    Re: Welding Fail! post pics here.

    If breaks free just use JB Weld it look great. Just do not stand under the shelf

    Dave

    Quote Originally Posted by dhem View Post
    Saw some good welds on the floor model Husky "Heavy Duty Industrial" shelving unit at my local Home depot:

    Attachment 1730711

    Attachment 1730712

    Attachment 1730713

  2. #2602
    Join Date
    May 2020
    Location
    Arizona
    Posts
    998
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by SweetMK View Post
    I wish I knew where I could get a large steel sphere,,

    I would build that in a heartbeat, and add it to my driveway entrance,,,

    https://customironworks.com/balls-st...810-p-437.html
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  3. #2603
    Join Date
    Sep 2015
    Location
    West coast of Florida
    Posts
    528
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by psacustomcreations View Post
    Is this a fail?? Trying to keep a tight arc and this happens.



    Sent from my SM-G996U using Tapatalk
    Technically yes, but it can be easily overlooked
    Richard
    West coast of Florida

  4. Likes psacustomcreations liked this post
  5. #2604
    Join Date
    Mar 2008
    Location
    Georgetown, Texas
    Posts
    2,033
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Stopped at a country store a couple days ago and saw this on the bollard pipes protecting the gas pumps. Oh yeah, they're well protected.
    Attached Images Attached Images  

  6. Likes 12V71, whtbaron liked this post
  7. #2605
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    8,119
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Bob View Post
    Stopped at a country store a couple days ago and saw this on the bollard pipes protecting the gas pumps. Oh yeah, they're well protected.
    A few more coats of paint, the gap will close.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  8. Likes 12V71, VaughnT, Shootr, Alphonse liked this post
  9. #2606
    Join Date
    Jan 2009
    Location
    Sonoma County
    Posts
    949
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Bob View Post
    Stopped at a country store a couple days ago and saw this on the bollard pipes protecting the gas pumps. Oh yeah, they're well protected.
    What is that, Bondo on there to smooth over the 'weld' ?

    Likely hit, weld tore open, repaired (sort of), several times.
    * Amico MIG-130A Flux, Dual Voltage. Truly portable!
    * HF MIG-180 with all the mods. Heavy.
    * Grizzly H8153 Stick/Tig 130/160.
    * Wards PowrKraft AC-230. Stick & carbon arc.

  10. Likes Alphonse liked this post
  11. #2607
    Join Date
    Sep 2009
    Location
    Cleveland, OH USA
    Posts
    58
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Here is a recent video of a E7018 "tack" weld of re-bar to 1" mild A36 steel that failed...FAILS @3:25 IN THE VIDEO
    Last edited by Alphonse; 11-12-2021 at 04:42 PM.
    Century AC/DC 250 Amp & Midstates 300 Amp Industrial AC stick welders, Century Flux core 80 amp. wire feed welder Harris Oxy-Acet. cutting & welding outfit:
    SEE MY INFORMATIVE VIDEOS AT http://www.youtube.com/user/alpho52

  12. Likes California liked this post
  13. #2608
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    4,073
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Just a little JB Weld will make look great.

    Dave

    Quote Originally Posted by Bob View Post
    Stopped at a country store a couple days ago and saw this on the bollard pipes protecting the gas pumps. Oh yeah, they're well protected.

  14. #2609
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    1,862
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    I can fill that crack.

  15. #2610
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    1,862
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    I dont know how I did it but has a little gap in this one,,, but I fill it, ha
    Attached Images Attached Images  

  16. #2611
    Join Date
    Mar 2008
    Location
    Georgetown, Texas
    Posts
    2,033
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Sberry View Post
    I can fill that crack.
    I could easily weld that gap up with a little Cajun tig welding.

  17. #2612
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    4,073
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    I would fill with welding.
    May be E6013 or E71T-11 or even brazing.

    Dave

    Quote Originally Posted by Sberry View Post
    I can fill that crack.

  18. #2613
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    5,837
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by smithdoor View Post
    I would fill with welding.
    May be E6013 or E71T-11 or even brazing.

    Dave
    Oh come on Dave.... lol, we know you want to use hot 7018's....
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  19. #2614
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    4,073
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    One I work in construction and E7018 runs smoother hot.
    If read all technical notes and do not heat why use E7018, just a different rod not so fussy like E7016 or E6013 no heat need.

    Dave

    Quote Originally Posted by whtbaron View Post
    Oh come on Dave.... lol, we know you want to use hot 7018's....

  20. #2615
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    5,837
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Plasma fail.... yea, this is what happens to the consumables when you get in a hurry and forget to open both valves to the air supply. They become consumed.
    Name:  IMG_7301 (2).jpg
Views: 922
Size:  109.2 KB
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  21. #2616
    Join Date
    Apr 2016
    Location
    CA
    Posts
    8,271
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    It’s a good thing they are cheap cost consumables.
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  22. Likes whtbaron liked this post
  23. #2617
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    6,032
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by N2 Welding View Post
    Itís a good thing they are cheap cost consumables.
    Am I the only one that keeps used plasma consumables around ? Have no idea why. Iím going to make a point of throwing them out.


    Sent from my iPad using Tapatalk
    :

  24. #2618
    Join Date
    Apr 2016
    Location
    CA
    Posts
    8,271
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    I have a couple used consumables laying around myself. Think I’m saving them for when I run out and need to order but the used ones will work well enough to separate two pieces quickly. I have yet to ever see the machine tell me the consumables need changed. Perhaps I don’t use them long enough to the point of meltdown. I still need a water separator etc for optimum clean dry air. ATM I just have the motorguard paper filter canister thing.
    Last edited by N2 Welding; 11-16-2021 at 12:20 PM.
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  25. #2619
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    5,837
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Lis2323 View Post
    Am I the only one that keeps used plasma consumables around ? Have no idea why. I’m going to make a point of throwing them out.


    Sent from my iPad using Tapatalk
    I just had that same discussion with myself. I think only the ceramics could be used again, so everything else is going. Questionable tips are only going to be hard on the machine.
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  26. #2620
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    1,004
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by psacustomcreations View Post
    Is this a fail?? Trying to keep a tight arc and this happens.





    Sent from my SM-G996U using Tapatalk

    Here's a tight one,

    Attachment 1733396

    This happened when I tripped over a hose, stepped all the way down on the pedal, and put my torch hand down on the aluminum by accident. I Didn't think it was that stuck, so I quickly flicked my wrist to free the tungsten.
    ooops.... Oh well got plenty of green tungsten left (lots came with the machine) This is the aluminum block I use to test to make sure everything is OK before I weld on an important piece. Good thing my torch didn't land on the top of the cabinet, at 250 amps there would probably be a big hole.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D
    Primeweld 225 ac/dc
    Primeweld mig180
    Miller AEAD-200

  27. Likes psacustomcreations, whtbaron liked this post
  28. #2621
    Join Date
    Mar 2008
    Location
    Georgetown, Texas
    Posts
    2,033
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    My step son bought a gym several months ago. Things have been breaking ever since. I was there a while back and he showed me something that broke. He said they had "fixed" it once as a little Lincoln welder came with the business to "fix" things. I welded it back with the little Lincoln and a hood that didn't even have head gear in it.
    Attached Images Attached Images   

  29. Likes mcspeed liked this post
  30. #2622
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    6,032
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Bob View Post
    My step son bought a gym several months ago. Things have been breaking ever since. I was there a while back and he showed me something that broke. He said they had "fixed" it once as a little Lincoln welder came with the business to "fix" things. I welded it back with the little Lincoln and a hood that didn't even have head gear in it.
    What is that? A 2Ē pipe for hanging weights?


    Sent from my iPad using Tapatalk
    :

  31. #2623
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,546
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Definitely a fail when the tungsten comes out of the side of the cup. I thought they were more prone to shattering.

  32. #2624
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    4,073
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    You think at sweet shop working 12 hour days 6 days a week the welder could do better job.

    Dave

    Quote Originally Posted by dhem View Post
    Saw some good welds on the floor model Husky "Heavy Duty Industrial" shelving unit at my local Home depot:

    Attachment 1730711

    Attachment 1730712

    Attachment 1730713

  33. #2625
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,546
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by smithdoor View Post
    You think at sweet shop working 12 hour days 6 days a week the welder could do better job.

    Dave
    What do you think the issue was? The consistently start bad the get better at the corner. Hot day moving away from the fan?

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,642,739,372.24732 seconds with 15 queries