    Part 1 of a bad day with made over seas crap. Changing master cylinder, little flimsy 3/8ths flare nut, found a 11mm HF made india open end because it was a more flush fit. Give a litt oomph and it opened right up, split the jaw off. Just a couple more like that and it'll be 100% of the end wrenches I've been given from there are officially crap.

    Oh BTW, chucked my 3rd and final HF grinder in the can about a week ago. Sparks, smoke and molten plastic came out of the back end where the cord goes in.
    Last edited by Sandy; 07-24-2010 at 08:03 PM.
    "The things that will destroy America are prosperity at any price, peace at any price, safety first instead of duty first, the love of soft living and the get rich quick theory of life." -Theodore Roosevelt

  2. #102
    Join Date
    Aug 2008
    Location
    Dansville NY
    Posts
    5,141
    Post Thanks / Like

    Re: HF Tools That Suck

    Gee Sandy I am glad I am not the only one that had bad luck with those HF 4 1/2" grinders. I stopped buying them for the shop trucks and went to Rigid which has a great warranty.
    Co-Own CNC shop:Miller :1251 plasma cutter, MaxStar 700 TIG/Stick, & XMT 456 Multiprocess Welder.& 2 Hypertherm HPR260's Plasma Cutter

    Sorry I had a bad stroke but now I am back.

  3. #103
    Join Date
    Aug 2010
    Posts
    6
    Post Thanks / Like

    Re: HF Tools That Suck

    when it comes to harbour break I stick with wrenches,hammers,scewdrivers etc... my rule of thumb is no HB products that plug in.

  4. #104
    Join Date
    Jan 2010
    Location
    The Tombs
    Posts
    281
    Post Thanks / Like

    Re: HF Tools That Suck

    Quote Originally Posted by rdoss1970 View Post
    harbour
    Like a fugitive?
    SQUARE WAVE 175 TIG
    DUAL MIG 151

  5. #105
    Join Date
    Mar 2007
    Posts
    13
    Post Thanks / Like

    Re: HF Tools That Suck

    Quote Originally Posted by PilotAlso View Post
    Moderators: Is there some kind of IGNORE feature to keep from having every attempt at providing real information regarding HF tools hijacked by PapaLion? Talk about drifting way, way off track and into stupid RANTS.
    ... let me see if I can help with the idiot savant that doesn't realize Nikita Khrushchev wasn't from China ...
    Attached Images Attached Images    
    Last edited by -lecroix-; 08-22-2010 at 01:02 AM.

  6. #106
    Join Date
    Nov 2009
    Location
    Arizona
    Posts
    2,754
    Post Thanks / Like

    Re: HF Tools That Suck

    Quote Originally Posted by DougAustinTX View Post
    The absolute MOST ANNOYING things that I have purchased at HF are the automatic tank bleeder/drains for the bottom of the air compressor. Made of solid brass so you think they will work, but the guts of the things start leaking within a couple of weeks. The floor around my compressor is littered with the rejects... which just goes to show what a dumb_*ss I am because I kept buying the same thing over and over thinking I would eventually get a good one. After FIVE attempts, I just gave up and plumbed a curved copper tube to the bottom of the tank with a quarter turn plumbing shutoff and I try to remember to drain the tank every month or so. I can't believe they keep selling those auto drains....
    HA! mine only lasted 3 days!!! I did notice the instructions said not to use over 100 PSI, who runs their compressor under 100 PSI???

    I've decided except for bungie cords and gloves, I won't be wasting my time with their tools any more.
    Miller Challenger 172
    Miller Thunderbolt AC/DC 225/150
    Miller Maxstar 150 STL
    Victor 100C
    Victor Journeyman
    Oxweld OA
    Harris O/A
    Smith O/A little torch

    No, that's not my car.

  7. #107
    Join Date
    Aug 2010
    Posts
    29
    Post Thanks / Like

    Re: HF Tools That Suck

    Their garden hose menders leave a lot to be desired.

    http://www.harborfreight.com/lawn-ga...rden-hose.html

    They seem like the people who designed them didn't actually test them out on several different hoses.

    The center black plastic piece works just fine.

    It is the green or yellow plastic clamps, and screws that don't work worth a damn.

    The supplied screws are a little too short to thread into the opposite half of the clamp properly, so the part that does thread ends up tearing out and damaging the thread hole while tightening.

    It seems like the only answers to being able to use this product properly is to:
    1. supply your own longer screws
    or
    2. only use it on a very thin-walled hose (one which might allow the 2 halves of the clamps to close closer together.

  8. #108
    Join Date
    Dec 2005
    Location
    Midland, Texas
    Posts
    1,199
    Post Thanks / Like

    Re: HF Tools That Suck

    I've got some of their brass garden hose couplings and they are very good. I don't see them in the online catalog, but I saw some recently at our local store.
    America Needs AMERICA'S Oil!!!

    "Global warming is the greatest scam in history ...There is no run away climate change. The impact of humans on climate is not catastrophic. Our planet is not in peril."--John Coleman, Founder of The Weather Channel

  9. #109
    Join Date
    Sep 2010
    Location
    Concord, NC
    Posts
    89
    Post Thanks / Like

    Re: HF Tools That Suck

    Chicago (Harbor Freight) 4-1/2" Angle Grinder

    I get just enough email from my viewers about looking at "cheap" tools that I actually do from time to time. this time it was the Chicago 4-1/2" Angle Grinder. See the link below for the full review but suffice it to say that the trend continues......

    Chicago (Harbor Freight) 4-1/2" Angle Grinder Review

  10. #110
    Join Date
    Jun 2010
    Posts
    44
    Post Thanks / Like

    Re: HF Tools That Suck

    I have two of those grinders and have put them through hell and they are still going, so i am happy with them.

  11. #111
    Join Date
    Jan 2009
    Location
    Sonoma County
    Posts
    893
    Post Thanks / Like

    Re: HF Tools That Suck

    Quote Originally Posted by Tomhintz View Post
    Chicago (Harbor Freight) 4-1/2" Angle Grinder

    I get just enough email from my viewers about looking at "cheap" tools that I actually do from time to time. this time it was the Chicago 4-1/2" Angle Grinder.
    Your post looks like you are fishing for more readers for your own site rather than coming here to share useful information with us. Why didn't you write your conclusions in this post?

    What a surprise! You evaluated, and concluded that a 4.5 amp tool isn't the same thing as 9 amp tool!!!

    And the page after page of safety instructions and inclusion of spare brushes somehow causes you concern. (Or gives you something to pad your review.)

    These are cheap grinders that serve well in occasional use, not tradesman grade or the over-the-top 'pride of ownership' gear often collected by woodworkers. They are what they are. Many of us need a grinder for very few hours per year and this one is sufficient to get the work done. That is simply all we need. I wish you had listed the cost of your 9 amp grinder that this one didn't quite equal. This could help some of us decide which one we need.

    Of course anyone should buy top quality tools where greater productivity is important and cost-effective. That is a different market. You might be happier if you avoid Harbor Freight entirely, I wouldn't want you to endure another disappointment.

  12. #112
    Join Date
    Jan 2010
    Location
    West Virginia
    Posts
    137
    Post Thanks / Like

    Re: HF Tools That Suck

    That was very well said california i really enjoyed reading your reply...
    In the words of the great philosopher Quagmire.Gigedy Gigedy Gigedy Gigidey Goo.

  13. #113
    Join Date
    Aug 2010
    Posts
    29
    Post Thanks / Like

    Re: HF Tools That Suck

    Several months ago, I saw some welding aprons on clearance for dirt cheap (I think they marked down less than a dollar each).
    They weren't leather. They were like a tightly woven burlap kind of fabric, and colored green.

    I bought some, but THOROUGHLY and quickly regretted it.

    You know how some of the items in Harbor Fright can smell a bit?

    Well, those aprons made all the other smells in that store seem like roses in comparison.
    I wouldn't be surprised if that was the whole reason they were clearance in the first place.

    I don't know what they put in that fabric, but it made it stink so bad, I wouldn't be surprised if they had soaked it for a few months at the bottom of a cesspool.

    This may all sound like an exaggeration, but it's not. It really did stink so bad, it made you want to vomit. I never even wore it. Just getting near it made me feel like it might have been made out of dogsh!t.

    I did return all but 1 though, since I no longer had the package for it.
    When the cashier asked what was wrong with them, I told her they reeked way too bad to be able to use. She just looked at them with a disgusted look, and then took them and refunded my money.
    Last edited by SuperNinja; 10-20-2010 at 01:23 AM.

  14. #114
    Join Date
    Dec 2005
    Posts
    13
    Post Thanks / Like

    Re: HF Tools That Suck

    Sorry to say this, but their 4.5" angle grinders suck. I bought 4-5 before I swore off of them. A couple had really bad vibration, but most of all they are severely underpowered compared to the Milwaukee, Makita, and old Dewalt grinders I have. Very rough operation overall. I also bought the electric die grinder from them and it burned up in 30 minutes.

    I also had to return their metric deepwell impact sockets. They "stuck" themselves to good lugnuts as if they were oversized.

    The 8" bench grinder I bought as well as some of their air tools (earthquake impact, die grinders, etc.) have been great. Oh and the 4x6 bandsaw of course.
    Engineer/CWI/Welder

  15. #115
    Join Date
    Dec 2005
    Location
    Midland, Texas
    Posts
    1,199
    Post Thanks / Like

    Re: HF Tools That Suck

    Quote Originally Posted by SuperNinja View Post
    ...They were like a tightly woven burlap kind of fabric, and colored green.

    ...You know how some of the items in Harbor Fright can smell a bit?

    Well, those aprons made all the other smells in that store seem like roses in comparison.
    I wouldn't be surprised if that was the whole reason they were clearance in the first place.

    I don't know what they put in that fabric, but it made it stink so bad, I wouldn't be surprised if they had soaked it for a few months at the bottom of a cesspool.
    Sounds like their Russian made welding blankets. They stink.
    America Needs AMERICA'S Oil!!!

    "Global warming is the greatest scam in history ...There is no run away climate change. The impact of humans on climate is not catastrophic. Our planet is not in peril."--John Coleman, Founder of The Weather Channel

  16. #116
    Join Date
    Jan 2004
    Location
    Northern Cal., Shasta County
    Posts
    9,327
    Post Thanks / Like

    Re: HF Tools That Suck

    Screwed up and bought a couple of HF long ram jacks. Momentarily reverted back to the old sour logic "they're just for occasional use", "gonna set there and sleep most of the time", "light and limited duty".. Bought two of 'em. Need them for this frame rotisserie thing I'm working on.

    The one that did work wouldn't pump up all the way. About 16" out of it's claimed 19+", not enough fluid. Added about a cup or cup 'n and now it goes to the top. Oozes back down about an inch with any slight weight. Still some air in there I suppose.

    The other one I added some fluid to it right off so it pumped up to about 15" or so then stalled then lurched on up after about three pumps. Now the big problem, it sticks at the top, won't come down. Hold it by the ram and slam the base on the floor and it'll go down once it gets past whatever it is at that 15-16" spot. Two or three times of the same ole chit and I left it in the up position, took it back and got another. At least they've got that "we'll replace them till you run out of gas money" policy.

    The replacement goes right to the top but won't hold there. Oozes down a couple of inches. Needs fluid I suppose. I'll have to get some. Used all I had on the other two jacks.

    SO how do I rate these? one out of two failed so that's would be 50% DOA but the replacement seems okay so maybe I should rate them at only a 30% out of the box failure. Maybe 30% out of the box failure with points taken away for the lack of adequate fluid.
    "The things that will destroy America are prosperity at any price, peace at any price, safety first instead of duty first, the love of soft living and the get rich quick theory of life." -Theodore Roosevelt

  17. #117
    Join Date
    Dec 2010
    Location
    Olathe Kansas
    Posts
    665
    Post Thanks / Like

    Re: HF Tools That Suck

    Whats this Harbor Freight stuff , I dont know if ive ever heard of this equipment ......lol junk all junk.....i wouldnt trust my life with a hf grinding wheel ive had a norton come unglued on me once and it scared me enough the reason it came apart the grinder was dropped.... i have used a hf wheel i used it long enough to get it up to speed and slow back down .....never again......You get what you pay for .... my time isnt cheap why would i want to break a tool every day ......i rarely have any of my quality stuff break
    I forgot how to change this.

  18. #118
    Join Date
    Dec 2005
    Location
    Midland, Texas
    Posts
    1,199
    Post Thanks / Like

    Re: HF Tools That Suck

    Thanks, LawsonWeldingLLC, for contributing absolutely nothing of value to this thread.
    America Needs AMERICA'S Oil!!!

    "Global warming is the greatest scam in history ...There is no run away climate change. The impact of humans on climate is not catastrophic. Our planet is not in peril."--John Coleman, Founder of The Weather Channel

  19. #119
    Join Date
    Sep 2010
    Location
    Concord, NC
    Posts
    89
    Post Thanks / Like

    Re: HF Tools That Suck

    Chicago/Harbor Freight 4-1/2" Angle grinder. See my full review at the link below but this thing is trash and scary to run. The gears are badly meshed so this thing get very loud, vibrates and scary at speed. the up side is that the box it comes in says that you even get a spindle nut! Free!

    http://www.newmetalworker.com/Review...ggrndrrvu.html
    Tom Hintz, publisher
    www.newmetalworker.com
    Lincoln Pro Mig 180
    Lincoln AC 255
    Determination

  20. #120
    Join Date
    Jan 2010
    Posts
    118
    Post Thanks / Like

    Re: HF Tools That Suck

    I got the 66787 tig/inverter arc welder a few months ago.It worked fine at first, but now its doing this thing where a squeeking noise like comes from the tungsten and the amperage goes very low..If you long arc it for a second the arc comes back but everytime you dip the filler rod it happens again..It used to do it only ocasionally but now its at the point where it does this everytime I weld ..saving for a real welder now..

  21. #121
    Join Date
    Nov 2010
    Posts
    9
    Post Thanks / Like

    Re: HF Tools That Suck

    Bought this small ring roller on my trip to the USA at HF. Didnt figure i can go wrong,
    I was wrong. The rollers do not align. Now i get to try and fix it myself or try to return it, which might be a problem, since i had it for a while.
    Oh well
    Attached Images Attached Images  

  22. #122
    Join Date
    Jan 2011
    Location
    Coronado. CA across the bay from San Diego, CA
    Posts
    1,271
    Post Thanks / Like

    Re: HF Tools That Suck

    I took a chance on a 9.95 harbor freight grinder, and bought a seconed one so I could have a cup brush and flap wheel without having to change attachments. The grinder with the cup brush goes back on Monday, it will be DOA.

    I am glad I bought the insurance policy, I can see myself going to Harbor Freight frequently. I am getting what I paid for.
    I offer three choices: Good, Fast, & Cheap. You may pick two.

    Hobart AC/DC StikMate LX
    Harbor Freight AD Hood
    Harbor Freight Industrial Chop Saw
    DeVilbis 20 Gallon, 5 HP Compressor

  23. #123
    Join Date
    Mar 2010
    Posts
    392
    Post Thanks / Like

    Re: HF Tools That Suck

    ok, i now have 2 of the HF 4 1/2" grinders. one is a old model given to me 4 years ago, one i just bought a month ago. they both seem to have about the same power, fine use for a flap disc or cut-off.
    when doing some actual grinding, they suck. but lives up to "10$ grinder expectations"

    i just got a dewalt 818, 9 amp unit. the difference is night and day (cost w/ SH was $50)better switch, better guard,theres less vibration, it sounds like higher rpms, and when you put the wheel to metal and apply pressure it actually keeps grinding.

  24. #124
    Join Date
    Jan 2009
    Location
    Sonoma County
    Posts
    893
    Post Thanks / Like

    Re: HF Tools That Suck

    HF sells more expensive 4.5" grinders aside from the $10 and $18 ones.

    Does anyone recommend their better models?

  25. #125
    Join Date
    Nov 2010
    Location
    North Hollywood, CA
    Posts
    26
    Post Thanks / Like

    Re: HF Tools That Suck

    I bought their 18 Volt 1/2" Magnesium Drill/Driver and it work fine for 2 weeks. Then one day it stopped. The battery does not make good contact with the base, hence no power.

    I got a refund, but HF didn't want the thing back.
    Bill

    Millermatic 211

    1960 Ford Ranchero
    1975 Dodge B200

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,570,129.40182 seconds with 12 queries