    NH 650 Baler Wheel Rebuild

    I guess it's time to bore y'all to tears again

    Name:  wheel1.jpg
Views: 2971
Size:  184.5 KB

    The wheel is in better shape than the one that's on the loader, but it's still reached the end of its useful life. The hub is also damaged, and will need a rebuild.

    This style wheel is available relatively reasonably priced https://www.ebay.com/itm/6-Hole-Farm...4383.l4275.c10 The problem is the offset. I'll have to verify tomorrow, but I believe the standard implement wheel has less offset.

    I'm pretty sure I can come up with a new hub, but I'm not sure. New Holland is pretty famous for "obsoleting" parts for balers, and other hay equipment.

    Either way......it's a few hundred dollars to get all the parts together, If they're available. The NH 650 is circa sometime in the 1990's.

    The idea of just slapping on a reinforcing ring, which is pretty widely available, is real tempting.........but the hub damage precludes it. There's no way around rebuilding the hub, and installing automotive style press-in studs.........which I can't find in the proper length to match a reinforcing ring.
    Last edited by farmersammm; 10-22-2020 at 11:26 PM. Reason: changed the title

  2. #2
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    783
    Post Thanks / Like

    Re: NH 650 Baler Wheel Rebuild

    If you ever got a simple swap out repair you'd have nuthin to post about or use for your repair shop tools and machines. Then with all that spare time you'd have to do a yard tidy up and cut the grass. Better this way.

  3. #3
    Join Date
    Sep 2015
    Location
    SE Pa
    Posts
    1,918
    Post Thanks / Like

    Re: NH 650 Baler Wheel Rebuild

    Come on Sam I know you can make something to fix this . Cut the center out ,make a ring with appropriate holes weld in in ring ,done . 10 minutes 15 tops

  4. #4
    Join Date
    Mar 2009
    Posts
    384
    Post Thanks / Like

    Re: NH 650 Baler Wheel Rebuild

    Did you ever do the other loader wheel?

  5. #5
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: NH 650 Baler Wheel Rebuild

    Quote Originally Posted by Zimm View Post
    Did you ever do the other loader wheel?
    No, not yet.......it's holding on for now. Might have to get to it this Winter. The rebuilt one is working out fine.

  6. #6
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: Another Wheel

    First thing is to measure offset, and other key dimensions. Offset, required plate thickness, and disc diameter requirement.

    Name:  wheel2.jpg
Views: 2721
Size:  219.9 KB This is the tool I made for centering the new disc on the loader wheel rebuild. Having it already made has cut time on this project by hours already.

    Name:  wheel3.jpg
Views: 2704
Size:  191.0 KB It serves as a known straightedge at this point.

    Then I can rough out the center of the wheel. I'm just paring away the "high" points where the lug nuts go.

    Name:  wheel4.jpg
Views: 2711
Size:  197.5 KB

    I clean it up a skosh more, not much.......just enough to get in the ballpark.

    Name:  wheel5.jpg
Views: 2731
Size:  215.7 KB

    The template from the loader wheel rebuild lets me know I have enough meat left on the wheel.

    Name:  wheel6.jpg
Views: 2794
Size:  222.6 KB

    This is going very fast due to the tooling. I was curious as to how much it would matter.

  7. Likes AlabamaJoe liked this post
  8. #7
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: Another Wheel

    Now, I can rough out my new disc blank.

    Name:  wheel7.jpg
Views: 2700
Size:  224.7 KB The blank is made from 3/4" plate so that I have shoulders to weld to when the finished disc is attached to the wheel.

    I don't try to cut something like this in one go around. I do it in manageable arcs where my arm/hands are comfortable.

    Tomorrow the plate will be remarked, and ground to those marks...........then off to the Uranus Global Master Machinist Center

  9. Likes Lis2323 liked this post
  10. #8
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    939
    Post Thanks / Like

    Re: Another Wheel

    That is where having a turntable to spin that as you cut would be a huge benefit. Still far better than any torch cutting i could do
    -Dave
    XMT304 with: 22A Feeder, or HF251 Hi Freq DC TIG air cooled

  11. #9
    Join Date
    Sep 2015
    Location
    SE Pa
    Posts
    1,918
    Post Thanks / Like

    Re: Another Wheel

    I knew you had something in mind

  12. #10
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: Another Wheel

    Re drew the circle for grinding to the right size. I never get the cut on the money the first time around. I just don't do round stuff for crap

    Name:  wheel8.jpg
Views: 2678
Size:  233.5 KB I always cut outside the line, but sometimes I go too far outside, and it makes for extra grinding.

    Name:  wheel9.jpg
Views: 2676
Size:  209.1 KB

    All dug in for the Winter I guess Name:  itsok.gif
Views: 2520
Size:  1.3 KB

    Name:  wheel10.jpg
Views: 2627
Size:  204.8 KB

    Spent some time examining my navel, and deciding how I'm gonna work with the hub. It's not a true hub piloted wheel like the loader. The centering shoulder isn't really solid...........more of a raised ring. But, I'm thinking that it's probably capable of supporting quite an axle load.

    Name:  wheel11.jpg
Views: 2706
Size:  219.0 KB This is the good hub, but it's the usual drill. The guy chowdered (I love that word) the threads on the bad one, and hammered some bolts into the holes to hold the wheel like a stud would. So.......have to bore out the bad holes for studs.

  13. #11
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: Another Wheel

    Had some time to work on the wheel insert today.

    Blank needs 3 holes. Two for clamping it to the rotary table, and one center hole for indicating.

    Name:  wheel12.jpg
Views: 2372
Size:  175.7 KB For less than dead nutz.....the wiggler makes a fine tool to line up on a punch mark.

    Name:  wheel13.jpg
Views: 2363
Size:  217.4 KB

    Name:  wheel14.jpg
Views: 2369
Size:  235.0 KB

    The table is centered next..............

    Name:  wheel15.jpg
Views: 2340
Size:  194.5 KB Sometimes I'll sweep the hole with a "Last Word", but generally a coax is just as accurate. Gotta remember that indicators are just comparators..............whether they're accurate as to thousands is irrelevant........what matters is that they're repeatable. I don't run the mill to use the coax......instead, I loosen the belts,, and hand spin the spindle....slower, and more accurate.

  14. Likes Joegreen02 liked this post
  15. #12
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: Another Wheel

    The annular cutter caught some serious chips as it worked.........leaving a rough bore.

    Name:  wheel16.jpg
Views: 2360
Size:  221.4 KB Luckily, the beginning of the bore was good, and made a reliable place to indicate off of.

    Name:  wheel17.jpg
Views: 2353
Size:  197.3 KB This is where I get my TRUE center. The inital hole was within whatever..........but everything else has to be accurate from here on. Everything is based on this center.

    Name:  wheel18.jpg
Views: 2363
Size:  239.6 KB

    Name:  wheel19.jpg
Views: 2363
Size:  193.5 KB After drilling, the holes are chamfered to take the lug nut.

  16. #13
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: Another Wheel

    Somebody on the forum recommended a single blade cutter for chamfering sometime back. Again........THANKS! (forgot who it was )

    Name:  wheel20.jpg
Views: 2361
Size:  172.7 KB

    Name:  wheel21.jpg
Views: 2358
Size:  203.9 KB

    Name:  wheel22.jpg
Views: 2365
Size:  227.7 KB The chamfers are carefully made in order to give full bearing to the lug nut. Not too far down, and not too far above the surface of the plate.

    Ready for the lathe work...........

    Name:  wheel23.jpg
Views: 2396
Size:  197.4 KB

    Quick check to ascertain just how much more of the wheel center needs to be ground out, and whether the blank has sufficient meat around the circumference to cut it down to size.

    Name:  wheel24.jpg
Views: 2419
Size:  244.0 KB

  17. Likes N2 Welding liked this post
  18. #14
    Join Date
    Apr 2011
    Location
    minnesota
    Posts
    2,098
    Post Thanks / Like

    Re: Another Wheel

    Could your replacement disk be made to fit in the lathe to true up the od or is it not worth the hassle
    Millermatic 252
    millermatic 175
    miller 300 Thunderbolt
    lincoln ranger 250
    smith torches
    lots of bfh's
    If it dont fit get a bigger hammer

  19. #15
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: Another Wheel

    Quote Originally Posted by farmshop View Post
    Could your replacement disk be made to fit in the lathe to true up the od or is it not worth the hassle
    I have a fixture I made for the lathe that's set up to hold this sort of thing. I made it when I did the front wheel on the loader.

  20. #16
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: Another Wheel

    I've looked at everything in the tool kit for a way to drop the thickness of the plate. It's driven me nuts for about a year.

    Drop the thickness, and you're lookin' at welding an open root..........not welding to shoulders (fillet). AN OPEN ROOT ON SOMETHING LIKE THIS WILL BEND THE RIM LIKE A PRETZEL. I mean, not INCHES, but enough to mess it up. I just don't feel comfortable with it.

    The rims are two pieces as they come from the factory. The 4 tabs are welded to the outer rim, and not subject to much dimensional change. You start filling gaps, and ya got mondo shrinkage.

    It's bad enough that I have a gap due to fitup..............I hate to hang the whole thing on filling those gaps, and nothing else.

  21. Likes Joegreen02 liked this post
  22. #17
    Join Date
    May 2017
    Location
    Pitman PA
    Posts
    763
    Post Thanks / Like

    Re: Another Wheel

    Sam...if there is anyone that can figger out how to do stuff this its you...Ive seen some of what you do and it amazes me you got the patience to do that stuff

  23. Likes farmersammm, Lis2323, Dave66 liked this post
  24. #18
    Join Date
    Feb 2016
    Location
    Myrtle Beach
    Posts
    899
    Post Thanks / Like

    Re: Another Wheel

    I always enjoy your projects!
    Lincoln 350MP
    Millermatic 350P
    Syncrowave 250
    1969 SA200
    HTP Invertig 221

  25. Likes whtbaron, farmersammm liked this post
  26. #19
    Join Date
    Aug 2014
    Location
    BC Canada
    Posts
    14,711
    Post Thanks / Like

    Re: Another Wheel

    Quote Originally Posted by Capt B View Post
    I always enjoy your projects!
    Same here!


    Sent from my iPad using Tapatalk
    :

  27. Likes Capt B, farmersammm liked this post
  28. #20
    Join Date
    Aug 2011
    Location
    North Central Mo
    Posts
    409
    Post Thanks / Like

    Re: Another Wheel

    Sam do you have any heat in your container? I have a trailer that i have some of my tools in lathe,a mill,shaper,drill press and other junk. It has plywood on the walls.I thought about putting in some kind of sealing so maybe i could heat it.

  29. #21
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    14,972
    Post Thanks / Like

    Re: Another Wheel

    Quote Originally Posted by Old Doug View Post
    Sam do you have any heat in your container?
    LOL.... I just wasn't sure where this was going... sounds sooo suggestive! Sorry.... I'll be quiet now... for awhile anyway...
    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Vevor MIG 200A
    Victor Medalist 350 O/A
    Vevor Cut 50 Plasma
    Les

  30. Likes ronsii, 12V71 liked this post
  31. #22
    Join Date
    Aug 2014
    Location
    BC Canada
    Posts
    14,711
    Post Thanks / Like

    Re: Another Wheel

    Quote Originally Posted by whtbaron View Post
    LOL.... I just wasn't sure where this was going... sounds sooo suggestive! Sorry.... I'll be quiet now... for awhile anyway...
    Sheesh. It's only mid November. Gonna be a looong winter......


    Sent from my iPhone using Tapatalk
    :

  32. Likes ronsii, 12V71, whtbaron liked this post
  33. #23
    Join Date
    Apr 2016
    Location
    CA
    Posts
    12,117
    Post Thanks / Like

    Re: Another Wheel

    Were all the holes wallowed out? I’m wondering if it would have just been easier to cut some flat plates into thick weldable washers and bolt them into place on the wheel using the lug nuts then weld into place, or is there too much weight on the wheels for that to work i.e. cracking etc?

    Thinking of a way I’d try the repair with out all those fancy shop machines.
    Last edited by N2 Welding; 11-19-2020 at 10:18 PM.
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  34. Likes 12V71 liked this post
  35. #24
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    8,196
    Post Thanks / Like

    Re: Another Wheel

    Quote Originally Posted by N2 Welding View Post
    Were all the holes wallowed out? I’m wondering if it would have just been easier to cut some flat plates into thick weldable washers and bolt them into place on the wheel using the lug nuts then weld into place, or is there too much weight on the wheels for that to work i.e. cracking etc?

    Thinking of a way I’d try the repair with out all those fancy shop machines.
    Most of those six hole implement wheels are available aftermarket for $80 give or take. About the same for most hubs from the local bearing house.

  36. Likes ronsii, N2 Welding liked this post
  37. #25
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,347
    Post Thanks / Like

    Re: Another Wheel

    Man! Thats a **** ton of work for a wheel. I dont envy you those repairs. A small cnc plasma machine would make your life a fair bit easier. I have made low speed wheel centers with that and an ironworker and haven’t had any problems at all.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,261,634.02378 seconds with 21 queries