    Re: Welding Fail! post pics here.

    Name:  657230B4-19BE-448F-82E4-EA4BAC6DE472.jpg
Views: 1175
Size:  78.9 KBName:  1741170B-C103-456B-A1B6-CFCB3F36EDEC.jpg
Views: 1180
Size:  52.1 KB impressive

  2. #2752
    Join Date
    Jun 2008
    Location
    Hardwood Lands, Nova Scotia, Canada
    Posts
    2,079
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Didn't want to risk bending the tube by over welding. No idea why it's not centered, I'd guess a FU. Gouges in the bar...an add on feature purely for looks ;-)........M

  3. #2753
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,440
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Tack let it cool tack let it cool tack let it cool if necessary. Very unprofessional

  4. Likes John T liked this post
  5. #2754
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,062
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by motolife313 View Post
    Tack let it cool tack let it cool tack let it cool if necessary. Very unprofessional
    I agree.
    (Imagine that)

    You go through all that trouble trying to figure out how to fix it ....

    Then dont even take the time to mock it up for proper fitment????

    Good grief.

    Id be embarrassed to post those pics ...

    Actually good thing moto quoted it
    Because I think he tried to delete them
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  6. #2755
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    7,786
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    I agree 👍
    It some most learn the hard way in beginning too.

    Dave

    Quote Originally Posted by motolife313 View Post
    Tack let it cool tack let it cool tack let it cool if necessary. Very unprofessional

  7. #2756
    Join Date
    Sep 2020
    Location
    VT
    Posts
    355
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Name:  PXL_20220813_222249648.jpg
Views: 848
Size:  123.9 KB

    Put your Mig on the wrong settings and give the gun to a monkey high on caffeine and you get high dollar artwork
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

  8. Likes whtbaron, LtBadd, VaughnT liked this post
  9. #2757
    Join Date
    Jan 2004
    Location
    South Central Kansas
    Posts
    450
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Sorry I did not get a photo of it, but I was very pissed at the time. While driving home late this last Friday night from an out of state football game, I ran over and hit something on the highway. I drove back to see what it was that I had ran over, and discovered it looked like someone had tried to repair a broken front bumper on a large truck. The bumper had been broken and the person that had tried to repair it with pigeon dropping welds had welded the break somewhat and then pigeon pooped welded 2 pieces of angle iron on the back side of the broken piece of bumper. The section that I hit was about 2' in length, about 10-12" wide, the two pieces of angle iron were about 1 1/2' each in length. They had about 8" of angle iron pigeon pooped welded to the back side of the piece of bumper that I hit and about 8" of each piece of angle iron that had been pigeon pooped to the bumper that was still attached to the truck. I disposed the piece that I ran over so that no one else would run over it.

    I am a hobby welder myself but I would have never welded anything together that poorly that would have been going up and down the highway. Please guys if you don't know how to weld do your practice welding on something other than that which could kill or injure others! I am sure I have some tire damage, but hopefully I did not damage anything else on my pickup.
    Last edited by gnewby; 3 Weeks Ago at 02:38 PM.

  10. Likes California liked this post
  11. #2758
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    9,001
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by gnewby View Post
    Sorry I did not get a photo of it, but I was very pissed at the time. While driving home late this last Friday night from an out of state football game, I ran over and hit something on the highway. I drove back to see what it was that I had ran over, and discovered it looked like someone had tried to repair a broken front bumper on a large truck. The bumper had been broken and the person that had tried to repair it with pigeon dropping welds had welded the break somewhat and then pigeon pooped welded 2 pieces of angle iron on the back side of the broken piece of bumper. The section that I hit was about 2' in length, about 10-12" wide, the two pieces of angle iron were about 1 1/2' each in length. They had about 8" of angle iron pigeon pooped welded to the back side of the piece of bumper that I hit and about 8" of each piece of angle iron that had been pigeon pooped to the bumper that was still attached to the truck. I disposed the piece that I ran over so that no one else would run over it.

    I am a hobby welder myself but I would have never welded anything together that poorly that would have been going up and down the highway. Please guys if you don't know how to weld do your practice welding on something other than that which could kill or injure others! I am sure I have some tire damage, but hopefully I did not damage anything else on my pickup.
    13 years ago Me & the Missus went from VT to Boston to a car dealer. They were advertising prices too good to be true.
    We were driving 70 MPH in several lanes of bumper to bumper traffic. We came to a high point on a hill. I could see down a long hill. Far ahead, I could see dozens of brake lights. All seemed at the same place. Soon it was our turn, we hit the object in the road like hundreds of cars before & hundreds after. I believe it was a bumper from a 1960s Volkswagen Beetle.

    I imagine millions of dollars damage to 1000s of cars before it could be removed.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  12. #2759
    Join Date
    Jan 2004
    Location
    South Central Kansas
    Posts
    450
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    I wasn't for sure just what I had hit when I ran over it, I am glad I went back and found out what it was and got it off of the hiway. From looking at the scuff marks on the hiway I would say I was not the only one that had ran over it. I carried it off of the hiway and set it along fence line.

    The company I worked for before I retired had a truck driver that lost driveline on the truck he was driving. Person behind him driving a Jetta hit it. His car was totaled out. Luckily the driver was not hurt, our company insurance payed out quite a bit.

  13. #2760
    Join Date
    Sep 2013
    Posts
    1,796
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    That's got to be embarrassing.....



    They should have used 7018's.

  14. Likes N2 Welding, whtbaron, motolife313 liked this post
  15. #2761
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    7,786
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Do not cut the ribbon 🎗 it holds the bride up.

    Dave

    Quote Originally Posted by VaughnT View Post
    That's got to be embarrassing.....



    They should have used 7018's.

  16. #2762
    Join Date
    Nov 2005
    Location
    ca
    Posts
    127
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Syncrowave 250 w/ coolrunner
    MM210 W/spoolgun
    SP 135
    Victor O/A
    Ramsond cut 50
    Titanium Stick 225.

  17. Likes N2 Welding liked this post
  18. #2763
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    7,786
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Must be a wood rod and he made a video 📹 too.

    Dave

    Quote Originally Posted by Tbones View Post

  19. #2764
    Join Date
    Sep 2013
    Posts
    1,796
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    I'm not saying you can't scavenge some truck frames to make a foot bridge support, but there's a reason why they say Found On Road Dead.....


  20. #2765
    Join Date
    Apr 2016
    Posts
    488
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    best part of the bridge collapse is the people in the background on the junky old bridge.... walking by like "see, told you this one was good enough"

  21. Likes VaughnT liked this post
  22. #2766
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,440
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    The guy did this in the flat position knowing he was supposed to weld in the horizontal 2g position Name:  FCE91615-03A1-45F2-AAFD-0CED53073B91.jpg
Views: 347
Size:  133.9 KBguess he was supplied with a short backer and he didnít wanna put it on even

  23. #2767
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    8,064
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    So do you have to re-do it, or is he going to have to learn from his mistakes?
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  24. #2768
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,440
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    He got told it’s over after that root pass.

  25. Likes 12V71, whtbaron, Lis2323, 52 Ford liked this post
  26. #2769
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    6,690
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by motolife313 View Post
    He got told it’s over after that root pass.
    I would hope so. Did it even stick?

  27. #2770
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    2,832
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    "Problems are like root welds. Bury them deep enough and it doesn't matter when the root looks like.

    Sent from my Lincoln Buzzbox using Tapatalk
    Last edited by 52 Ford; 1 Week Ago at 01:43 AM.

  28. #2771
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    1,031
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by whtbaron View Post
    So do you have to re-do it, or is he going to have to learn from his mistakes?
    During my welding training in the US Navy,, for the first few plates, they made us GRIND OFF THE 1/4" THICK BACKING STRIP before x-ray.

    I think that was to encourage us to learn how to make an adequate root pass, that could pass x-ray.

    If there was a root problem, the backing strip had to be removed, and the weld ground out, and fixed.
    I NEVER had another backing strip have to come off,,, some of those guys were gluttons for punishment, because of poor root welds.

  29. #2772
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,440
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Name:  E68ED0D1-C029-40F9-9F81-F78AAD85791F.jpg
Views: 252
Size:  98.2 KBName:  6E044824-640C-4DD5-9F81-9997D225E79C.jpg
Views: 251
Size:  80.9 KBI asked the qc guy if he was going to start writing novels. We stuck the worst guy under here and donte came to fix it. Kinda funny I fixed a bunch of his stuff today

  30. #2773
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    2,832
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by motolife313 View Post
    Name:  E68ED0D1-C029-40F9-9F81-F78AAD85791F.jpg
Views: 252
Size:  98.2 KBName:  6E044824-640C-4DD5-9F81-9997D225E79C.jpg
Views: 251
Size:  80.9 KBI asked the qc guy if he was going to start writing novels. We stuck the worst guy under here and donte came to fix it. Kinda funny I fixed a bunch of his stuff today
    I gotta say, being the QC guy sounds kinda fun. Getting PAID to judge other peoples welds. I've been doing that for free for YEARS!

    Sent from my Lincoln Buzzbox using Tapatalk

  31. #2774
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    2,832
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by 12V71 View Post
    I would hope so. Did it even stick?
    The spatter did.

    Sent from my Lincoln Buzzbox using Tapatalk

  32. #2775
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,440
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    They actually have about the hardest job. We all judge welds. Every time a guy takes a test most of us look at it

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,664,831,226.43832 seconds with 15 queries