    Re: Welding Fail! post pics here.

    Quote Originally Posted by whtbaron View Post
    I've tried that... too far from the cities full of people that want them. I've had ads out before... get people showing up that want to fill their trunk with little stones. The guys that move 100 tonne at a time want nicely sorted piles that are sized with no dirt. Oddly enough, that's not how stonepiles in the field grow. If they see the 6 to 8 footers they turn tail and run. Anyway... sorry for taking the thread off topic... somebody better rip some welding apart...
    I did get a Chinese fellow, wanted six boulders to "sit on". I asked if he was OK with where they are? Or did he have a special place in mind? In his version of English, he explained he wanted them along his driveway. I delivered. He "paid" me with a pottery coffee cup. WOW! (sarcasm).
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  2. Likes whtbaron, 52 Ford liked this post
  3. #2727
    Join Date
    Dec 2018
    Posts
    7,326
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by motolife313 View Post
    Attachment 1739665Attachment 1739666more of a cutting fail. They know how to make my job easy
    That they would tell you to weld that is the real sin. Even with the tack welds, it will still pull. And if it doesn't pull(you get lucky), the locked in stress makes for a failure sometime down the road.

  4. #2728
    Join Date
    Sep 2020
    Location
    VT
    Posts
    305
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by whtbaron View Post
    I've tried that... too far from the cities full of people that want them. I've had ads out before... get people showing up that want to fill their trunk with little stones. The guys that move 100 tonne at a time want nicely sorted piles that are sized with no dirt. Oddly enough, that's not how stonepiles in the field grow. If they see the 6 to 8 footers they turn tail and run. Anyway... sorry for taking the thread off topic... somebody better rip some welding apart...

    In 2019 I did the dirt work for a 40'x40' garage. We found some rocks. The customer put a message on Facebook that they were giving away rocks. I sent out 7 tandem axle dump truck loads of rocks that were 3 to 6 foot in size. There was only one rock too big for the Deere 120 to lift. It earned a permanent home in the stone wall nearest the garage. 4 of the loads were picked up by a contractor in NH, probably nearly an hour drive each way. I can't believe it was worth their while. The rocks were round river rocks, not nice slabs of ledge that make good looking walls.

    To keep the two topics together... A local quarry I buy aggregate from frequently just broke the boom on a Deere 300 excavator yanking on a rock the size of a tri axle dump truck. Not exactly a welding fail, but I'm sure it required a lot of welding to repair.
    Last edited by ArcTan; 05-20-2022 at 10:13 PM.
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

  5. Likes whtbaron liked this post
  6. #2729
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,274
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Name:  E365BB97-FF7A-44CC-B624-5E4A8F430B64.jpg
Views: 973
Size:  123.5 KBback of a jeep. Pretty bad

  7. Likes whtbaron, Roert42 liked this post
  8. #2730
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    7,105
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Am I the only one wondering what the rest of the decal on the tailgate says?
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  9. #2731
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,387
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Looks like a high class China 120 volt welding

    Dave

    Quote Originally Posted by motolife313 View Post
    Name:  E365BB97-FF7A-44CC-B624-5E4A8F430B64.jpg
Views: 973
Size:  123.5 KBback of a jeep. Pretty bad

  10. Likes motolife313 liked this post
  11. #2732
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    6,232
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by smithdoor View Post
    Looks like a high class China 120 volt welding

    Dave
    No, that's operator error. I had a little Lincoln 125 with .030 fluxcore (NR211) that did a fine job on lighter steels 3/16" and under. Amazing how people that don't weld think that gobbing pigeon poop like that makes a weld.

  12. Likes NotaVegetarian liked this post
  13. #2733
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,274
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    I think that’s what he meant. Welded in china

    And I don’t think think those kinda folks you’re talking about no any better obviously lol

  14. #2734
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    6,232
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by motolife313 View Post
    I think that’s what he meant. Welded in china

    And I don’t think think those kinda folks you’re talking about no any better obviously lol
    Seriously, I once saw a repair on a 350 psi high pressure air line that looked more goobered than that Jeep bracket. Owner could not understand why it leaked so much air.

  15. Likes whtbaron liked this post
  16. #2735
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    1,217
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Willie B View Post
    I did get a Chinese fellow, wanted six boulders to "sit on". I asked if he was OK with where they are? Or did he have a special place in mind? In his version of English, he explained he wanted them along his driveway. I delivered. He "paid" me with a pottery coffee cup. WOW! (sarcasm).
    Something about Fung Shui, maybe.

    To each their own. I don't judge. As long as he didn't as to have to pointy bit facing up on his sitting stones..


    You shoulda gotten some free Karate lessons out of him, anyway.

    Sent from my Lincoln Buzzbox using Tapatalk

  17. #2736
    Join Date
    Dec 2018
    Posts
    7,326
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    I have a ton of welding fail pics of this damn ramp I'm trying to modify...............but I'm too embarrassed to post them. Just horrible. (sigh)

  18. #2737
    Join Date
    May 2011
    Posts
    619
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by farmersammm View Post
    I have a ton of welding fail pics of this damn ramp I'm trying to modify...............but I'm too embarrassed to post them. Just horrible. (sigh)
    Create a new account and make fun of yourself when no one else knows.

  19. Likes farmersammm, Roert42 liked this post
  20. #2738
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,387
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    When saw it was welder error.
    But I put some of error Chinese welders thinking are need to buy a low cost 120volt welder makes you a pro.

    Dave

    Quote Originally Posted by 12V71 View Post
    No, that's operator error. I had a little Lincoln 125 with .030 fluxcore (NR211) that did a fine job on lighter steels 3/16" and under. Amazing how people that don't weld think that gobbing pigeon poop like that makes a weld.

  21. #2739
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,387
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    FYI
    I have own 120volt welder in pass and I can make good bead with the Chinese welder.

    Dave

    Quote Originally Posted by 12V71 View Post
    No, that's operator error. I had a little Lincoln 125 with .030 fluxcore (NR211) that did a fine job on lighter steels 3/16" and under. Amazing how people that don't weld think that gobbing pigeon poop like that makes a weld.

  22. #2740
    Join Date
    Jan 2009
    Location
    Sonoma County, Northern California
    Posts
    1,035
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by smithdoor View Post
    FYI
    I have own 120volt welder in pass and I can make good bead with the Chinese welder.

    Dave
    Yeah but ... AC, flux core, and a voltage switch with just two positions: too high / way too high?

    The HF 'MIG-100' and several similar versions before the present black ones, really weren't suitable to learn on.

    I could do adequate farm work with my AC buzzbox but when I bought the MIG-100 thinking it would be more convenient ... it wasn't.

    After I replaced that with a Century 130, 110v DC and still using flux core, I could finally do work that looked decent.

    DC and an adjustable voltage knob, seem to be the minimum specs for a 110v wire welder to be a useful shop tool.
    * Amico MIG-130A Flux, Dual Voltage. Truly portable!
    * HF MIG-180 with all the mods. Heavy.
    * Grizzly H8153 Stick/Tig 130/160.
    * Wards PowrKraft AC-230. Stick & carbon arc.

  23. Likes Roert42 liked this post
  24. #2741
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    505
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by smithdoor View Post
    When saw it was welder error.
    But I put some of error Chinese welders thinking are need to buy a low cost 120volt welder makes you a pro.

    Dave
    Don't even know wtf any of that means

  25. #2742
    Join Date
    Apr 2016
    Location
    CA
    Posts
    8,939
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Country Metals View Post
    Create a new account and make fun of yourself when no one else knows.
    WOW exposing your new account that’s not so new. Bravo FarmerSamm!
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  26. #2743
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    901
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by N2 Welding View Post
    WOW exposing your new account that’s not so new. Bravo FarmerSamm!

    ,,,,,,,,,,,,,,,, 0r, did you mean &1FarmerSammmmm,,,, `~`



  27. #2744
    Join Date
    Jul 2021
    Posts
    98
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by California View Post
    Yeah but ... AC, flux core, and a voltage switch with just two positions: too high / way too high?

    The HF 'MIG-100' and several similar versions before the present black ones, really weren't suitable to learn on.

    The only thing worse is those little "70amp" stick welders that have a two position amperage switch. "way too low" and "Is it even turned on?"
    Airco Auto-Pak 130

    Forney 235AC/DC

  28. #2745
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    6,811
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Roert42 View Post
    The only thing worse is those little "70amp" stick welders that have a two position amperage switch. "way too low" and "Is it even turned on?"
    Actually if you set them up for scratch start tig they work pretty good for sheet-metal or small steel repairs.

    I had the 90 amp version for a while and it was pretty convenient for on mobile quick fix.

    120 V you can plug it in anywhere.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  29. Likes Roert42 liked this post
  30. #2746
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    7,105
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    **Walks over to Dialarc..... turns dial up for 5/32 rods..... turns dial down for 3/32 rods.** I have no idea what you guys are complaining about. It has a hook on top. I have a loader. It's a portable.
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  31. Likes jay gill, Mikel_24 liked this post
  32. #2747
    Join Date
    Jul 2021
    Posts
    98
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by John T View Post
    Actually if you set them up for scratch start tig they work pretty good for sheet-metal or small steel repairs.

    I had the 90 amp version for a while and it was pretty convenient for on mobile quick fix.

    120 V you can plug it in anywhere.

    I could see that.

    You would have to drag the rod around a bit on the steel, like striking a match, to get it hot before you could start any welding. Using 1/16 6013. Once you got going it was ok, but a pita to restart.



    Airco Auto-Pak 130

    Forney 235AC/DC

  33. #2748
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,387
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    I could get good weld with 120v but on hot it flip the breaker a lot.

    Dave

    Quote Originally Posted by California View Post
    Yeah but ... AC, flux core, and a voltage switch with just two positions: too high / way too high?

    The HF 'MIG-100' and several similar versions before the present black ones, really weren't suitable to learn on.

    I could do adequate farm work with my AC buzzbox but when I bought the MIG-100 thinking it would be more convenient ... it wasn't.

    After I replaced that with a Century 130, 110v DC and still using flux core, I could finally do work that looked decent.

    DC and an adjustable voltage knob, seem to be the minimum specs for a 110v wire welder to be a useful shop tool.

  34. #2749
    Join Date
    Jun 2022
    Posts
    1
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Attached Images Attached Images  

  35. #2750
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    8,637
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by whtbaron View Post
    **Walks over to Dialarc..... turns dial up for 5/32 rods..... turns dial down for 3/32 rods.** I have no idea what you guys are complaining about. It has a hook on top. I have a loader. It's a portable.
    I miss my Dialarc!
    Somebody once said "There is no substitute for cubic inches." The Dialarc is the electrical equivalent of many cubic inches. It has power! I used one machine better for stick than Dialarc, by the time I owned it it suffered greatly from weather, it never welded again.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  36. Likes whtbaron liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,656,573,593.83306 seconds with 15 queries