I did find 1 more thing to try in another thread, with power set to max knobs turned all the way up , hf off , soft start off in dc max the thread said it should weld, only sparks when the electrode hits the work.
I think I have read all the posts for this machine or the ones that show up when I search for TIG300/300 or 7723-c