    Can i hook a spoolmatic 3 directly to a TB302 or do i need more,like a WC-24?
    Thanks Mike

  2. #2
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,402
    Post Thanks / Like

    Re: TB302/Spoolmatic 3

    Yes to your first question. The 15/30A spoolgun requires the WC-24.