in dry storage a few years. Mice made their home in the carburetor. Not a pretty sight! Basically, it is 1947, but there are parts from many sources, a bit like Johnny Cash's Cadillac.
    Last edited by Willie B; 6 Days Ago at 08:42 PM.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  19. #14
    Join Date
    Jul 2007
    Location
    Murphysboro, IL
    Posts
    198
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by Broccoli1 View Post
    It is everything to brag about!! Good job.

    It is time with your kid and sounds like he enjoyed it.

    that's all that matters.


    On that you are correct, we do about everything together, hes becoming my top hand on the farm.
    I told him this is how I first learned to weld in 1994 in my freshman year of high school, you'll have a leg up when you get to that class in 3 years as you'll have already done this.

    At 12 years old him and my 10 year old daughter have their own sweet corn patch, my daughter routinely does the daily chores with the horses and my son often runs the tractor while I'm the ground man.


    Not long ago we were doing something and they asked 'why do we have to do this' and I replied 'so that when you're at your first paying job and minimum wage is $15 an hour then by God you won't be the lazy *** and you'll be worth paying $15 dollar an hour.'

  20. Likes Broccoli1, whtbaron, Willie B liked this post
  21. #15
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    3,519
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by BD1 View Post
    I think the filler was 1/8 or 5/32. The old guy worked for the only shop that still did all gas welding. His speed and the end results were amazing. He was from Batron Rouge Louisiana. I'll never forget him.


    Sent from my iPhone using Tapatalk
    When I took Auto Body in the 70's it was still all O/A. I believe we used copper coated steel rods at 1/8". For practice we would slice up old hoods and fenders into strips and butt weld the pieces.
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  22. #16
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,743
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by BD1 View Post
    When I was an apprentice 50 years ago, oxy/act pipe welding was still being used.
    One oldtimer on the job told a young smart-*** stick welder he could do a 6" schedule 40 pipe weld faster with oxy/act.
    The kid said Ok.
    Well the old guy was done faster. I don't know by how much but it was something to see a one pass gas weld on 6" pipe.
    Talk about some heat !!


    Sent from my iPhone using Tapatalk
    Geez, that's impressive.
    My first welder was a torch, stick came later.
    So I welded up some heavy stuff with a torch and it's certainly hot after a while.

    Made tire chains for my truck, fixed stuff, etc.

    Welded the box sides on my 77 F150 with it too.
    They tend to break and rip metal at the corner of the tailgate.
    The metal had zippered up the sides a few inches too.

    OP: good for you and your kiddo - shop time is fun time
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  23. Likes Willie B liked this post
  24. #17
    Join Date
    Sep 2011
    Location
    Jasper TX
    Posts
    1,605
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by Birdhunter1 View Post
    On that you are correct, we do about everything together, hes becoming my top hand on the farm.
    I told him this is how I first learned to weld in 1994 in my freshman year of high school, you'll have a leg up when you get to that class in 3 years as you'll have already done this.

    At 12 years old him and my 10 year old daughter have their own sweet corn patch, my daughter routinely does the daily chores with the horses and my son often runs the tractor while I'm the ground man.


    Not long ago we were doing something and they asked 'why do we have to do this' and I replied 'so that when you're at your first paying job and minimum wage is $15 an hour then by God you won't be the lazy *** and you'll be worth paying $15 dollar an hour.'
    That's great parenting there, well done!
    Owner of Fast Leroy's Bar and Grill
    Liquor up Front, Poker in the Rear

  25. #18
    Join Date
    Nov 2004
    Location
    Southern Montana
    Posts
    938
    Post Thanks / Like

    Re: Oxy Acetylene welding

    I used O/A to fuse coat hangers and utility wire to join EMT when making the frame for my first recumbent bicycle, because that's all I had. Fortunately, none of the joints failed.

  26. #19
    Join Date
    Jul 2008
    Posts
    2,685
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by Stick-man View Post
    When I got rid of all of my acetylene cylinders, I kept one small 80cf. Someday I will try gas welding and also brazing.
    Brazing is a key skill IMHO. I don't know what I would have done without it on a lot of jobs.

    One of the nice things about it is that it's like glue: Even if you screw up, you don't normally alter the substrate/workpiece in the process (as you do when welding), so you can just remove the glue and re-glue it.

  27. Likes tapwelder liked this post
  28. #20
    Join Date
    Nov 2009
    Location
    Hellinois
    Posts
    5,784
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by Kelvin View Post
    Brazing is a key skill IMHO. I don't know what I would have done without it on a lot of jobs.

    One of the nice things about it is that it's like glue: Even if you screw up, you don't normally alter the substrate/workpiece in the process (as you do when welding), so you can just remove the glue and re-glue it.
    What are some current day uses for it? I guess I have never had the need. I hear it's easy, but someday I will try it.
    "Where's Stick man????????" - 7A749
    "SHHHHHH!! I sent him over to snag that MIC-4 while tbone wasn't looking!" - duaneb55
    "I have bought a few of Tbone's things unlike Stick-Man who helps himself" - TozziWelding
    "Stick-man"

  29. #21
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,971
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Great for modding tools without destroying the tool. Making socket/wrench extensions.

    For ornamental stuff, it is a great indicator for when the surface is ground flush
    And still have substantial material inside the joint.

    I primarily braze with propane. Acetylene and propane work differently. Much smaller heat point with acetylene offering easier application of heat. Propane heats a wider surface, better fir sweatting.

  30. Likes whtbaron liked this post
  31. #22
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    3,519
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by tapwelder View Post
    Great for modding tools without destroying the tool. Making socket/wrench extensions.

    For ornamental stuff, it is a great indicator for when the surface is ground flush
    And still have substantial material inside the joint.

    I primarily braze with propane. Acetylene and propane work differently. Much smaller heat point with acetylene offering easier application of heat. Propane heats a wider surface, better fir sweatting.
    I never tried propane, it was always acetylene, but when I worked I liked the small tips for detail work.... like 00 or 000 .
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  32. #23
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,971
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Name:  Curling iron with model.jpg
Views: 58
Size:  53.1 KB

    Here I decided to braze for ease of cleanup and blending. Mild steel. With brass lug. 3 parts.

  33. Likes whtbaron liked this post
  34. #24
    Join Date
    Nov 2004
    Location
    Southern Montana
    Posts
    938
    Post Thanks / Like

    Re: Oxy Acetylene welding

    Quote Originally Posted by Stick-man View Post
    What are some current day uses for it? I guess I have never had the need. I hear it's easy, but someday I will try it.
    Handy option for repairing cast iron, and joining small steel parts, if you don't have tig.

  35. Likes whtbaron liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,611,116,653.99716 seconds with 14 queries