    So I have been looking into the Everlast PowerPro 256 and I think I am ready to purchase one. Although one of my concerns is about the welding torch. It comes with the Water cooled torch but not the water cooler (an additional $1300). Because of this, I have been looking into the air cooled torches. Is this a good idea? or is there a reason why the welder comes with the water cooled torch?

  2. #2
    Join Date
    Jul 2011
    Location
    Long Island, Socialist Republic of NY
    Posts
    2,908
    Post Thanks / Like

    Re: Tig Welding Torch (air cooled vs. Water cooled)

    See this

    http://weldingweb.com/vbb/showthread.php?t=124011

    Water cooled torches are tougher to set up and require more equipment, but have higher duty cycles and smaller/more maneuverable designs than air cooled torches of the same amperage.
    TA Arcmaster 300
    CM3
    XMT 304
    S22P12 suitcase feeder
    X-Treme 12VS
    Optima pulser
    TA161S
    Maxstar 150STL
    Hypertherm PM45
    OP setup
    Stihl 020AVP, 039, 066 Magnum

  3. #3
    Join Date
    Feb 2008
    Location
    North of Philly
    Posts
    20,159
    Post Thanks / Like

    Re: Tig Welding Torch (air cooled vs. Water cooled)

    Just one of a long list of many unsatisfied customers... We'd point you towards other threads but unfortunately "problem" threads often got moved to their section where that company has editing privileges and they are promptly deleted.

    Do your home work carefully before you go and plunk down your hard earned money. Some are willing to gamble that they won't have any issues with the machine they order, but personally it's not worth it.
    .



    No government ever voluntarily reduces itself in size. Government programs, once launched, never disappear. Actually, a government bureau is the nearest thing to eternal life we'll ever see on this earth!

    Ronald Reagan

  4. #4
    Join Date
    Jul 2011
    Location
    Wv near ohio river
    Posts
    237
    Post Thanks / Like

    Re: Tig Welding Torch (air cooled vs. Water cooled)

    If 256 means amps output 25% duty cycle then it probably maxes out close to 300 amps. An air cooled torch big enough to take those amps probably is more expensive than a water cooled one. The collets gas lenses etc for a 150 amp air cooled are generally the larger size that is carried at local welding shops. Search my more recent posts, I put up a picture of a total loss water cooled torch set up.

  5. #5
    Join Date
    Dec 2011
    Posts
    275
    Post Thanks / Like

    Re: Tig Welding Torch (air cooled vs. Water cooled)

    Quote Originally Posted by walkerTX View Post
    So I have been looking into the Everlast PowerPro 256 and I think I am ready to purchase one.
    Don't expect a refund.

  6. #6
    Join Date
    May 2012
    Location
    south jersey
    Posts
    28
    Post Thanks / Like

    Re: Tig Welding Torch (air cooled vs. Water cooled)

    i'm a rookie but it really depends on what your expected uses of the torch is. i won't comment on the machine save to say i personally wouldn't invest in a machine made offshore (if it is).

    the syncrowave 250 i brought used came with a gas cooled torch and they're fine if you don't plan on doing a lot of higher (>100-125) current welding, if you are invest in a water cooled torch. for me the main drawback of the water torch is the heavier cable assembly. i purchased a HW-20 for a water cooled because i don't often do heavy stuff and i like the more compact torches.

    for a cooler i purchased a B&M plate type transmission cooler, a stainless food service pan with lid and a carpet cleaner pump. all the parts cost me less than $200 and i wanted to do it this way because i have the machine under my bench so this keeps a very low profile. everything mounted under the machine and the cooling fan for the machine draws air through the trans cooler. i also installed a pressure gauge and hobbs type pressure switch so if for some reason the cooling system fails it shuts down the ARC.

    the water cooled torch runs a LOT cooler than the gas cooled.

    i recently purchased a CK-9 gas cooled torch with the superflex cable and for $65 i am happy with it.

  7. #7
    Join Date
    Apr 2010
    Location
    The Peoples Republic of Kalifornia
    Posts
    3,246
    Post Thanks / Like

    Re: Tig Welding Torch (air cooled vs. Water cooled)

    Quote Originally Posted by walkerTX View Post
    So I have been looking into the Everlast PowerPro 256 and I think I am ready to purchase one. Although one of my concerns is about the welding torch. It comes with the Water cooled torch but not the water cooler (an additional $1300). Because of this, I have been looking into the air cooled torches. Is this a good idea? or is there a reason why the welder comes with the water cooled torch?
    Your first rookie mistake

    Buying junk
    Backed my CATMA over your CARMA oops clusmy me

    What would SATAN do ??


    Miller Trailblazer 302 AirPak
    Miller Digital Elite
    Optrel Welding Hat
    Arcair K4000
    Suitcase 12RC / 12 VS
    Hypertherm PM-45
    Rage 3 saw
    Rusty old Truck

  8. #8
    Join Date
    Dec 2011
    Location
    S.W. Michigan
    Posts
    386
    Post Thanks / Like
    Quote Originally Posted by killdozerd11 View Post
    Your first rookie mistake

    Buying junk
    How long ago did you buy yours?
    Hammer
    File
    Big Hammer
    ------------------------------
    Here, let me Google that for you...

  9. #9
    Join Date
    Apr 2010
    Location
    The Peoples Republic of Kalifornia
    Posts
    3,246
    Post Thanks / Like

    Re: Tig Welding Torch (air cooled vs. Water cooled)

    Quote Originally Posted by lamename View Post
    How long ago did you buy yours?
    My father was a pipeline welder with a a 400 amp Hobart that i learned on starting at 8 years old

    My first personally owned welder was a 180 Lincoln with the 2 cylinder hand crank motor .
    I was 15 when i bought it

    My second was a Lincoln 225 weld n power
    Bought it when i was 20 something

    My third is the Miller TB 302 Air Pak
    Now i'm over 50 years old and still don't know much

    All other welders that i have used were owned by the people that employed me

    Or places that i was learning at
    Last edited by killdozerd11; 06-09-2012 at 01:12 AM.
    Backed my CATMA over your CARMA oops clusmy me

    What would SATAN do ??


    Miller Trailblazer 302 AirPak
    Miller Digital Elite
    Optrel Welding Hat
    Arcair K4000
    Suitcase 12RC / 12 VS
    Hypertherm PM-45
    Rage 3 saw
    Rusty old Truck

  10. #10
    Join Date
    Jan 2010
    Location
    The Tombs
    Posts
    281
    Post Thanks / Like

    Re: Tig Welding Torch (air cooled vs. Water cooled)

    I sure wouldn't shell out no $1,300.00 for a cooler, you can get a name brand working used ones for ~$300 if you play your cards right...... I know nothing about Everlast except their amp pedals look cheap and clunky
    SQUARE WAVE 175 TIG
    DUAL MIG 151

  11. #11
    Join Date
    Jul 2011
    Location
    Utah
    Posts
    2,190
    Post Thanks / Like

    Re: Tig Welding Torch (air cooled vs. Water cooled)

    Do what I did.

    Get the everlast, throw away the junk torch (or try to get a discount by not getting a torch), buy an awesome 250amp WP-20f torch with rubber leads on ebay for $90, make your own simple and excellent working water cooler for about another $100.

    http://weldingweb.com/vbb/showthread.php?t=58517
    Welding/Fab Pics: www.UtahWeld.com

  12. #12
    Join Date
    May 2008
    Location
    Matthews NC
    Posts
    40
    Post Thanks / Like

    Re: Tig Welding Torch (air cooled vs. Water cooled)

    I just built a tig cooler,I got the plans off of one of the welding sites.I cost about $100.00 if that.Most of the stuff was from the garbage/junk pile.I just got it working yesterday although I have not welded yet.The torch ,WP-20 feels alot more comfortable and is smaller than the WP -17.I will try and post a picture later on.I searched pretty hard for a used one but they wanted almost as much a s new one IF they were available.I welded with a water cooled torch,its seamed alot less bulky and more easy to manuver compared to the air cooled.
    Last edited by LIGoomba; 06-11-2012 at 12:29 PM.

  13. #13
    Join Date
    Jan 2010
    Location
    The Tombs
    Posts
    281
    Post Thanks / Like
    Defiantly would like to see pics of this cooler you bought/got(?) plans for, I thought about building my own but after adding costs of parts and material (because I just don't have these parts laying around) I would come in the same price for a working used one, I opted for the assembled working used one, haven't looked back
    SQUARE WAVE 175 TIG
    DUAL MIG 151

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Tags for this Thread

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,310,670.04773 seconds with 19 queries